Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006048
EISBN: 978-1-62708-172-6
... Abstract This article describes the features, benefits and limitations of petrolatum and microcrystalline wax. It provides a detailed discussion on the steps to be followed before applying the various forms of the wax-based coatings. The wax-based coating forms include petrolatum...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006038
EISBN: 978-1-62708-172-6
... typically took place over the trench. For many years, the built-up coal tar and asphalt coatings were the predominant systems used on buried pipelines. Another popular system used petroleum-based wax coating reinforced with fiber mesh. These coatings accounted for nearly all of the protective coatings...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005255
EISBN: 978-1-62708-187-0
... foamed polystyrene patterns are frequently used in conjunction with relatively thin ceramic shell molds (such as the Replicast process). Waxes Wax is the preferred base material for most investment casting patterns, but blends containing only waxes are seldom used. Waxes are usually modified...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006519
EISBN: 978-1-62708-207-5
... on a casting produced in a monolithic mold. Investment casting uses an expendable/disposable pattern, typically made of wax and then coated with some type of slurry molding medium. The wax positive shape of the part is usually made from tooling mounted in some type of wax injection machine ( Fig. 1 ) ( Ref...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005253
EISBN: 978-1-62708-187-0
... (create/make) the part Introduce molten metal to the part in the selected casting process Investment Casting Investment casting uses an expendable/disposable pattern, typically made of wax and then coated with some type of slurry molding medium. The wax positive shape of the part is usually...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005256
EISBN: 978-1-62708-187-0
... of the investment casting process in terms of molding but with an expendable pattern made from high-quality expanded polystyrene (EPS) as in lost foam (instead of the lost wax pattern of investment casting). The EPS pattern is coated in ceramic slurry and then fired to produce the ceramic mold. The firing process...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005159
EISBN: 978-1-62708-186-3
... work operations require film strength in excess of that which is possible with solutions and emulsions, a paste, suspension, or coating may prove to be the best lubricant choice. Pastes may be oil- or water-base, pigmented or nonpigmented. Pigments include talc, mica, or similar inactive but effective...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003172
EISBN: 978-1-62708-199-3
... uniformly than hand application. Coating refractories are selected based on the metal being poured and the permeability desired. The carrier used in the slurry is usually water, because organic solvents attack the pattern material. The coating is dried thoroughly before the pattern is invested with sand...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001276
EISBN: 978-1-62708-170-2
... to control the amount of film being applied. Waxes Waxes also provide a barrier film that can be applied in a solvent cutback, which allows control of the coating weight, based on the amount of solids present, and facilitates application. After the solvent evaporates, a barrier film of lesser quantity...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006504
EISBN: 978-1-62708-207-5
... blasting is also used to prepare surfaces for organic or electroplated coatings. Ultrafine glass bead blasting is an alternative to wet blasting. Conditions for wet blasting of aluminum-base materials Table 3 Conditions for wet blasting of aluminum-base materials At a nozzle-to-work distance of 75...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002449
EISBN: 978-1-62708-194-8
... . Fig. 7 SGC process: (1) photomask exposure, (2) removal of uncured polymer, (3) coating with wax, (4) milling a flat surface, (5) coating the next polymer layer First, a thin layer of liquid photopolymer is deposited on a flat substrate. A photomask is generated that matches the cross section...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004126
EISBN: 978-1-62708-184-9
... Abstract This article focuses on the various coatings used on Department of Defense (DoD) systems. These include electroplated coatings; conversion coatings; supplemental oils, waxes, and lubricants; organic paint coatings; and other finishes such as vacuum deposits, mechanical plating, thermal...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001247
EISBN: 978-1-62708-170-2
... cast iron chemical analysis chromate conversion coating corrosion current density cyanide baths deposition rate drying electrodeposition hydrogen embrittlement plate thickness rinsing steel stripping toxicity Electrodeposits of cadmium are used to protect steel and cast iron against...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004141
EISBN: 978-1-62708-184-9
... and physical environments (acid rain, acid particulates, bird droppings), and they are also susceptible to damage by vandalism (graffiti, spray paint, theft). Windblown particles abrade sculptural details. Ultraviolet light and temperature extremes accelerate the breakdown of paints and other coating materials...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006297
EISBN: 978-1-62708-179-5
... with solid and brittle novolac resin (2 to 5%). The resin melts and coats the sand grains. An aqueous solution of 10 to 15% hexamethylenetetramine, based on the weight of the resin, is then added, together with calcium stearate as a lubricant. Stirring is continued while the mixture cools, so that every...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006551
EISBN: 978-1-62708-290-7
... are immediately flattened by a rotating roller as the print block moves along the x -axis. Wax-based MJ systems, such as those from Solidscape, have an incorporated machining tool that planes each layer. Both approaches provide a smooth surface for the deposition of the subsequent layer. To manufacture parts...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004213
EISBN: 978-1-62708-184-9
... enamel, wax, and asphalt coatings. With these coatings, the SCC is associated with coating disbondment and shielding of the CP current by the coating. The near-neutral-pH form of SCC is most prevalent on tape-coated pipelines, while high-pH SCC has occurred most frequently on coal-tar-coated pipelines...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005306
EISBN: 978-1-62708-187-0
.... Of necessity, the casting mold systems must be relatively inert to molten titanium. Proprietary lost wax ceramic shell systems were developed by the various foundries engaged in titanium casting. Usually, the face coats of the ceramic shells are made with the proprietary coatings, and conventional refractory...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005249
EISBN: 978-1-62708-187-0
... use, the preform pattern and other elements of the pattern assembly are coated or sprayed with a wax-silicone mixture to facilitate parting. Carbon dioxide gas is diffused into the mold material for hardening. One method of doing this consists of piercing the mold material in several locations...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003397
EISBN: 978-1-62708-195-5
... shape, which is most obvious on shallow slopes and curves. A most comprehensive classification of RP processes was proposed by J.P. Kruth ( Ref 1 ), in which the focus is on the initial state of the raw materials used, namely solid, liquid, and powder-based manufacture. Other sources for more detailed...