Abstract
The development of residual stress in an induction hardened small spur gear is numerically simulated. A full scale 3D simulation is utilized to obtain the results, providing the possibility to evaluate the complete distribution of residual stress in the hardened component. Electromagnetic and thermal solutions under induction heating conditions are obtained with Cedrat Flux 3D, whereas EDF Code Aster software is used for thermal simulation during the quenching stage, phase transformation, and stress-strain simulations. The simulated induction heating isotherms and distribution of residual stress are compared with experimental investigations done by Larregain et al. and Savaria et al.