Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005125
EISBN: 978-1-62708-186-3
... Abstract This article discusses the mill products most often formed by the three-roll forming process. It schematically illustrates some of the shapes commonly produced from flat stock by the three-roll forming process. The article describes the two basic types of three-roll forming machines...
Image
Published: 01 January 2006
Fig. 30 Use of three-roll forming in conjunction with press forming and hydraulic expansion forming, in the 14-operation production of a container for liquids. Dimensions given in inches Table 11 Sequence of operations Blank in die, in single-action press. Form edge radii More
Image
Published: 01 January 2006
Fig. 19 Use of three-roll forming to produce a curve in a U-section channel More
Image
Published: 01 January 2006
Fig. 1 Typical shapes produced from flat stock by three-roll forming More
Image
Published: 01 December 1998
Fig. 37 Typical shapes produced from flat stock by three-roll forming More
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003177
EISBN: 978-1-62708-199-3
... or nonferrous metals. The article reviews the various types of forming processes such as blanking, piercing, fine-edge blanking, press bending, press forming, forming by multiple-slide machines, deep drawing, stretch forming, spinning, rubber-pad forming, three-roll forming, contour roll forming, drop hammer...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005139
EISBN: 978-1-62708-186-3
..., press-brake forming, press forming, multiple-slide forming, deep drawing, spinning, rubber-pad forming, drop hammer forming¸ three-roll forming, contour roll forming, stretch forming, and bending of tubing. bending blanking contour roll forming deep drawing drop hammer forming formability...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005134
EISBN: 978-1-62708-186-3
... in the article “Three-Roll Forming” in this Volume. Example 1: Three-Roll Bending of a Structural Section A 7.6 kW (10 hp) three-roll bender was used to bend a steel angle 75 by 75 by 9.5 mm (3 by 3 by 3 8 in.) into a circular reinforcing flange 1520 mm (60 in.) in diameter. The angle...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005142
EISBN: 978-1-62708-186-3
... beryllium. The article discusses the role of lubrication, blank development, tool designs, and strain rates, in deep drawing. It also provides information on the tooling and applications of three-roll bending, stretch forming, and spinning. beryllium blank development deep drawing dies formability...
Book Chapter

By Robert Bolin
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003982
EISBN: 978-1-62708-185-6
... Abstract Ring rolling is a process for creating seamless ring shaped components using specialized equipment and forming processes. This article provides information on the applications of ring rolling. It discusses the types of machines used for ring rolling, namely, vertical rolling machines...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005146
EISBN: 978-1-62708-186-3
...-brake forming 4340 steel (36–40 HRC) Graphite suspension in a suitable solvent Contour roll forming, three-roll forming AISI A2 tool steel SAE 60 oil Stretch forming Epoxy-faced cast aluminum, cast zinc, cast bronze Grease-oil mixtures, wax; 10:1 wax-graphite mixture Hot forming...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005135
EISBN: 978-1-62708-186-3
... Programmable rotary draw bender with capacity to bend 50 mm (2 in.). Schedule 40 pipe. Courtesy of Baileigh Industrial Inc. Roll Bending of Tube Roll bending of tube is limited to thick-walled product, but it is used to produce full circles of helical coils (see the article “Three-Roll Forming...
Book Chapter

Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004012
EISBN: 978-1-62708-185-6
... Abstract Thread rolling is a cold-forming process for producing threads or other helical or annular forms by rolling the impression of hardened steel dies into the surface of a cylindrical or conical blank. Methods that use cylindrical dies are classified as radial infeed, tangential feed...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003971
EISBN: 978-1-62708-185-6
... Abstract Metalworking is one of the three major technologies used to fabricate metal products. This article tabulates the classification of metal forming processes. It discusses different types of metalworking equipment, including rolling mills, ring-rolling machines, and thread-rolling...
Book Chapter

Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002142
EISBN: 978-1-62708-188-7
... Evaluation of Metals for Thread Rolling The three characteristics that are important in evaluating and selecting metals for thread rolling are rollability, flaking, and seaming. Rollability Rollability involves ductility and the resistance of a metal to flow when subjected to cold forming...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001011
EISBN: 978-1-62708-161-0
... Abstract This article addresses classifications and designations for carbon and low-alloy steel sheet and strip product forms based on composition, quality descriptors, mechanical properties, and other factors. Carbon steel sheet and strip are available as hot-rolled and as cold-rolled products...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004014
EISBN: 978-1-62708-185-6
..., the process is effective in producing tubular components to various specifications. There are two basic methods of flow forming that are characterized by the position of the rolls during the forming process. One method involves the use of staggered rolls, where three rolls are staggered axially...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005138
EISBN: 978-1-62708-186-3
... the rolls shown are plain cylinders, these can be replaced with rolls ground to any shape that will form the desired cross section. Some sections require several passes through the machine. It may take two passes to roll an accurate sharp-cornered square wire, and three or more passes may be needed to make...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005126
EISBN: 978-1-62708-186-3
... in contour roll forming. (a) Upper roll constructed in five sections allows for minor adjustments. (b) Three-section upper roll allows replacement of center section. Figure 6(b) shows an upper forming roll made up of three sections—a narrow center section flanked by two wider sections. In use...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004010
EISBN: 978-1-62708-185-6
... that generally denotes cold forming of plate, sheet, bars, beams, pipe, or angular cross section lengths into selected shapes by passing the metal workpiece between three correctly spaced rolls ( Ref 1 , 5 ). The roll forming process employs pairs of small opposed rollers to shape a cylindrical workpiece...