Abstract
This study investigates the interaction between tempering processes and the formation of tempering transformation induced plasticity (T-TRIP) in 50CrMo4 steel during laser heat treatment. Various configurations, including single and double laser treatments, were examined along with different initial material states and heat treatment parameters.
This content is only available as a PDF.
Copyright © 2025 ASM International. All rights reserved.
2025
ASM International
Issue Section:
Fundamental Principles