This presentation is an introduction to machine learning techniques and their application in semiconductor failure analysis. The presentation compares and contrasts supervised, unsupervised, and reinforcement learning methods, particularly for neural networks, and lays out the steps of a typical machine learning workflow, including the assessment of data quality. It also presents case studies in which machine learning is used to detect and classify circuit board defects and analyze scanning acoustic microscopy (SAM) data for blind source separation.