1-20 of 1433

Search Results for welding machine

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 31 October 2011
Fig. 1 Schematic showing primary components of a resistance welding machine More
Image
Published: 31 October 2011
Fig. 4 Flash-welding machine used to fabricate a coiled steel strip into a small-diameter ring with a flange More
Image
Published: 31 October 2011
Fig. 5 Flash-welding machine with capacity to weld rings up to 4.6 m (15 ft) in diameter More
Image
Published: 31 October 2011
Fig. 6 Flash-welding machine installation equipped to weld band-saw blades More
Image
Published: 31 October 2011
Fig. 7 Electrode forces under different welding machine stiffnesses. Source: Ref 3 More
Image
Published: 31 October 2011
Fig. 9 Very large-chamber, low-voltage electron beam welding machine (600 m 3 , 80 kV/40 kW machine). Courtesy of pro-beam AG & Co. KGaA More
Image
Published: 01 January 1993
Fig. 7 Schematic showing primary components of a resistance welding machine More
Image
Published: 01 January 1993
Fig. 2 Flash-welding machine used to fabricate a coiled steel strip into a small-diameter ring with a flange More
Image
Published: 01 January 1993
Fig. 3 Flash-welding machine with capacity to weld rings up to 4.6 m (15 ft) in diameter More
Image
Published: 01 January 1993
Fig. 4 Flash-welding machine installation equipped to weld band-saw blades More
Image
Published: 01 January 1993
Fig. 3 Radial friction-welding machine with a 51 mm (2 in.) diameter More
Image
Published: 01 January 1993
Fig. 4 Schematic of the prototype radial friction-welding machine More
Image
Published: 01 January 1993
Fig. 2 Plot of welding machine power consumption versus material thickness for selected metals joined by ultrasonic welding More
Image
Published: 01 January 2001
Fig. 13 Schematic for ultrasonic welder and multiunit weld machine. Source: Ref 30 , 31 More
Image
Published: 01 January 2001
Fig. 17 Induction weld machine More
Image
Published: 01 August 2013
Fig. 18 Universal-chamber electron beam machine for hardening, welding, engraving, and structuring. Chamber volume: 0.5 m 3 ; beam parameters: 60 kV, 10 kW. Courtesy of FOCUS More
Image
Published: 31 October 2011
Fig. 8 Early machine for welding the longitudinal seam in a hot water tank with an automatic carbon arc welding head. More
Image
Published: 31 December 2017
Fig. 6 Example of modified milling machine for friction stir welding/friction stir processing. Reprinted with permission from Elsevier. Source: Ref 15 More
Book Chapter

By Neville T. Williams
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001363
EISBN: 978-1-62708-173-3
... of spot welding and the three principal elements, such as electrical circuit, control circuit, and mechanical system, of RSW machines. It reviews the three basic types of RSW machines: pedestal-type welding machines, portable welding guns, and multiple spot welding machines. The article provides...
Book Chapter

By E.D. Nicholas
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001382
EISBN: 978-1-62708-173-3
... illustrates a prototype of radial friction-welding machine and concludes with a discussion on applications that would be suitable for radial friction welding. radial friction welding welding machines THE CONVENTIONAL FRICTION-WELDING PROCEDURE of rotating one component against another while...