Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Thermochemical boriding
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
HT 2021, Heat Treat 2021: Extended Abstracts from the 31st Heat Treating Society Conference and Exposition, 38-43, September 14–16, 2021,
Abstract
View Papertitled, Electron-Beam Surface Modification of Boron-Based Diffusion Layers Obtained of the Surface of Steel H21
View
PDF
for content titled, Electron-Beam Surface Modification of Boron-Based Diffusion Layers Obtained of the Surface of Steel H21
This paper presents the results of a study on a new coating method for alloy steel. The coatings were synthesized on the surface of H21 die steel through a combination of thermal-chemical treatment (TCT) and electron beam processing (EBP). A paste containing boron and aluminum was applied to the test samples which were then heated to accelerate the diffusion process. After 2 h at 950 °C, the diffusion layers were found to be 120 μm thick, and after 2 h at 1050 °C, they were 580 μm thick. The subsequent EBP led to a complete transformation of the primary diffusion layer and an increase in thickness to 1.6 mm. XRD analysis showed significant differences in composition before and after EBP and the presence of tungsten and iron borides. It was also found that the distribution of microhardness and composition over the layer thickness had a more favorable profile after EBP.