EISBN: 978-1-62708-180-1
... Abstract This article reviews the abrasive and adhesive wear failure of several types of reinforced polymers, including particulate-reinforced polymers, short-fiber reinforced polymers (SFRP), continuous unidirectional fiber reinforced polymers (FRP), particulate-filled composites, mixed...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003453
EISBN: 978-1-62708-195-5
... Technologies, Inc. Fig. 5 Portable oven (Robo-Curing System) for curing columns wound from prepreg carbon tows. Courtesy of XXsys Technologies, Inc. Fig. 9 Flexural condition based upon ultimate compressive strain of the concrete ε C . b FRP = width of composite. The other terms...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003482
EISBN: 978-1-62708-195-5
... on Advanced Composite Materials Bridges ( Washington, D.C. ), May 1997 10. Taljsten B. , “Plate Bonding,” doctoral thesis, Lulea University of Technology, Sweden, 1994 11. Saadatmanesh H. and Ehsani M.R. , RC Beams Strengthened with FRP Plates I: Experimental Study...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003452
EISBN: 978-1-62708-195-5
... for the situation ( Ref 5 ). Materials that have been used effectively include boron/epoxy and graphite/epoxy composites (fiber-reinforced plastics, FRP), GLARE (a laminated metallic material reinforced with glass fibers in an adhesive layer), and conventional metallic materials. Fiber-reinforced plastic materials...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003267
EISBN: 978-1-62708-176-4
... for three principal groups of engineering materials: metals, ceramics, and polymers (including fiber-reinforced polymer, or FRP composites). An excellent source for an in-depth coverage of material properties at low temperatures is Ref 2 . Tensile and compression tests produce engineering data...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003351
EISBN: 978-1-62708-195-5
... for the bulk of the fiber-reinforced plastics (FRP) market. Polyesters offer a combination of low cost, versatility in many processes, and reasonably good property performance unmatched by any other resin type. The most common orthophthalic types and the premium isophthalic types, bisphenol A fumarate...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003417
EISBN: 978-1-62708-195-5
... FRP pultrusions  50% wt mat and roving 242 35 17.2 2.5 242 35  70% wt unidirectional roving 690 100 41.4 6.0 690 100 Metals  Aluminum 280 40 70 10 280 40  Steel 690 100 210 30 690 100 Source: Ref 4 Equivalent thickness factor of FRP fabricated...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003381
EISBN: 978-1-62708-195-5
...-Change Analysis of the Interphase in Hygrothermally Aged FRP: Considerations of Debonding , Compos. Sci. Technol. , Vol 57 , 1997 , p 985 – 990 • Mukhopadhyay A.K. and Sierakowski R.L. , On the Thermoelastic and Hygrometric Response of Sandwich Beams with Laminate Facings...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003353
EISBN: 978-1-62708-195-5
... in a press and molded into parts. Many fiber-reinforced plastic (FRP) automotive body panels are made by this process. Filament winding and pultrusion are processes that use single-end rovings in continuous form. Applications include pipes, tanks, leaf springs, and many other structural composites...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.9781627081955
EISBN: 978-1-62708-195-5
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003010
EISBN: 978-1-62708-200-6
...% of the total composition. General Characteristics Thermoset engineering plastics compete with metals, ceramics, and engineering thermoplastics. Compared with metals, they possess corrosion resistance, lighter weight, and sound and thermal insulating properties, and they can be processed at lower...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006433
EISBN: 978-1-62708-192-4
... Abstract Solid particle erosion (SPE) is the loss of material that results from repeated impact of solid particles energized in a carrier fluid. This article reviews important SPE variables, their effects for different classes of materials, composites and coatings, and the mechanisms...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.9781627082006
EISBN: 978-1-62708-200-6
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0001834
EISBN: 978-1-62708-181-8