1-20 of 316 Search Results for

ultrasonic atomization

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006084
EISBN: 978-1-62708-175-7
... and research methods. This article describes the key process variables and production factors for the industrial methods: two-fluid, centrifugal, vacuum or soluble-gas, and ultrasonic atomization. It also reviews the effect of atomization methods and process variables on key powder characteristics...
Image
Published: 30 September 2015
Fig. 15 Ultrasonic gas atomizer (U.S. t 2,997,245) More
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002363
EISBN: 978-1-62708-193-1
... emission techniques, ultrasonic methods, eddy current techniques, infrared techniques, exoelectron methods, and gamma radiography. The article explains the microscopy methods used to determine fatigue crack initiation and propagation. These include electron microscopy, scanning tunneling microscopy, atomic...
Series: ASM Handbook Archive
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000631
EISBN: 978-1-62708-181-8
... oxygen environment exposure effect, solar cell interconnect, integrated circuit defects, and fatigue failure of these materials. electronic materials fatigue failure fractograph integrated circuits ultrasonic cleaning Fig. 1326, 1327 Effect of exposure to the atomic oxygen environment...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006574
EISBN: 978-1-62708-290-7
... Atom probe tomography ( Ref 43 , 50 ) Understand the role of oxide dispersion during ultrasonic additive manufacturing Sometimes (especially when the parameters are not optimized) the demarcation between individual layers becomes more apparent, with voids and unbonded regions. This is evident...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003209
EISBN: 978-1-62708-199-3
... Abstract This article describes the mechanism, advantages and disadvantages, fundamentals, capabilities, variations, equipment used, and weldability of metals in solid-state welding processes, including diffusion bonding, explosion welding, friction welding, ultrasonic welding, upset welding...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005619
EISBN: 978-1-62708-174-0
... Abstract Ultrasonic welding (UW), as a solid-state joining process, uses an ultrasonic energy source and pressure to induce oscillating shears between the faying surfaces to produce metallurgical bonds between a wide range of metal sheets and wires. This article reviews the models...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003057
EISBN: 978-1-62708-200-6
.... Chemical analysis is carried out by X-ray fluorescence spectrometry, atomic absorption spectrophotometry, and plasma-emission spectrophotometry. Phase analysis is done by X-ray diffraction, spectroscopic methods, thermal analysis, and quantitative analysis. Techniques used for microstructural analysis...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006065
EISBN: 978-1-62708-175-7
... and centrifugal atomization, ultrasonic or pulsed atomization, melt spinning with attrition, and mechanically alloying. Gas atomization is used for several applications. In gas atomization, a high-velocity gas jet disintegrates molten aluminum into droplets that solidify to form the powder. In the Alcoa...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006470
EISBN: 978-1-62708-190-0
... performance. General Characteristics of Ultrasonic Waves Ultrasonic waves are mechanical waves (in contrast to, for example, light or x-rays, which are electromagnetic waves) that consist of oscillations or vibrations of the atomic or molecular particles of a substance about the equilibrium positions...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001472
EISBN: 978-1-62708-173-3
... of top-surface or root reinforcement affects the sensitivity of inspection, and the presence of foreign material, such as loose scale, flux, or weld spatter, may interfere with the interpretation of results. Ultrasonic inspection is capable of detecting subsurface porosity. However...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003236
EISBN: 978-1-62708-199-3
... in ordinary pulse-echo testing. General Characteristics of Ultrasonic Waves In contrast to electromagnetic waves, such as light and x-rays, ultrasonic waves are mechanical waves consisting of oscillations, or vibrations, of the atomic or molecular particles of a substance about the equilibrium position...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006557
EISBN: 978-1-62708-290-7
... or ceramic powders into bulk materials with improved mechanical strength, although in most cases, residual porosity results. The steps of solid-state sintering consist of solid-state atomic diffusion, recrystallization, and grain growth, while six different mechanisms are involved with mass transfer...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003436
EISBN: 978-1-62708-195-5
... Abstract This article introduces the principal methodologies and some technologies that are being applied for nondestructive evaluation of composite materials. These include ultrasonic testing (UT), air-coupled UT, laser UT, ultrasonic spectroscopy, leaky lamb wave method, acousto-ultrasonics...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006478
EISBN: 978-1-62708-190-0
... Abstract This article introduces the principal methodologies and some advanced technologies that are being applied for nondestructive evaluation (NDE) of fiber-reinforced polymer-matrix composites. These include acoustic emission, ultrasonic, eddy-current, computed tomography, electromagnetic...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006446
EISBN: 978-1-62708-190-0
... Abstract Nonlinear ultrasonic nondestructive examination (NDE) techniques are based on nonlinear interaction of ultrasonic waves with the material to be characterized and defects to be detected. This article introduces the basic principles of nonlinear material-wave interaction, the origin...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.9781627081900
EISBN: 978-1-62708-190-0
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006473
EISBN: 978-1-62708-190-0
... Abstract This article discusses the inspection/reference standards that are absolutely critical for proper application of ultrasonic inspection systems. Many of the standards and specifications for ultrasonic inspection require the use of standard reference blocks. The article lists...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006647
EISBN: 978-1-62708-213-6
... Abstract This article provides a clear but nonexhaustive description of the general principle of atomic emission, with a particular focus on instrumentation, and summarizes the main characteristics of the inductively coupled plasma optical emission spectrometer technique. Basic atomic theory...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0001730
EISBN: 978-1-62708-178-8
... of sample are available, fritted disk or ultrasonic nebulizers are preferable to conventional pneumatic types because they produce a spray with a finer mean droplet size. For the more easily atomized elements, such as lead and cadmium, the air-acetylene flame is preferred because it is less expensive...