1-20 of 257 Search Results for

torsional stability

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003040
EISBN: 978-1-62708-200-6
... Abstract Braiding is a textile process that is known for its simplicity and versatility. Braided structures are unique in their high level of conformability, torsional stability, and damage resistance. This article describes the braiding process and the mechanical properties of two-dimensional...
Book Chapter

By Frank K. Ko
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003361
EISBN: 978-1-62708-195-5
... Abstract Braided structures are unique in their high level of conformability, torsional stability, and damage resistance. This article describes the classifications of braiding such as two-dimensional braiding and three-dimensional braiding. It presents the governing equations for computer...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003296
EISBN: 978-1-62708-176-4
... Abstract This article describes the techniques involved in measuring the high-strain-rate stress-strain response of materials using a split-Hopkinson pressure bar (SHPB). It focuses on the generalized techniques applicable to all SHPBs, whether compressive, tensile, or torsion. The article...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009011
EISBN: 978-1-62708-185-6
... Abstract This article discusses the equipment design, procedures, experimental considerations, and interpretation of the torsion tests used to establish workability. It describes the application of torsion testing to obtain flow-stress data and to gage fracture-controlled workability and flow...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003295
EISBN: 978-1-62708-176-4
... Abstract This article reviews the dynamic factors, experimental methods and setup, and result analysis of different types of high strain rate shear tests. These include high strain rate torsion testing, double-notch shear testing and punch loading, drop-weight compression shear testing, thick...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006347
EISBN: 978-1-62708-179-5
... content is kept low because of the carbide-stabilizing effect of this element and because it retards both the first-stage and second-stage annealing reactions. A mixture of gray iron and white iron in variable proportions that produces a mottled (speckled) appearance is particularly damaging...
Book Chapter

By Mark Hayes
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002377
EISBN: 978-1-62708-193-1
... support the maximum applied stress, at which time overload failure will occur. Fatigue is a likely failure mechanism for all types of springs (compression, extension, torsion, leaf, presswork, spiral, constant force, disc, etc.) as well as for all spring sizes (fatigue occurs in springs made from...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009007
EISBN: 978-1-62708-185-6
... Abstract This article discusses a number of workability tests that are especially applicable to the forging process. The primary tests for workability are those for which the stress state is well known and controlled. The article provides information on the tension test, torsion test...
Book Chapter

Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001005
EISBN: 978-1-62708-161-0
...-stabilizing effect of this element and because it retards both the first-stage and second-stage annealing reactions. A mixture of gray iron and white iron in variable proportions that produces a mottled (speckled) appearance is particularly damaging to the mechanical properties of the annealed casting...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003290
EISBN: 978-1-62708-176-4
... relaxation testing used for the most convenient and common uniaxial tensile test. It concludes with information on compression testing, bend testing, torsion testing, and tests on springs. stress relaxation testing metallic materials long-term tests accelerated testing uniaxial tensile test...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005873
EISBN: 978-1-62708-167-2
... Abstract Tempering of induction-hardened steel is a form of subcritical heat treatment, primarily carried out to increase ductility, toughness, and dimensional stability, to relieve residual stresses, and to obtain specific values of mechanical properties. This article describes tempering...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002453
EISBN: 978-1-62708-194-8
... in Table 5(f) and 5(g) of this article. Performance Index for a Light, Strong Tie The loading on a component can generally be decomposed into some combination of axial tension or compression, bending, and torsion. Almost always, one mode dominates. So common is this that the functional name given...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001032
EISBN: 978-1-62708-161-0
... and specialized tests. The article compares the processing of microalloyed plate and bar products. The article focuses on the use of torsion testing to evaluate the forgeability of carbon and alloy steels and presents information on measuring flow stress. The article discusses the metallurgy and thermomechanical...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006836
EISBN: 978-1-62708-329-4
... can be made. While most of the failures discussed in this article involve fracture, it is also noted below that a spring will fail to perform its function if it relaxes due to temperature exposure beyond the limits of its material stability. Corrosive Environments Most springs are not subjected...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004016
EISBN: 978-1-62708-185-6
..., such an approach may be linked to the work in the 1930s and 1940s of P. Bridgeman, who used torsion combined with compression to attain very large plastic strains. Although “Bridgeman's anvils” ( Ref 1 ) could be applied only to thin discs, this technique realizes intensive simple shear under high hydrostatic...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003108
EISBN: 978-1-62708-199-3
.... The article also talks about the effects of composition, graphite shape, and section size on the mechanical properties of ductile iron. Tables and graphs provide helpful information on the tensile properties, compressive properties, torsional properties, damping capacity, impact properties, fracture toughness...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002398
EISBN: 978-1-62708-193-1
... considerable toughness at cryogenic temperatures. Comparative data for other cast stainless steels are summarized in Fig. 2 . The lower carbon duplex cast stainless steel grades CF3M, CF8, and CF8M and the austenitic CN7M and CF20 exhibit significantly higher toughness than the stabilized grade of CF8C...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005413
EISBN: 978-1-62708-196-2
... be expected to collapse when the next dislocation traverses the slip plane and attempts to add another loop to the same area. Thus, a stabilizing mechanism must be found. It was proposed by Kocks ( Ref 11 ) that secondary dislocations in the neighborhood (i.e. belonging to a slip system not active...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006253
EISBN: 978-1-62708-169-6
... Abstract This article introduces the different types, distinctions, and grades of commercially pure titanium and titanium alloys. It describes three types of alloying elements: alpha stabilizers, beta stabilizers, and neutral additions. The article discusses the basic categories of titanium...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003319
EISBN: 978-1-62708-176-4
... and behavior of ceramics and glasses. The article explains the double torsion and double-cantilever beam fracture mechanics methods, which employ test specimens with relatively large, induced cracks. Crack growth data are typically determined directly by the observation of the crack or by devices that monitor...