Abstract

Practice and training samples have been manufactured using 3D-printing methods. These 3D-printed samples mimic the exact geometry of focused ion beam (FIB) prepared specimens and can be used to help master ex situ and in situ lift out micromanipulation methods. An additively manufactured array of samples yields numerous samples needed for repetition and deliberate practice necessary to master the lift out and micromanipulation steps. The 3D-printed samples are cost effective and negates expensive FIB time needed to prepare FIB specimens.