1-20 of 219 Search Results for

wrought nickel-based superalloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006582
EISBN: 978-1-62708-290-7
...-base superalloys were designed for either wrought or casting processes. The nickel-base superalloy Inconel 718, in use for over 60 years, is one of the most studied and remains the most widely used nickel-base superalloy, due to its legacy status within the aerospace community. The focus for AM...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006581
EISBN: 978-1-62708-290-7
... D. , Ackelid U. , and Wicker R.B. , Microstructural Architecture, Microstructures, and Mechanical Properties of a Nickel-Base Superalloy Fabricated by Electron Beam Melting , Metall. Mater. Trans. A , Vol 42 , 2011 , p 3491 – 3508 , 10.1007/s11661-011-0748-2 34. Lambrakos...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006566
EISBN: 978-1-62708-290-7
... be performed before or after HIP. Recognizing the importance of thermal postprocessing of AM parts, ASTM International developed a standard for L-PBF parts ( Ref 82 ), which is limited to recommendations for 4340 alloy steel and 316 stainless steel. Work on the nickel-base superalloy IN-625...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006552
EISBN: 978-1-62708-290-7
.... Powder metallurgy HIP is commonly used to produce billets of high-performance tool steels and high-speed steels and nickel-base superalloy and stainless steel NNS components mainly for the oil, gas, and nuclear industries. The main advantages of powder metallurgy HIP include good material properties as a...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.9781627082907
EISBN: 978-1-62708-290-7
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006557
EISBN: 978-1-62708-290-7
... relaxation, stress concentrations, or by “buttering” the substrate used as the base plate for joining ( Ref 4 ). On the other hand, SAC occurs intergranularly in the heat-affected zone (HAZ) of precipitation-strengthened nickel-base alloys. The simultaneous local strain and aging conditions applied to...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005886
EISBN: 978-1-62708-167-2
... superalloys computational modeling forming heat treatment induction heating stainless steel superalloys temperature wrought nickel-based superalloys Induction heating and heat treating processes are used for a range of materials and applications ( Ref 1 , 2 , 3 ). These processes also apply to...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003120
EISBN: 978-1-62708-199-3
... mechanical properties and chemical composition of nickel, iron, and cobalt-base superalloys in both the cast and wrought forms. chemical composition cobalt-base superalloys environmental factors high-temperature applications iron-base superalloys mechanical properties metal processing...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001049
EISBN: 978-1-62708-161-0
... Abstract This article focuses on the properties of conventional wrought superalloys based on nickel, iron, and cobalt, as well as on the properties of alloys produced from powder. The powder metallurgy (P/M) category includes alloys that were originally developed as casting alloys; new alloy...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001050
EISBN: 978-1-62708-161-0
... problems experienced with the early nickel-chromium-iron solid-solution wrought superalloys. This work ultimately led to the successful manufacture of investment cast components for the first U.S. production gas turbine engine in 1945 ( Ref 1 ). Nickel-base and nickel-iron-base superalloys owe their high...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005961
EISBN: 978-1-62708-168-9
....) As noted, iron-base superalloys evolved from austenitic stainless steels, and the PH alloy A-286 is considered to be part of the family of iron-nickel superalloys ( Table 20 ). Iron-nickel superalloys, which are produced only in wrought form, are classified as either solid-solution hardened or PH...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005459
EISBN: 978-1-62708-196-2
... Abstract This article summarizes the general features of microstructure evolution during the thermomechanical processing (TMP) of nickel-base superalloys and the challenges posed by the modeling of such phenomena. It describes the fundamentals and implementations of various modeling...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006094
EISBN: 978-1-62708-175-7
... engine for the F-18 Hornet fighter aircraft. René 95 was a higher strength nickel-base alloy that GE hoped to produce via cast and wrought methods and cross roll into heavy plate. Due to the difficulty, the company approached Crucible Steel Co., owned by Colt Industries, to manufacture René 95 in its 600...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006265
EISBN: 978-1-62708-169-6
... alloys, and the effects of cold work on aging response and grain growth with examples. annealing chemical composition fixtures heat treatment precipitation hardening solution heat treatment stress relieving superalloys surface degradation wrought nickel alloys NICKEL ALLOYS derive...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001425
EISBN: 978-1-62708-173-3
...-strengthened nickel superalloy relative to conventional dispersion-strengthened nickel superalloys and cast nickel-base alloys Once the assembly has been fabricated, it is normally put into service at temperatures of 760 to 1095 °C (1400 to 2000 °F). At these temperatures, the chromium (and sometimes...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001053
EISBN: 978-1-62708-161-0
... refined out of the nickel product and not recovered. This breakdown of the 25 × 10 3 Mg (55 × 10 6 lb) includes the 2 × 10 3 Mg (4.3 × 10 6 lb) that was exported. Downgrading refers to the practice of including an alloy in the feedstock of a less critical alloy. For example, a nickel-base superalloy...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003993
EISBN: 978-1-62708-185-6
... superalloys, namely, iron-nickel superalloys, nickel-base alloys, cobalt-base alloys, and powder alloys. The article discusses the microstructural mechanisms during hot deformation and presents processing maps for various superalloys. It concludes with a discussion on heat treatment of wrought heat-resistant...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003147
EISBN: 978-1-62708-199-3
... mining and extraction of nickel and describes the uses of nickel. It discusses the categories of nickel-base alloys, including wrought corrosion-resistant alloys, cast corrosion-resistant alloys, heat-resistant alloys (superalloys), and special-purpose alloys. The article covers the corrosion resistance...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001412
EISBN: 978-1-62708-173-3
... Oct 1963 , p 98 12. Aggen G. , “Phase Transformations and Heat Treatment Studies of a Controlled Transformation Stainless Steel Alloy,” Dr. Eng. Sc. Thesis, Rensselaer Polytechnic Institute, Aug 1963 13. Muzyka D.R. , The Metallurgy of Nickel-Iron Alloys, The Superalloys...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0