Published: 01 November 1995
Fig. 48 BPA vinyl ester resin More
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006009
EISBN: 978-1-62708-172-6
... Abstract This article provides a discussion on polyester coating applications such as powder coatings, can coatings, and automotive paints. It includes an overview, structure, properties, and benefits of vinyl ester resins. The article discusses the additives for both unsaturated polyester...
Book Chapter

By Tim Pepper
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003363
EISBN: 978-1-62708-195-5
... Abstract This article provides an overview of the various types of unsaturated polyester resins and low-profile additives. The resins include general-purpose resins, isophthalic resins, bisphenol A fumarate resins, chlorendic resins, and vinyl ester resin. The article describes the mechanical...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003031
EISBN: 978-1-62708-200-6
... Abstract This article discusses the types, properties, and uses of continuous-fiber-reinforced composites, including glass, carbon, aramid, boron, continuous silicon carbide, and aluminum oxide fiber composites. While polyester and vinyl ester resins are the most used matrix materials...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003406
EISBN: 978-1-62708-195-5
... and spray-up process. Workmanship for hand lay-up and spray-up processes is reviewed. The article provides information on the matrix-resin materials used for open molding, including unsaturated polyester resins, epoxy vinyl ester resins, and reinforcements. It explains the component design and short...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003036
EISBN: 978-1-62708-200-6
..., and autoclave molding - suited for making parts on open-faced molds using polyester and vinyl ester resins. The article also provides information on mechanically assisted lay-up which can be automated to alleviate some of the manual work. autoclave molding contact molding hand lay-up mechanical...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003845
EISBN: 978-1-62708-183-2
... Abstract This article describes the resin and fabrication requirements associated with fiberglass-reinforced plastic equipment. It provides a discussion on various resins and their resistance to various environments. These include polyester, epoxy, epoxy vinyl-ester, and furan and phenolic...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003010
EISBN: 978-1-62708-200-6
... the general and family characteristics of thermosetting resin families, including allyls, aminos (urea formaldehyde and melamine formaldehyde), cyanates, epoxies, polybenzimidazoles, unsaturated polyesters, thermoset polyimides, phenolics, and vinyl esters. It also explains processing methods, including...
Image
Published: 30 September 2015
Fig. 20 Vinyl ester prepared by diglycidyl ether of bisphenol A epoxy resin and methacrylic acid More
Image
Published: 01 November 1995
Fig. 50 Vinyl ester polymerization. R , backbone of epoxy resin More
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003038
EISBN: 978-1-62708-200-6
... in the transverse and longitudinal directions. More than 90% of all pultruded products are fiberglass-reinforced polyester. When better corrosion resistance is required, vinyl ester resins are used. When a combination of superior mechanical and electrical properties is required, epoxy resin is used. Higher...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003417
EISBN: 978-1-62708-195-5
... on fiberglass reinforced polyester resin. When better corrosion resistance is required, vinyl ester resins are used and represent the next largest product segment. Both of these resin types are also available as flame-retardant versions. When a combination of superior mechanical and electrical properties...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003356
EISBN: 978-1-62708-195-5
... mixture will reduce the renewable resource content of the final resin, they should result in higher T g values for the end polymer. The synthesis of maleate half-esters of organic polyols, including NPG and BPA, and the cross linking of the resulting maleate half- esters with a vinyl monomer...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004137
EISBN: 978-1-62708-184-9
... application in which temperatures do not exceed 120 °C (250 °F) (preferably 95 °C, or 205 °F), regardless of whether there are high chlorides or low pHs. The best choices would be premium grades of vinyl-ester and polyester resins. Polypropylene, chlorinated polyvinyl chloride (CPVC), and other thermoplastics...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003692
EISBN: 978-1-62708-182-5
... Thermosetting, or cross-linking, acrylics can be obtained by combining the methacrylate or acrylate esters with reactive nonacrylic polymers. The most common cross-linking agents in use are the epoxy resins, the urea or melamine-formaldehyde resins, and the vinyl resins. Generally, the nonacrylic polymer...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003020
EISBN: 978-1-62708-200-6
... physical properties, but at a premium price. Vinyl ester resin has also been used in a number of RTM products and provides properties between those of polyester and epoxy at a moderate price. Other resin systems, such as the acrylamate resin system family and methylmethacrylate vinyl ester, are newer...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003398
EISBN: 978-1-62708-195-5
...-references resin systems with performance and processing methods to aid the selection of resin systems. Comparison of resin system performance and processing characteristics Table 6 Comparison of resin system performance and processing characteristics Attribute Polyester Vinyl ester Epoxy...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003403
EISBN: 978-1-62708-195-5
...- reinforced elastomeric products are available for use in flexible and semirigid tool fabrication. Resin temperature comparison Table 2 Resin temperature comparison Resin Cure temperature Service temperature °C °F °C °F Polyester RT–121 RT–250 60–140 140–285 Vinyl ester RT RT...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003366
EISBN: 978-1-62708-195-5
... spread index and smoke density comparison of thermosetting resins (ASTM E 84 tunnel test) Resin Flame spread index Smoke density Phenolic 10 10 Halogenated polyester 15 600–800 Halogenated vinyl ester 45 600–800 Methacrylate vinyl ester with 150 phr aluminum trihydrate 20 40...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006071
EISBN: 978-1-62708-172-6
... paint driers protective coatings waterborne paints AN ALKYD is an ester-based polymer derived from the polycondensation reaction of a polyhydric alcohol and a polybasic acid. In addition to these ingredients, the resulting resin is modified with an oil or a fatty acid to make it more flexible...