1-20 of 314 Search Results for

yellowness

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003027
EISBN: 978-1-62708-200-6
...Abstract Abstract Optical testing of plastics includes characterization of materials and analysis of optical components. This article focuses on procedures for testing various characteristics of optical components, including transmission and haze, yellowness, refractive index, birefringence...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006635
EISBN: 978-1-62708-213-6
... of a crystalline precipitate melting between 121 and 123 °C (250 and 253 °F) 3. Silver nitrate White precipitate of silver benzoate from cold solutions, soluble in hot water and also in dilute ammonia solution 4. Iron(III) chloride Buff-colored (light yellow-red) precipitate of iron (III) benzoate from...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001316
EISBN: 978-1-62708-170-2
... Chromium-manganese-zinc brown spinel 71750-83-9 (Zn,Mn)Cr 2 O 4 13-51-7 Yellow Zirconium-vanadium yellow baddeleyite 68187-01-9 (Zr,V)O 2 1-01-4 Tin-vanadium yellow cassiterite 68186-93-6 (Sn,V)O 2 11-22-4 Zirconium-praseodymium yellow zircon 68187-15-5 (Zr,Pr)SiO 4 14-43-4...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005332
EISBN: 978-1-62708-187-0
...-zinc (semired brasses) C84 xxx Copper-zinc (yellow brasses) C85 xxx Manganese bronzes C86 xxx Copper-silicon C87 xxx Copper-bismuth C88 xxx , C89 xxx Copper-tin (tin bronzes) C90 xxx , C91 xxx Copper-tin-lead (leaded tin bronzes) C92 xxx Copper-tin-lead (high-leaded...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001068
EISBN: 978-1-62708-162-7
... brass 5.7 1010 1850 2 6 C84400 Leaded semired brass 2.0 980 1795 2 6 C84800 Leaded semired brass 1.4 955 1750 2 6 C85400 Leaded yellow brass 1.5–1.8 940 1725 4 3 C85800 Yellow brass 2.0 925 1700 4 3 C86300 Manganese bronze 2.3 920 1690 5 2 C86500...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006280
EISBN: 978-1-62708-169-6
... Prince metal 75 25 … A type of alpha brass. Due to its yellow color, it is used as an imitation of gold. Also called Prince Rupert’s metal, the alloy was named after Prince Rupert of the Rhine. Red brass, rose brass 85 5 5% Sn and 5% Pb An American term for the Cu-Zn-Sn alloy known as gunmetal...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006512
EISBN: 978-1-62708-207-5
... using oxalic acid, which produces very hard films with yellow to light bronze colors, but because these coatings required very thick films to develop colors, they were not very popular. Schering ( Ref 2 ) in Germany investigated acids with sulfonic groups that became the bases for the integral coloring...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003134
EISBN: 978-1-62708-199-3
... Shrinkage allowance, % Approximate liquidus temperature Castability rating (a) Fluidity rating (a) °C °C C83600 Leaded red brass 5.7 1010 1850 2 6 C84400 Leaded semired brass 2.0 980 1795 2 6 C84800 Leaded semired brass 1.4 955 1750 2 6 C85400 Leaded yellow brass...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006629
EISBN: 978-1-62708-213-6
... used acid-base indicators Table 11 Frequently used acid-base indicators Name Acid color Approximate pH range for color change Base color Methyl violet Yellow 0.0–1.6 Violet Cresol purple Red 1.2–2.8 Yellow Bromophenol blue Yellow 3.0–4.6 Blue Bromocresol green...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003776
EISBN: 978-1-62708-177-1
... image of the outer edge of the platinum-aluminum sample. (a) 25×. (b) The interface between the predominantly blue Pt 2 Al 3 phase area (light gray) and the predominantly yellow PtAl 2 phase area (dark gray). 220× Fig. 54 Scanning electron microscope image in secondary electron mode of 56Pt...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003844
EISBN: 978-1-62708-183-2
..., Indian, or Persian Gulf red Excellent Excellent Cadmium red … Excellent Poor Molybdate orange … Poor to fair Poor Lead Minium, mineral orange Good Poor Yellow iron oxide Ferrite yellow, sienna, ochre, umber Excellent Fair Chrorme yellow … Poor to fair Fair Zinc yellow...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005997
EISBN: 978-1-62708-168-9
... to cherry 900 1652 Cherry proper 1000 1832 Bright cherry red 1100 2012 Orange red 1200 2192 Orange yellow 1300 2372 White 1400 2552 Brilliant white 1500 2732 Dazzling white 1600 2912 Bluish white Source: Ref 1 Colors of tempering heats Table 2 Colors...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006259
EISBN: 978-1-62708-169-6
..., and zinc as the main constituents. Depending on the silver/copper/zinc ratios, these alloys exhibit yellow, green, and red colors. Colored gold alloys normally are annealed in a protective and reducing atmosphere, usually in a mixture of hydrogen and nitrogen, at temperatures between 550 and 650 °C (1020...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001255
EISBN: 978-1-62708-170-2
... on a high-speed copper plating process by DuPont were extended to a high-speed process for plating of both yellow and white brass (alloys containing about 70 to 80% Cu). The solution was cyanide based with a relatively high hydroxide content. The treatment of waste water from brass and bronze plating...
Book Chapter

By Nabil Zaki
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001257
EISBN: 978-1-62708-170-2
... of such parts. Available chromates include clear, yellow, iridescent and black. Typical zinc-cobalt bath compositions and process parameters are given in Table 1 . Tin-zinc alloys contain 70 to 90% Sn and 10 to 30% Zn. Cyanide, acid, and neutral commercial baths are available. Tin-zinc baths...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001821
EISBN: 978-1-62708-180-1
... Board , Washington , June 1979 5. Bowers D.G. , Loading History Span 10 Yellow Mill Pond Bridge 195 Bridgeport, Connecticut , Research project HPR 175-332, Connecticut Department of Transportation , Whethersfield, CT , 1972 6. Dickey R.L. and Severga T.P...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006073
EISBN: 978-1-62708-172-6
... to fair Poor Lead Minium, mineral orange Good Poor Yellow iron oxide Ferrite yellow, sienna, ochre, umber Excellent Fair Chrorme yellow … Poor to fair Fair Zinc yellow Zinc potassium chromate Fair Poor Cadmium yellow … Excellent Poor Nickel titanate yellow … Excellent...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0001739
EISBN: 978-1-62708-178-8
... Remarks Dimethylglyoxime Ni and Pd Red Ni and yellow Pd precipitates are relatively clean, high Co requires reprecipitation Chloride ion Ag and Hg(l) AgCl may be photoreduced if not protected from light; HgCl shows slight solubility Mandelic acid Zr and Hf Best precipitated from hot...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005303
EISBN: 978-1-62708-187-0
... casting is best suited for tin, silicon, aluminum and manganese bronzes, and yellow brasses. Dies casting is well suited for yellow brasses, but increasing amounts of permanent mold alloys are also being die cast. Size is a definite limitation for both methods, although large slabs weighing as much...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002437
EISBN: 978-1-62708-194-8
... for the designer, Vol 2 is a handbook of anthropometric data, and Vol 3 is an annotated bibliography) available from the NASA Scientific and Technical Information Office, Yellow Springs, OH. The Department of Defense (DOD) has a basic handbook, Human Engineering Procedures Guide , DOD-HDBK-763. One of the basic...