1-20 of 49 Search Results for

waterborne coatings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001325
EISBN: 978-1-62708-170-2
.... It describes their characteristics and limitations compared to conventional noncompliant materials. The article addresses the methods and products commonly used achieve regulatory compliance: waterborne coatings, exempt-solvent-based coatings, high-solids coatings, powder coating, and electro-deposition...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006044
EISBN: 978-1-62708-172-6
... between structure and properties when they are formulated into coatings, and how they are being used in coatings. The main discussion points are the differences between solventborne and waterborne technologies and some of the challenges in formulating and applying waterborne acrylic coatings. The article...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004125
EISBN: 978-1-62708-184-9
... is H; if it is ketimine, X is methyl or greater. In minor II, Y=X−2H; for example, if X is CH 3 , then Y is CH. Fig. 5 Schematic diagram of a resin micelle (approximately 120 nm in diameter) in a waterborne coating Fig. 10 Schematic diagram of the Sempen, a self-contained paint...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006077
EISBN: 978-1-62708-172-6
.... Motawie A.M. , Sherif M.H. , Badr M.M. , Amer A.A. , and Shehat A.S. , Synthesis and Characterization of Waterborne Epoxy Resins for Coating Application , Aust. J. Basic Appl. Sci ., Vol 4 ( No. 6 ), 2010 , p 1376 – 1382 5. Shechter L. , Wynstra J...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006071
EISBN: 978-1-62708-172-6
... in the formulation of the paint to control the transport and drying of the coating, the common term solvent-borne usually implies a formulation based on organic solvents. Though water is also a solvent, formulations that use water are usually referred to as “waterborne” or “water-based” coatings. In traditional...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006026
EISBN: 978-1-62708-172-6
.... The standard indicates that storage for one month at 52 °C (125 °F) simulates some of the effects of storage for six months at 23 °C (73 °F), so that the testing can be accelerated. Rating is assessed on a scale of 10 (none) to 0 (complete failure). When waterborne coatings are shipped during cold weather...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006011
EISBN: 978-1-62708-172-6
... waterborne polyurethane coatings. Photo used by permission of Bayer MaterialScience LLC Abstract Abstract Polyurethane is any polymer consisting of a chain of repeating organic units joined by urethane linkages. Polyurethane polymers are formed through step-growth polymerization by making a monomer...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006031
EISBN: 978-1-62708-172-6
... with these finishes, provided formulators develop their coatings from high-quality pigments and additives. Solvent-based, waterborne, and powder-coating-bakeable formulations are available for use on metal substrates. Low-temperature-bake and air-dry formulations have recently been developed for use on heat...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006009
EISBN: 978-1-62708-172-6
... when using polyesters and vinyl esters. automotive paints chemical resistance industrial paints polyester coating polymerization powder coating unsaturated polyester resins vinyl ester resins waterborne paints POLYESTER AND VINYL ESTER resin-based linings are known for their solvent...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006041
EISBN: 978-1-62708-172-6
... of FEVE resins with cross linkers such as melamine formaldehyde and polyisocyanate. The FEVE resins are available as solution resins, solids resins for powder coatings, and waterborne resins. The fluoroethylene groups are the strength of the FEVE resin. These groups are what make this class...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006006
EISBN: 978-1-62708-172-6
... Is It a Coating or Is It a Lining? Alkyd Epoxy Waterborne Acrylics Urethane Nonskid Paints Intumescent Coatings Railcar owners generally are aware that a good blast at the outset adds greatly to the performance of a paint system. Virtually all freight cars are abrasive blasted, probably...
Book Chapter

By Barry Law
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006060
EISBN: 978-1-62708-172-6
... coatings, excluding industrial maintenance (IM) coatings 50 Solvent-based IM 600 Waterborne IM 50 Note: Limits are in grams of volatile organic compound (VOC) per liter of colorant, less water and less exempt compounds. Effective January 1, 2014 (Rule 1113 amended September 6, 2013...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006028
EISBN: 978-1-62708-172-6
... Therefrom , U.S. Patent 5,449,716 , Sept 12 , 1995 Zinc-Rich Primers Solvent-Borne Primers Waterborne Primers Chromium Replacement Ablative Marine Coatings Marine Fouling Release Chemistry Uses Of Alkoxy Silanes Silicates and Siliconates Silicone Fluids Silicone...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004162
EISBN: 978-1-62708-184-9
...: Understanding Rust , Mach. Des. , Oct 7 , 1976 , p 108 – 113 ; Part II: Resisting Rust , Mach. Des. , Nov 11 , 1976 , p 146 – 152 6. Kargol J.A. et al. , The Influence of High Strength Cold Rolled Steel and Zinc Coated Steel Surface Characteristics on Phosphate Pretreatment...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004127
EISBN: 978-1-62708-184-9
..., Waterborne,” MIL-PRF-85582, U.S. Department of Defense , 2002 9. “Coating: Polyurethane, Aircraft and Support Equipment,” MIL-PRF-85285, U.S. Department of Defense , 2002 Selected References Selected References • Aircraft Weapons Systems Cleaning and Corrosion Control , NAVAIR 01-1A...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006050
EISBN: 978-1-62708-172-6
... floor coatings is available to protect and beautify floors, to provide a surface that is easily cleaned, and one that possesses the desired wet and dry slip-resistance properties. Epoxy coatings include waterborne, solventborne, and 100% solids. They provide good abrasion and chemical resistance...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004204
EISBN: 978-1-62708-184-9
... Design Service or Operating Temperature Insulation Materials Protective Coatings Weatherproofing and Vaporproofing Polytetrafluoroethylene (PTFE) Perfluoroalkoxytetrafluoroethylene (PFA) Fluorinated Ethylene Propylene (FEP) Ethylene-Chlorotrifluoroethylene (ECTFE...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006072
EISBN: 978-1-62708-172-6
... √ √ … Inorganic zinc-rich primer/waterborne acrylic √ … … Organic zinc-rich primer/waterborne acrylic … √ … Thermal spray coating/sealer √ √ … Epoxy sealer/epoxy mastic/acrylic polyurethane or polyaspartic … … √ Epoxy mastic/acrylic polyurethane … … √ Epoxy mastic/waterborne acrylic...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006051
EISBN: 978-1-62708-172-6
...Particle shape and coating film properties of pigments Table 1 Particle shape and coating film properties of pigments Particle shape Benefit Usage Pigment type Platey Barrier properties Corrosion resistance Bleed and stain killing Enamel holdout TiO 2 extension (spacers) in high...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003366
EISBN: 978-1-62708-195-5
... with either solvent or waterborne phenolic resole resins ( Ref 17 ). There is no alternate resin that meets the adhesion, low flammability, and processing requirements of Nomex honeycomb. For aerospace honeycomb applications, the honeycomb phenolic resin should meet requirements, such as those specified...