Numerous trademarked, standardized or proprietary nitriding and ferritic nitrocarburizing recipes and control methods are used in industrial furnaces. Surface Combustion has developed a new tool to predict the in-process composition of nitriding and ferritic nitrocarburizing atmospheres from these different processes. In addition, the activities and potentials of carbon, nitrogen and oxygen can be found, leading to prediction of the associated equilibrium phase on the part surface. The theory behind the tool and the application of the tool to control nitriding and ferritic nitrocarburizing atmospheres will be discussed. An overview of different equipment designs that can use the tool will also be presented.