EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data tungsten binary system THIS ARTICLE includes systems where tungsten is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006178
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data molybdenum binary system phase data THIS ARTICLE includes systems where molybdenum is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006172
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data iridium binary system phase data THIS ARTICLE includes systems where iridium is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006147
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which boron (B) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006193
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data palladium binary system phase data THIS ARTICLE includes systems where palladium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006157
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams chromium binary system crystallographic data phase data THIS ARTICLE includes systems where chromium is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006144
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. aluminum binary system binary phase diagrams crystallographic data phase data THIS ARTICLE includes systems where aluminum is the first-named element...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005215
EISBN: 978-1-62708-187-0
... kinetics of microsegregation are discussed for the binary isomorphous systems: titanium-molybdenum; binary eutectic systems: aluminum-copper and aluminum-silicon; binary peritectic systems: copper-zinc; multicomponent eutectic systems: Al-Si-Cu-Mg; and for systems with both eutectic and peritectic...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006221
EISBN: 978-1-62708-163-4
... weak interatomic bonds melt at lower temperatures. This includes several soft metals such as lead, tin, and bismuth. In contrast, the refractory metals have high melting points. The refractory metals include niobium, tantalum, molybdenum, tungsten, and rhenium. A two-phase system exists when a...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003836
EISBN: 978-1-62708-183-2
.... The first group includes the transition metal-metal binary alloy systems, such as copper-zirconium, nickel-titanium, and nickel-niobium, as well as binary alloys in the aluminum-refractory metal and Al-TM type. The second class consists of TM-metalloid alloys. These alloys are usually iron-, nickel...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001099
EISBN: 978-1-62708-162-7
... Moving parts that require control of expansion, such as pistons for some internal-combustion engines Bimetal strip Glass-to-metal seals Thermostatic strip Vessels and piping for storage and transportation of liquefied natural gas Superconducting systems in power transmissions Integrated...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001258
EISBN: 978-1-62708-170-2
...-tungsten show very high resistance to corrosion, but they are believed not to be true alloys ( Ref 2 ) and have not been used in practice. This article will discuss the alloys nickel-iron, nickel-cobalt, and nickel-manganese that are of practical interest, plus a few paragraphs on nickel-chromium binary...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003159
EISBN: 978-1-62708-199-3
... strip, glass-to-metal seals, thermostatic strip, vessels and piping for storage and transportation of liquefied natural gas, superconducting systems in power transmissions, integrated-circuit lead frames, components for radios and other electronic devices, and structural components in optical and laser...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003590
EISBN: 978-1-62708-182-5
... binary alloy, a mixed (A,B)O oxide may form as the internal oxide. This will occur if AO and BO have considerable mutual solubility so that the free energy of the system is lowered by precipitation of the mixed oxide. For example, the internal oxide that forms in unalloyed steels is (Fe,Mn)O ( Ref 12...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001426
EISBN: 978-1-62708-173-3
... porosity, which often occurs from welding a powder metallurgical product. It has been proposed that tungsten and molybdenum be alloyed with rhenium to improve both room-temperature ductility and weldability. The binary alloy of molybdenum with 50% rhenium can be easily welded using the GTAW and EBW...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005190
EISBN: 978-1-62708-187-0
... Titanium (s) 0.038 −7440 − 10.75 T Vanadium (s) 0.1 −4950 − 10.90 T Tungsten (s) 1.2 7500 − 15.20 T Zirconium (s) 0.043 −8300 − 11.95 T Detailed equilibrium diagrams of the Fe-C-B, Fe-C-Cr, Fe-C-Cu, Fe-C-Mn, Fe-C-Mo, Fe-C-N, Fe-C-Ni, Fe-C-Si, and Fe-C-W systems are available in...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006412
EISBN: 978-1-62708-192-4
... Abstract A sliding bearing (plain bearing) is a machine element designed to transmit loads or reaction forces to a shaft that rotates relative to the bearing. This article discusses the properties of bearing materials. It provides information on bearing material systems: single-metal systems...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003777
EISBN: 978-1-62708-177-1
... development of molybdenum alloys with higher alloy content was limited by the inability of existing facilities to work the alloys. On an experimental basis, however, binary alloys of molybdenum and niobium, tantalum, titanium, tungsten, vanadium, hafnium, and zirconium were prepared as arc-cast ingots and...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001313
EISBN: 978-1-62708-170-2
... deposition of binary disilicides combined with a molybdenum-vanadium system shows no pest phenomenon during service. This process can be considered commercial for small parts. A fluidized-bed, three-step silicon-vanadium-silicon process may be used for niobium as well as Ta-10W. Complex titanium...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003059
EISBN: 978-1-62708-200-6