1-20 of 345 Search Results for

wear ratio

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003102
EISBN: 978-1-62708-199-3
... (see Fig. 5 ). The wear rate for a quenched and tempered low-carbon low-alloy steel (ASTM 517, type B, at 269 HB), which was used as a comparative standard in each test, is also shown. When the relative wear rate (wear ratio) of each test material is plotted against increasing carbon content on a log...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005666
EISBN: 978-1-62708-198-6
... produce larger (micrometer-sized) wear debris that is more elongated in shape (aspect ratio > 2) ( Fig. 1 , 2 ). The particles produced by metal-on-polymer bearing implants are almost exclusively polymeric. Metallic debris can be produced by metal-on-polymer articulating implants but not typically...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006789
EISBN: 978-1-62708-295-2
... rolling-sliding conditions with different degrees of sliding, commonly indicated with the relevant slip ratio (percent difference in surface speeds). The most important parameter in determining the rolling-sliding wear of a mechanical part is the lubrication regime, which is expressed by the Λ-factor (Eq...
Book Chapter

Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006790
EISBN: 978-1-62708-295-2
... particle size, the wear rate decreases rapidly with decreasing particle size ( Ref 11 ). This particle size effect is usually attributed to the nature of the abrasive/wear material contact, with decreasing size favoring elastic rather than plastic contact. Abrasive hardness, or the ratio of hardness...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005678
EISBN: 978-1-62708-198-6
... (UHMWPE). The principal physical properties and tribological characteristics of these materials are summarized. The article discusses the pin-on-disk experiments and pin-on-plate experiments for determining friction and wear characteristics. It details the use of various types of joint simulators, such as...
Book Chapter

By Peter J. Blau
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003242
EISBN: 978-1-62708-199-3
... corrosion-related measurements Abrasive wear, 3-body G 65 Test Method for Measuring Abrasion Using the Dry Sand/Rubber Wheel Apparatus Mass loss G 81 Practice for Jaw Crusher Gouging Abrasion Test Mass loss ratio G 105 Test Method for Conducting Wet Sand/Rubber Wheel Abrasion Tests Mass loss...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003976
EISBN: 978-1-62708-185-6
... and velocity and interface pressures are important considerations. The hardness ratio (hardness of the abrasive/hardness of the surface) has a major influence on the amount of wear. Surface platings and coatings that increase surface hardness significantly reduce abrasive wear. Care must be taken in...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006793
EISBN: 978-1-62708-295-2
... Abstract Impact or percussive wear is defined as the wear of a solid surface that is due to percussion, which is a repetitive exposure to dynamic contact by another body. Impact wear, however, has many analogies to the field of erosive wear. The main difference is that, in impact wear...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003030
EISBN: 978-1-62708-200-6
... Abstract Tribology is the science and technology of interacting surfaces in relative motion or, the study of friction, wear, and lubrication. This article focuses on friction and wear processes that aid in the evaluation and selection of materials, for polymers and some composites used in...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005677
EISBN: 978-1-62708-198-6
... effective subgingival scaling and root planning in periodontal therapy. Cuttability is affected primarily by cutting forces, chip thickness ratios, chip form, and tool wear ( Ref 229 , Ref 230 , Ref 231 ). Edge quality may be evaluated by the angle between the two edge-forming contiguous surfaces, the...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006791
EISBN: 978-1-62708-295-2
... possible, with its polar/dispersion ratio depending on the surface energy of the formed material ( Ref 179 ). Adhesive wear is best eliminated by preventing the metal-to-metal contact of sliding surfaces, which is most effectively established by lubricating the contact and using a lubricant with the...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006829
EISBN: 978-1-62708-295-2
... Abstract Fretting is a wear phenomenon that occurs between two mating surfaces; initially, it is adhesive in nature, and vibration or small-amplitude oscillation is an essential causative factor. Fretting generates wear debris, which oxidizes, leading to a corrosion-like morphology. This...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004004
EISBN: 978-1-62708-185-6
... Abstract Cold heading is typically a high-speed process where a blank is progressively moved through a multi-station machine. This article discusses various cold heading process parameters, such as upset length ratio, upset diameter ratio, upset strain, and process sequence design. It describes...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003104
EISBN: 978-1-62708-199-3
... Abstract Wear of metals occurs by plastic displacement of surface and near-surface material, and by detachment of particles that form wear debris. This article presents a table that contains the classification of wear. It describes the testing and evaluation of wear and talks about the abrasive...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005339
EISBN: 978-1-62708-187-0
.... It illustrates the three broad categories of MMCs depending on the aspect ratio of the reinforcing phase. The categories include continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. The article discusses the two main classes...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003101
EISBN: 978-1-62708-199-3
... Abstract Ultrahigh-strength steels are designed to be used in structural applications where very high loads are applied and often high strength-to-weight ratios are required. This article discusses the composition, mechanical properties, processing, product forms, and applications of commercial...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005331
EISBN: 978-1-62708-187-0
... Abstract This article begins with a discussion on the effects of alloying and impurity elements on the properties of aluminum cast alloys and their chemical compositions. It describes various means of structural control, namely, chemistry control, control of element ratios based on the...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006640
EISBN: 978-1-62708-213-6
... OES, along with various types of emission sources commonly used for OES. Some of the processes involved in calibration and quantification of OES for direct solids analysis by the ratio method are then described. The article ends with a discussion on the applications of each type of emission sources...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003061
EISBN: 978-1-62708-200-6
... Abstract Structural applications for advanced ceramics include mineral processing equipment, machine tools, wear components, heat exchangers, automotive products, aerospace components, and medical products. This article begins with an overview of the wear-resistant applications and the...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003225
EISBN: 978-1-62708-199-3
... Abstract Analysis of the failure of a metal structure or part usually requires identification of the type of failure. Failure can occur by one or more of several mechanisms, including surface damage (such as corrosion or wear), elastic or plastic distortion, and fracture. This leads to a wide...