The reliability of a pure CMOS One-time Programmable (PCOP) Memory was investigated. The memory is programmed with and anti-fuse formed by the breakdown of the thin gate oxide. The results of reliability stress tests show that the PCOP memory is stable and reliable for normal using environmental conditions.