Published: 30 September 2015
Fig. 34 Diagram of water induction nozzle for wet abrasive blast cleaning More
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001228
EISBN: 978-1-62708-170-2
..., indirect-suction (induction) wet or dry blast nozzle systems. This article focuses on the abrasive media, equipment, applications, and limitations of dry and wet blast cleaning. It discusses the health and safety precautions to be taken during mechanical cleaning. airless centrifugal blast blade...
Image
Published: 01 December 2008
Fig. 4 Typical wet scrubber with heat recuperation hot blast used to clean emission gases More
Image
Published: 31 August 2017
Fig. 6 Typical wet scrubber with heat recuperation hot blast used to clean emission gases More
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006024
EISBN: 978-1-62708-172-6
... on surface preparation methods that range from simple solvent cleaning to hand and power tool cleaning, dry and wet abrasive blast cleaning, centrifugal wheel blast cleaning, chemical stripping, and waterjetting for the application of the coating system. In addition, the article provides a description...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003694
EISBN: 978-1-62708-182-5
... for Power- and Hand-Tool Cleaned Steel.” (c) SSPC-VIS 4/NACE VIS 7, “Guide and Reference Photographs for Steel Surfaces Prepared by Waterjetting.” (d) SSPC-VIS 5/NACE VIS 9, “Guide and Reference Photographs for Steel Surfaces Prepared by Wet Abrasive Blast Cleaning” Although there are other...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006504
EISBN: 978-1-62708-207-5
... predetermine the potential consequences of such methods so as not to damage the parts before they are finished and in their final end use. Abrasive Blast Cleaning One of the simplest and most effective methods for cleaning aluminum surfaces is by blasting with dry nonmetallic or metallic abrasives...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006062
EISBN: 978-1-62708-172-6
... expanses of mostly flat surfaces that help contain the vacuum and is mostly impractical for cleaning angular small surfaces and complex structural steel members. Wet Abrasive Blasting Wet abrasive blasting generally uses some combination of water and abrasive to clean and prepare the surface...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006070
EISBN: 978-1-62708-172-6
... is by using both blast cleaning and water. Wet abrasive blast cleaning (where the abrasive is wetted in a conventional dry blast-cleaning stream) and abrasive injection into a high-pressure waterjet blast-cleaning stream are the best means of removing salt contamination. The abrasive particulate in the blast...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003220
EISBN: 978-1-62708-199-3
... for initiation of pitting. prevent corrosion. Passivation, pickling, electro- Sand blasting is effective for rapid removal polishing, and, in some cases, mechanical clean- of heavy or tightly adhering scale. The types of Wet blasting is adaptable for use with stain- ing are important surface treatments...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006016
EISBN: 978-1-62708-172-6
... standards. Visual guides prepared by the SSPC for abrasive blast cleaning, hand and power tool cleaning, water jetting, and wet abrasive blast cleaning can be used to aid in the evaluation of surface cleanliness. These are described later in the article. In the event of a dispute, it is the written...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001307
EISBN: 978-1-62708-170-2
... is recommended, regardless of the abrasive used. Wet abrasive blasting, also referred to as vapor honing, is also used to clean heat-resistant alloys. This process uses Nos. 200 to 1250 silica abrasive particles (0.074 to 0.010 mm, or 0.0029 to 0.0004 in.) mixed with water to produce a slurry that removes...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006335
EISBN: 978-1-62708-179-5
... preparation also must be consistent with the recommendations of the intended coating manufacturer. Surface-preparation methods can range from simple solvent cleaning to hand and power tool cleaning; from dry and wet abrasive blast cleaning to chemical stripping; and from waterjetting to other, more...
Image
Published: 30 September 2015
Fig. 15 Fusion-bonded epoxy (FBE) application for rebar is similar to pipe. Abrasive blast clean, heat, FBE spray application, provide time to cure before quench, holiday test using a wet-sponge system, and bundle. Courtesy of J.A. Kehr More
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001453
EISBN: 978-1-62708-173-3
... be taken that the surfaces are not burnished and that mechanical cleaning materials are not embedded in the metals to be brazed. In grit blasting, choice of the blasting medium is critical. Wet and dry grit blasting commonly are used, but wet mediums are subject to additional cleaning requirements...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006492
EISBN: 978-1-62708-207-5
... attachments. Blast Cleaning Dry abrasive blast cleaning, wet abrasive blast cleaning, and vacuum blast cleaning are common means of preparing aluminum surfaces in the field. Relatively low blast-cleaning pressure, on the order of 275 to 415 kPa (40 to 60 psi) air pressure, should be used to minimize...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003221
EISBN: 978-1-62708-199-3
... blasting. Conditions for wet blasting of aluminum-base materials Table 2 Conditions for wet blasting of aluminum-base materials Operation Abrasive Type Mesh size Deburr and clean Alumina 220 Blend and grind Silica flour 325 Lap and hone Glass 1000 Diatomite 625–5000...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001269
EISBN: 978-1-62708-170-2
... Abstract This article focuses on the various techniques for removing contaminants in the surface preparation of steel for hot-dip coatings: wet cleaning methods, including alkaline cleaning, electrolytic cleaning, chemical pickling, and electrolytic pickling; flame cleaning and furnace...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006517
EISBN: 978-1-62708-207-5
... abrasive blast cleaning aluminum barrel finishing buffing honing lapping abrasive belt polishing satin finishing shot peening abrasive wheel grinding aluminum alloys MECHANICAL finishing methods remove surface irregularities and smooth the surface, and they apply a texture to the product...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004108
EISBN: 978-1-62708-184-9
... International (formerly the National Association of Corrosion Engineers), and standards groups in Sweden, Germany, the United Kingdom, and Japan have all issued standards for surface preparation. Examples of these are listed in Table 1 . Wet abrasive blast cleaning and waterjetting (waterblasting) are not yet...