Skip Nav Destination
Close Modal
By
Lisa Pruitt, Amy Wat, Louis Malito
Search Results for
ultrahigh molecular weight polyethylene
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 120
Search Results for ultrahigh molecular weight polyethylene
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Comparison of ultrahigh molecular weight polyethylene (UHMWPE) pin wear fro...
Available to Purchase
in Environmental and Application Factors in Solid Friction
> Friction, Lubrication, and Wear Technology
Published: 31 December 2017
Fig. 6 Comparison of ultrahigh molecular weight polyethylene (UHMWPE) pin wear from uniaxial reciprocating motion at 2 Hz ( Fig. 3d ) and crossing motion at cycle rates of 1 and 2 Hz ( Fig. 3e ) for 2-million cycles. Source: Ref 37
More
Image
SEM fractographs of ultrahigh-molecular-weight polyethylene, showing the fr...
Available to PurchasePublished: 15 May 2022
Fig. 23 SEM fractographs of ultrahigh-molecular-weight polyethylene, showing the fracture surface of a specimen fracture in slow bending at ambient temperature. The direction of crack propagation is from left to right. (a) At low magnification showing layered fracture with mixture of coarse
More
Image
SEM fractographs of ultrahigh-molecular-weight polyethylene, showing the fr...
Available to PurchasePublished: 15 May 2022
Fig. 24 SEM fractographs of ultrahigh-molecular-weight polyethylene, showing the fracture surface of a specimen fracture under impact testing at ambient temperature. The direction of crack propagation is from left to right. (a) Flat fracture. Original magnification: 250×. (b) Flat fracture
More
Book Chapter
Fatigue and Fracture Mechanisms in Polymers
Available to PurchaseSeries: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006918
EISBN: 978-1-62708-395-9
... engineering polymers. The article describes fracture mechanics solutions and approaches to the fatigue characterization of engineering polymers when dealing with macroscale fatigue crack growth. It includes mechanistic images for high-density polyethylene, ultrahigh-molecular-weight polyethylene, nylon 6, 6...
Abstract
This article reviews generalized test methodologies for fatigue characterization of polymers and examines fatigue fracture mechanisms in different engineering plastics. It provides detailed micromechanistic images of crack-tip processes for a variety of semicrystalline and amorphous engineering polymers. The article describes fracture mechanics solutions and approaches to the fatigue characterization of engineering polymers when dealing with macroscale fatigue crack growth. It includes mechanistic images for high-density polyethylene, ultrahigh-molecular-weight polyethylene, nylon 6, 6, polycarbonate, and polypropylene. The article describes the micromechanisms of toughening of plastics and uses a macroscale approach of applying fracture mechanics to the fatigue life prediction of engineering polymers, building on the mechanistic concepts. It also describes the factors affecting fatigue performance of polymers.
Book Chapter
Friction and Wear of Medical Implants and Prosthetic Devices
Available to PurchaseSeries: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005678
EISBN: 978-1-62708-198-6
... Abstract Total joint replacement in orthopedic surgery can be achieved by excision, interposition, and replacement arthroplasty. This article details the most common materials used in total replacement synovial joints: metals, ceramics, and ultrahigh molecular weight polyethylene (UHMWPE...
Abstract
Total joint replacement in orthopedic surgery can be achieved by excision, interposition, and replacement arthroplasty. This article details the most common materials used in total replacement synovial joints: metals, ceramics, and ultrahigh molecular weight polyethylene (UHMWPE). The principal physical properties and tribological characteristics of these materials are summarized. The article discusses pin-on-disk experiments and pin-on-plate experiments for determining friction and wear characteristics. It explains the use of various types of joint simulators, such as hip joint simulators and knee joint simulators, to evaluate the performance of engineering tribological components in machine simulators. The article concludes with a section on the in vivo assessment of total joint replacement performance.
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005659
EISBN: 978-1-62708-198-6
... Abstract This article provides a summary of the biocompatibility or biological response of metals, ceramics, and polymers used in medical implants, along with their clinical issues. The polymers include ultrahigh-molecular-weight polyethylene, nonresorbable polymer, and resorbable polymers...
Abstract
This article provides a summary of the biocompatibility or biological response of metals, ceramics, and polymers used in medical implants, along with their clinical issues. The polymers include ultrahigh-molecular-weight polyethylene, nonresorbable polymer, and resorbable polymers.
Image
Specific wear rate for several polymers as reported in the literature. The ...
Available to PurchasePublished: 15 May 2022
, polyethylene; PEEK, polyetheretherketone; PMMA, polymethyl methacrylate; PTFE, polytetrafluoroethylene; UHMWPE, ultrahigh-molecular-weight polyethylene.
More
Image
Electrical properties of triboelectric materials. Materials near the positi...
Available to Purchase
in Additively Manufactured Biomedical Energy Harvesters
> Additive Manufacturing in Biomedical Applications
Published: 12 September 2022
Fig. 1 Electrical properties of triboelectric materials. Materials near the positive direction release electrons, and those near the negative direction gain electrons. EVA, ethylene-vinyl acetate; LDPE, low-density polyethylene; HDPE, high-density polyethylene; UHMWPE, ultrahigh-molecular
More
Image
Schematic diagram of artificial hip joint. UHMWPE, ultrahigh-molecular-weig...
Available to PurchasePublished: 01 June 2012
Fig. 15 Schematic diagram of artificial hip joint. UHMWPE, ultrahigh-molecular-weight polyethylene
More
Image
Typical polymers used in powder-bed fusion additive manufacturing technique...
Available to PurchasePublished: 12 September 2022
, polyetherketone; PEEK, polyetheretherketone; UHMWPE, ultrahigh-molecular-weight polyethylene; PE, polyethylene; PET, polyethylene terephthalate; PA, polyamide. T m , melting temperature; T f , fictive temperature, T g , glass transition temperature
More
Image
Generic types of transfer wear behavior when semicrystalline polymers are s...
Available to PurchasePublished: 15 May 2022
properties of the polymer and the surface topography of the counterface. PE, polyethylene; PTFE, polytetrafluoroethylene; UHMWPE, ultrahigh-molecular-weight polyethylene. Reprinted with permission from Ref 1
More
Image
Fatigue plot illustrating the devastating effect of gamma radiation sterili...
Available to PurchasePublished: 01 January 2000
Fig. 15 Fatigue plot illustrating the devastating effect of gamma radiation sterilization on the fatigue resistance of orthopedic grade ultrahigh molecular weight polyethylene used for total joint replacements
More
Image
Friction coefficients of a calcium phosphate coating (deposited on a steel ...
Available to PurchasePublished: 01 June 2012
Fig. 20 Friction coefficients of a calcium phosphate coating (deposited on a steel substrate) when sliding against an ultrahigh-molecular-weight polyethylene pin at various sliding speeds and in both dry and lubricated conditions
More
Image
Wear behavior of various femoral head/cup combinations. Even higher ultrahi...
Available to PurchasePublished: 01 June 2012
Fig. 13 Wear behavior of various femoral head/cup combinations. Even higher ultrahigh-molecular-weight polyethylene (UHMWPE) wear rates are encountered with titanium-base femoral heads. Source: Ref 8
More
Image
Artificial hip joint on which titanium (Ti) and hydroxyapatite (HA) coating...
Available to Purchase
in Biomedical Coatings Made by Thermal Spraying for Orthopaedic Joint Applications
> Thermal Spray Technology
Published: 01 August 2013
Fig. 1 Artificial hip joint on which titanium (Ti) and hydroxyapatite (HA) coatings were applied by plasma spraying for promotion of bone growth. UHMWPE, ultrahigh-molecular-weight polyethylene. Courtesy of Stryker Howmedica Osteonics
More
Image
Overview of typical wear particle sizes versus wear rates reported for vari...
Available to PurchasePublished: 31 December 2017
Fig. 11 Overview of typical wear particle sizes versus wear rates reported for various acetabular liners used in total hip replacement (THR). Data is presented based on (a) the volumetric wear rate and (b) wear particle generation rate. PCU, polycarbonate-urethane; UHMWPE, ultrahigh molecular
More
Image
Implant debris from two types of materials. The metal (cobalt alloy) is mor...
Available to PurchasePublished: 01 June 2012
Fig. 1 Implant debris from two types of materials. The metal (cobalt alloy) is more rounded versus the polymeric (ultrahigh-molecular-weight polyethylene, or UHMWPE) debris, which is more elongated in shape. Metal debris can be produced at modular connections of implants, at articulating
More
Image
Examples of pneumatic seals shown on the left and their housings on the rig...
Available to PurchasePublished: 31 December 2017
Fig. 8 Examples of pneumatic seals shown on the left and their housings on the right. (a) Single-acting, polyurethane rod seal with U-shaped cross section. (b) Double-acting rod seal, comprising an ultrahigh-molecular-weight-polyethylene (UHMWPE) slipper seal and an energizing acrylonitrile
More
Image
Typical components found in an unassembled total hip replacement (THR) impl...
Available to PurchasePublished: 01 June 2012
Fig. 11 Typical components found in an unassembled total hip replacement (THR) implant. It should be noted that this is one of many artificial joint designs used in THR arthroplasty. For example, implants secured by bone cements would not be porous coated. Similarly, the ultrahigh-molecular
More
Image
SEM fractographs of fatigue fracture surface of ultrahigh-molecular-weight ...
Available to PurchasePublished: 15 May 2022
Fig. 26 SEM fractographs of fatigue fracture surface of ultrahigh-molecular-weight polyethylene, using compact-tension specimens in the Paris regime. Direction of crack growth indicated by the white arrows. (a) Sterilized specimen tested at ambient temperatures. Original magnification: 1000