This study investigates the effect of vapor blanket duration in quenching oil on the mechanical properties and distortion of JIS-S45C carbon steel and JIS-SCM435 low-alloy steel. Four types of heat treatment oils with varying vapor blanket stage lengths were tested on key-grooved cylindrical specimens. Results indicate that quenching oils with longer vapor blanket durations produced smaller distortions, while oils with shorter durations caused larger distortions.