Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005668
EISBN: 978-1-62708-198-6
... Abstract This article provides an overview of the fundamentals of tribology. It describes the advantages, disadvantages, and applications of pin-on-disk method, which is the most commonly used configuration for testing biomaterials and for the reproducible measurement of friction and wear. The...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005678
EISBN: 978-1-62708-198-6
... tribological advantages of ceramics over metals as counterfaces for polyethylene, but decreases in the wear rates of the polyethylene of at least 50% have been reported ( Ref 19 , 20 ) from laboratory tests. Other studies have yielded a more confusing picture ( Ref 21 , 22 ), but it is now generally...
Book Chapter

By Peter J. Blau
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003242
EISBN: 978-1-62708-199-3
... Abstract Wear is mechanically-induced surface damage that results in the progressive removal of material. Because different types of wear occur in machinery, many different types of wear tests have been developed to evaluate its effects on materials and surface treatments. This article provides...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.9781627081764
EISBN: 978-1-62708-176-4
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003030
EISBN: 978-1-62708-200-6
... friction and wear applications. It provides information on friction, types of wear, and lubrication. The article includes a brief description of the friction and wear test methods, laboratory-scale friction, and wear testing, usually performed either to rank the performance of candidate materials for an...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001302
EISBN: 978-1-62708-170-2
... Abstract Standardization, repeatability, convenience, short testing time, and simple measuring and ranking techniques are desirable in wear and erosion tests. This article provides a brief review of the wear testing methods and wear and erosion test equipment. General elements of a wear test...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003057
EISBN: 978-1-62708-200-6
.... The article describes testing methods such as room and high-temperature strength test methods, proof testing, fracture toughness measurement, and hardness and wear testing. It also explains methods for determining thermal expansion, thermal conductivity, heat capacity, and emissivity of ceramics and...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001296
EISBN: 978-1-62708-170-2
... salt spray test NaCl + CH 3 COOH Salted roads Copper-accelerated acetic acid salt spray test As in acetic acid salt spray test As in acetic acid salt spray test, but more aggressive Immersion tests Artificial sweat testWearing of decorative parts Immersion tests Solutions of HCl...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003025
EISBN: 978-1-62708-200-6
... anisotropic behavior. They can be used to modify properties and reduce shrinkage without causing property changes that are dependent on flow direction. The amount and type of reinforcement affect other properties. Glass fibers are very abrasive and tend to increase the wear and coefficient of friction of...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005683
EISBN: 978-1-62708-198-6
... forms as wear corrosion and erosion-corrosion. The mutual motion under load destroys the protective passive films, making the surfaces vulnerable to the corrosion attack, and the small gap between the surfaces creates occluded crevice corrosion conditions. An interaction with the environment is also...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006026
EISBN: 978-1-62708-172-6
... dispensed through the guide tube and against the coated surface; the reduction in coating thickness is then determined. Alternatively, the testing can continue until wear-through is visually evident, although this can be costly and time-consuming. Fig. 3 Falling abrasion tester. Courtesy of Humboldt...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006063
EISBN: 978-1-62708-172-6
... chemical attack by electrolytic, acidic, or caustic solutions; mechanical stress; wear; freeze-thaw; and the influence of electrical currents (such as cathodic disbonding). These and a host of other mechanisms are recreated in laboratory tests. Laboratory recreation of these stressors is desirable because...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003241
EISBN: 978-1-62708-199-3
... testing mechanical testing shear testing stress-strain curves tension testing torsion testing HARDNESS is a term that has different meanings to different people: it is resistance to penetration to a metallurgist, resistance to wear to a lubrication engineer, a measure of flow stress to a...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005677
EISBN: 978-1-62708-198-6
... under intraoral circumstances do not behave in this way; therefore, it is difficult to rank dental materials performance. Most wear tests have not faithfully predicted clinical performance. Wear information on dental materials has been collected from fundamental studies with simple laboratory tests...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005666
EISBN: 978-1-62708-198-6
... use in predicting excessive wear and pain. While many labs are now conducting this testing, few document the basic precautions needed to test serum metal in the parts per billion ranges (e.g., verifying that all digestion protocols and processing containers used for inductively coupled plasma mass...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003102
EISBN: 978-1-62708-199-3
... almost paper thin before fracturing. Pearlitic white cast iron, which has a hardness of about 400 to 450 HB, is equally brittle but less resistant to wear. Comparative tests on log washer lugs indicated that manganese steel was about 25% worn out with no breakage, whereas in the same period white...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003976
EISBN: 978-1-62708-185-6
... dies are typically of rather complex geometry. Therefore, the interface pressure and amount of relative sliding can vary from one area to another. Hence, characterization of abrasive wear in a systematic manner typically makes use of simulative tests of simple geometry. Most simple dies wear studies...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003104
EISBN: 978-1-62708-199-3
... Abstract Wear of metals occurs by plastic displacement of surface and near-surface material, and by detachment of particles that form wear debris. This article presents a table that contains the classification of wear. It describes the testing and evaluation of wear and talks about the abrasive...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005653
EISBN: 978-1-62708-198-6
... Abstract This article reviews the corrosion interactions between biomedical alloys, in particular iron-base, titanium-base, and cobalt-base alloys, in complex geometries and in applications where there are significant cyclic stresses and potential for wear and fretting motion. It discusses the...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003162
EISBN: 978-1-62708-199-3
... Abstract Hardfacing is defined as the application of a wear-resistant material, in depth, to the vulnerable surfaces of a component by a weld overlay or thermal spray process Hardfacing materials include a wide variety of alloys, carbides, and combinations of these materials. Iron-base...