Abstract
This study examines the impact of thermal post processing, specifically induction hardening and tempering, on the fatigue performance of laser powder bed fusion (PBF-LB) manufactured AISI 4140 steel. Results highlight the importance of porosity control, with induction hardening effectively addressing near-surface porosity issues in non-machined parts.