1-20 of 717 Search Results for

transformation-induced plasticity steels

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 February 2024
Fig. 55 Temperature changes during continuous annealing of transformation-induced plasticity steel sheets. M s , martensite start temperature; A, austenite; F, ferrite; A R , retained austenite; B, bainite. Adapted from Ref 58 More
Series: ASM Handbook
Volume: 4F
Publisher: ASM International
Published: 01 February 2024
DOI: 10.31399/asm.hb.v04F.a0006995
EISBN: 978-1-62708-450-5
... with the transformations observed and critical temperatures during heat treatment. Additionally, the different types of steels, heat treatments, and their purposes are also discussed. microstructure quenching steel HEAT TREATMENT is defined as the controlled heating and cooling cycles of material in the solid...
Image
Published: 01 February 2024
, low-alloy; TRIP, transformation-induced plasticity; DP, dual-phase; CP, complex-phase; MART, martensitic; L-IP, lightweight induced plasticity; AUST SS, austenitic stainless steel; TWIP, twinning-induced plasticity. Adapted from Ref 55 More
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002354
EISBN: 978-1-62708-193-1
... materials tested in initially soft, dislocation-poor conditions resulting from a prior heat treatment. The article discusses deformation-induced phase transformations in austenitic stainless steels and commercial age-hardened aluminum alloys. It describes the interaction of dislocations...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005948
EISBN: 978-1-62708-168-9
... cycling and transformation-induced plasticity maraging methods. aging austenite grain refinement heat treatment maraging steel martensite nitriding solution annealing transformation-induced plasticity Introduction Maraging steels are highly alloyed low-carbon iron-nickel martensite...
Series: ASM Handbook
Volume: 4F
Publisher: ASM International
Published: 01 February 2024
DOI: 10.31399/asm.hb.v04F.a0007015
EISBN: 978-1-62708-450-5
.... Source: Ref 9 Residual Stress Pattern Induced by Thermal and Transformational Volume Changes A steel component undergoing quenching treatment is typically subjected to a fluctuating tri-axial stress state and plastic strains up to 2 to 3%. Thermal stresses are generated in the component due...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005936
EISBN: 978-1-62708-166-5
... tempering thermal stress through hardening transformation-induced plasticity IN THE CASE OF STEELS, heat treatment plays a fundamental role because no other process step can manipulate the microstructure in order to fulfill such a wide variety of possible in-service conditions. For the predominant...