1-5 of 5 Search Results for

ultra supercritical power plants

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004133
EISBN: 978-1-62708-184-9
...Candidate alloys for ultra supercritical power plant boilers Table 1 Candidate alloys for ultra supercritical power plant boilers Trade designation ASME code/code case Preferred application (a) Metal temperature of application (b) , °C Ferritic steels HCM2S 2199 WW ≤575...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... power plant classifications Nomenclature Steam conditions Net plant efficiency (higher heating value), % Subcritical 16.5 MPa (2400 psig), 540–565 °C (1000–1050 °F) 35 Supercritical >24.8 MPa (3600 psig), ~565–600 °C (1050–1110 °F) 38 Ultrasupercritical >24.8 MPa (3600...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.9781627082006
EISBN: 978-1-62708-200-6
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.9781627082136
EISBN: 978-1-62708-213-6
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.9781627081788
EISBN: 978-1-62708-178-8