By Arlen Hoebergen, J. Anders Holmberg
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003414
EISBN: 978-1-62708-195-5
... Abstract Vacuum infusion is a resin injection technique derived from resin transfer molding. This article discusses the characteristics of the technique and its applications. It presents the theory and background of the technique and provides an illustration of how parts are made. The article...
Image
Published: 01 December 2004
Fig. 9 Vacuum infusion apparatus used for removing entrapped air in the mounting resin before it is added to the mold. In this apparatus, vacuum is maintained in the chamber. The mold is placed under the chamber, and a tube for resin transport is placed above the sample that connects More
Image
Published: 01 January 2001
Fig. 3 Contest 55 sailing yacht with hull manufactured by vacuum infusion. Courtesy of Conyplex Shipyard, Medemblik, the Netherlands More
Image
Published: 01 January 2001
Fig. 6 Vacuum infusion of a 3.2 × 12 m (10.5 × 39 ft) glass fiber/vinyl ester sandwich illustrating the technique for creating a hull panel for the corvette shown in Fig. 7 . Courtesy of Kockums Shipyard, Karlskrona, Sweden More
Image
Published: 01 January 2001
Fig. 23 Schematic of a basic vacuum infusion setup More
Image
Published: 01 January 2001
Fig. 5 Vacuum infused 5.1 m (17 ft) boat hull More
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003413
EISBN: 978-1-62708-195-5
... that use hard tooling and positive (superatmospheric) pressures to produce structures. The techniques include vacuum-assisted resin injection, vacuum infusion, resin-film infusion, and injection-compression molding. The article provides an overview of the materials that are commonly used together with some...
Book Chapter

By Shahid P. Qureshi
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003366
EISBN: 978-1-62708-195-5
... Abstract This article describes the chemistry of phenolic resins and reviews their characteristics and properties for various composites fabrication processes. The fabrication processes include solution/hot-melt process, pultrusion, vacuum infusion, filament winding, sheet molding, and hand lay...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003401
EISBN: 978-1-62708-195-5
... covered in the present edition also were described in the 1987 edition, some techniques now covered are new (vacuum infusion and several thermoplastic techniques), and a couple that previously were reported as representing recent developments are now well established (fiber placement and tape laying...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009071
EISBN: 978-1-62708-177-1
... transfer molding, vacuum-assisted resin transfer molding, and resin film infusion. It explains the composite- and matrix-toughening methods for fiber-reinforced composites, such as dispersed-phase toughening and interlayer toughening. The article concludes with information on optical microscopy, which...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009072
EISBN: 978-1-62708-177-1
.... Although this increases the cure speed, it also leads to greater cure shrinkage of the mounting resin. To ensure complete impregnation of the specimens, the mold can be placed in a vacuum chamber while infusing the resin ( Fig. 9 ). This is essentially a bell jar with a vacuum and resin port and a pinch...
Book Chapter

By A.P. Mouritz, R.S. Trask, A.J. Russell
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003454
EISBN: 978-1-62708-195-5
.... The laminating process used in the repair should be similar to that used for original construction of the ship laminate to ensure the repair material has the same fiber-to-resin ratio as the original structure. In other words, a ship laminate originally made using vacuum bagging or resin infusion should...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003407
EISBN: 978-1-62708-195-5
... of the foam materials may also be excluded, due to interaction with styrene under vacuum. Reinforcements need to be designed to assist flow through the laminate during infusion, and consequently, tight, highly anisotropic unidirectional tapes are not favored. Reinforcements Despite the apparent drive...
Book Chapter

By Vistasp M. Karbhari
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003482
EISBN: 978-1-62708-195-5
... and/or squeegees. The composite and bond are formed at the same time. Slower and needs more set-up Vacuum infusion Reinforcing fabric is placed over the area under consideration and the entire area is encapsulated in a vacuum bag. Resin is infused into the assembly under vacuum with compaction taking place...
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0005754
EISBN: 978-1-62708-195-5
... conductiv- NOL Naval Ordnance Laboratory Ref reference No. number RFI resin- lm infusion ity NPG neopentyl glycol RGA residual gas analysis K Kelvin OD outside diameter RH relative humidity K coef cient of thermal conductivity; bulk OEM original equipment manufacturer RI refractive index OHC open-hole...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003395
EISBN: 978-1-62708-195-5
... “Resin Transfer Molding and Structural Reaction Injection Molding,” , “Vacuum Infusion,” and “Compression Molding” in this Volume. Preimpregnated Tapes and Fabrics Laminated preimpregnated materials often offer the greatest mechanical properties. High specific strength and stiffness...
Book Chapter

By Grover Aaron Henson, III
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003431
EISBN: 978-1-62708-195-5
... affordability, out-of-autoclave curing has become a common goal. Processes such as vacuum-assisted resin transfer molding, resin transfer molding, electron beam curing, room- temperature curing, oven curing, and resin-fiber infusion are being adopted to meet the new affordability objectives. The tooling...
Book Chapter

By John D. Russell
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003432
EISBN: 978-1-62708-195-5
... to document the presence of each ingredient and to ensure that the proper chemical reaction state has been obtained. These resins can be used to make preimpregnated reinforcing fibers (prepreg) or to infiltrate a fiber preform via resin transfer molding, vacuum assisted resin transfer molding, or resin film...
Book Chapter

By John Bootle, Frank Burzesi, Lynda Fiorini
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003398
EISBN: 978-1-62708-195-5
... out. Once a good vacuum is achieved, resin is infused into the part. Balsa or foam cores are typically used; honeycomb core cannot be used. Because VARTM uses continuous fibers and is cured under typical vacuum pressure of 84 MPa (25 in. of mercury), the resulting laminate is very high quality...