Skip Nav Destination
Close Modal
By
Jeffrey Gotro, R. Bruce Prime
By
Brian S. Hayes, Luther M. Gammon
By
Terry W. Cowley
By
Brian S. Hayes, Luther M. Gammon
By
John M. Henshaw
By
Paul J. Gramann
Search Results for
thermosets
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 545
Search Results for thermosets
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
Thermosets
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003010
EISBN: 978-1-62708-200-6
... Abstract A thermosetting resin, or thermoset, is a synthetic organic polymer that cures to a solid, infusible mass by forming a three-dimensional network of covalent chemical bonds. Significant applications include construction and thermoset engineering plastics. This article discusses...
Abstract
A thermosetting resin, or thermoset, is a synthetic organic polymer that cures to a solid, infusible mass by forming a three-dimensional network of covalent chemical bonds. Significant applications include construction and thermoset engineering plastics. This article discusses the general and family characteristics of thermosetting resin families, including allyls, aminos (urea formaldehyde and melamine formaldehyde), cyanates, epoxies, polybenzimidazoles, unsaturated polyesters, thermoset polyimides, phenolics, and vinyl esters. It also explains processing methods, including curing and curing agents. The article provides descriptions of commercial product forms and the wide array of applications of thermosetting resins. It also tabulates the performance properties (mechanical, thermal, electrical and chemical resistance) of some families of unfilled or unreinforced thermosetting resins and reinforced or filled grades.
Image
Published: 01 January 2001
Fig. 4 Structures of selected addition-type polyimides (thermosets)
More
Image
Published: 01 January 2001
Fig. 1 Compression properties of thermosets and thermoplastics. Source: Ref 9 and manufacturer data (PEI, Hexcel Corp.; PEEK, Cytec Fiberite)
More
Image
Schematic comparing the processing of (a) thermoplastics and (b) thermosets...
Available to Purchase
in Characterization of Thermosetting Resins and Polymers
> Characterization and Failure Analysis of Plastics
Published: 15 May 2022
Fig. 1 Schematic comparing the processing of (a) thermoplastics and (b) thermosets
More
Book Chapter
Characterization of Thermosetting Resins and Polymers
Available to PurchaseSeries: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006924
EISBN: 978-1-62708-395-9
... Abstract This article discusses the most common thermal analysis methods for thermosetting resins. These include differential scanning calorimetry, thermomechanical analysis, thermogravimetric analysis, and dynamic mechanical analysis. The article also discusses the characterization of uncured...
Abstract
This article discusses the most common thermal analysis methods for thermosetting resins. These include differential scanning calorimetry, thermomechanical analysis, thermogravimetric analysis, and dynamic mechanical analysis. The article also discusses the characterization of uncured thermosetting resins as well as the curing process. Then, the techniques to characterize the physical properties of cured thermosets and composites are presented. Several examples of stress-strain curves are shown for thermosets and thermoplastic polymers.
Book Chapter
Toughening Methods for Thermoset-Matrix Composites
Available to PurchaseSeries: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009080
EISBN: 978-1-62708-177-1
... Abstract This article describes the dispersed-phase toughening of thermoset matrices by the development of multiphase-structure thermosetting matrices using rubber and/or thermoplastic materials. It discusses two main methods for manufacturing prepregs, namely, single-pass impregnation...
Abstract
This article describes the dispersed-phase toughening of thermoset matrices by the development of multiphase-structure thermosetting matrices using rubber and/or thermoplastic materials. It discusses two main methods for manufacturing prepregs, namely, single-pass impregnation and double-pass impregnation. The article illustrates reflected-light optical microscopy techniques to evaluate the morphology of thermoplastic materials for determining the material quality and correlating key microstructural features with material performance.
Book Chapter
Environmental Performance of Thermosetting Plastics and Resin Matrix Composites
Available to PurchaseBook: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003845
EISBN: 978-1-62708-183-2
... thermosetting resins. The article concludes with a discussion on the curing system of thermosetting resins. furan fabrication fiberglass-reinforced plastic equipment polyester epoxy vinyl-ester phenolic thermosetting resins MANY FACTORS contribute to the corrosion-resistant effectiveness...
Abstract
This article describes the resin and fabrication requirements associated with fiberglass-reinforced plastic equipment. It provides a discussion on various resins and their resistance to various environments. These include polyester, epoxy, epoxy vinyl-ester, and furan and phenolic thermosetting resins. The article concludes with a discussion on the curing system of thermosetting resins.
Book Chapter
Forms and Properties of Composite Materials
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003032
EISBN: 978-1-62708-200-6
... the mechanical properties, physical properties, and service characteristics of representative composite fiber-resin combinations, including thermoplastic matrix composites such as thermoplastic polyester resins, thermoplastic polyamide resins, and thermoplastic polysulfone resins, and thermoset matrix composites...
Abstract
The design and analysis of aerospace and industrial composite components and assemblies requires a detailed knowledge of materials properties, which, in turn, depend on the manufacturing, machining, and assembly methods used. This article, through several tables and graphs, provides the mechanical properties, physical properties, and service characteristics of representative composite fiber-resin combinations, including thermoplastic matrix composites such as thermoplastic polyester resins, thermoplastic polyamide resins, and thermoplastic polysulfone resins, and thermoset matrix composites such as thermoset polyester resins, thermoset phenolic resins, thermoset epoxy resins, thermoset polyimide resins, and thermoset bismaleimide resins.
Book Chapter
Injection Molding
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003014
EISBN: 978-1-62708-200-6
... Abstract Injection molding is a process of forcing or injecting a fluid plastic material into a closed mold. The process generally has the advantages of being more readily automated and of permitting finer part details. Injection-molding compounds are thermoplastic or thermosetting materials...
Abstract
Injection molding is a process of forcing or injecting a fluid plastic material into a closed mold. The process generally has the advantages of being more readily automated and of permitting finer part details. Injection-molding compounds are thermoplastic or thermosetting materials and their composites that are specifically formulated for the injection-molding process. This article discusses the injection molding process, which includes the two basic categories of thermoplastic and thermoset injection molding, and lists the common thermoplastic and thermoset molding compounds and applications. It also describes the operation of the different types of injection molding machines as well as mold design and process controls. The article also describes the selection of injection-moldable thermosets, and provides an overview of part performance, properties, blowing agents, and aesthetic concerns related to thermoplastic structural-foam injection molding.
Book Chapter
Impact Response of Composites
Available to PurchaseSeries: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009081
EISBN: 978-1-62708-177-1
... of composite failure mechanisms such as thermoplastic-matrix composite failure mechanisms, untoughened thermoset-matrix composite failure mechanisms, toughened thermoset-matrix composite failure mechanisms, dispersed-phase and rubber-toughened thermoset-matrix composite failure mechanisms, and particle...
Abstract
This article describes methods for analyzing impact-damaged composites in the aircraft industry. These include C-scan and x-radiography methods and optical microscopy. The article reviews brittle-matrix composite and tough-matrix composite failures. It explains the different types of composite failure mechanisms such as thermoplastic-matrix composite failure mechanisms, untoughened thermoset-matrix composite failure mechanisms, toughened thermoset-matrix composite failure mechanisms, dispersed-phase and rubber-toughened thermoset-matrix composite failure mechanisms, and particle interlayer-toughened composite failure mechanisms.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001466
EISBN: 978-1-62708-173-3
... Abstract Successful adhesive bonding of organic-matrix composites is dependent on the nature of the adherend surfaces. This article emphasizes the critical importance of proper surface preparation in both thermoset and thermoplastic composites. It provides information on surface preparation...
Abstract
Successful adhesive bonding of organic-matrix composites is dependent on the nature of the adherend surfaces. This article emphasizes the critical importance of proper surface preparation in both thermoset and thermoplastic composites. It provides information on surface preparation for thermoset composite adherends along with a standard technique (water-break test) for verifying the adequacy of surface preparation for metal bonding. In addition, the article provides examples of good and bad adhesive bonds and describes some important process variables that are considered and controlled in bonding process for thermoset adhesives. The article concludes with a discussion on three different approaches for bonding thermoplastic composite composite panels together.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003441
EISBN: 978-1-62708-195-5
... materials used for thermoset and thermoplastic resin matrices. It reviews the identification of the individual characteristics of thermoset and thermoplastic resin along with the test methods normally used for their determination. The article contains a table that lists properties and tests for uncured...
Abstract
This article describes the most significant tests to characterize the properties of constituent materials. It discusses the chemical, physical, and mechanical tests for determining the properties of reinforcement fibers and fabrics. The article provides information on some of the basic materials used for thermoset and thermoplastic resin matrices. It reviews the identification of the individual characteristics of thermoset and thermoplastic resin along with the test methods normally used for their determination. The article contains a table that lists properties and tests for uncured and cured thermoset-matrix resins and prepregs.
Book Chapter
Engineering Tables: Polymeric Materials
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003002
EISBN: 978-1-62708-200-6
... Abstract This article is a comprehensive collection of engineering tables providing information on the mechanical properties of and the techniques for processing and characterizing polymeric materials, such as thermosets, thermoset-matrix unidirectional advanced composites, and unreinforced...
Abstract
This article is a comprehensive collection of engineering tables providing information on the mechanical properties of and the techniques for processing and characterizing polymeric materials, such as thermosets, thermoset-matrix unidirectional advanced composites, and unreinforced and carbon-and glass-reinforced engineering thermoplastics. Values are also provided for chemical resistance ratings for selected plastics and metals, and hardness of selected elastomers.
Book Chapter
Recycling and Disposal of Polymer-Matrix Composites
Available to PurchaseBook: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003471
EISBN: 978-1-62708-195-5
... Abstract This article begins with a discussion on the driving forces for recycling composites. It reviews the recycling process of thermoset-matrix composites and thermoplastic-matrix composites. The recycling of thermoset-matrix composites includes regrind, chemical, energy recovery...
Abstract
This article begins with a discussion on the driving forces for recycling composites. It reviews the recycling process of thermoset-matrix composites and thermoplastic-matrix composites. The recycling of thermoset-matrix composites includes regrind, chemical, energy recovery, and thermal processes. Thermoplastic-matrix composites are recycled by regrinding, compounding/blending and reprocessing. The article concludes with discussion on the properties of recycled composite fibers.
Book Chapter
Navigating the Plastic Material Selection Process
Available to PurchaseSeries: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006922
EISBN: 978-1-62708-395-9
.... This article reviews the numerous considerations that are equally important to help ensure that part failure does not occur. It provides a quick review of thermoplastic and thermoset plastics. The article focuses primarily on thermoset materials that at room temperature are below their glass transition...
Abstract
There are many reasons why plastic materials should not be considered for an application. It is the responsibility of the design/materials engineer to recognize when the expected demands are outside of what the plastic can provide during the expected life-time of the product. This article reviews the numerous considerations that are equally important to help ensure that part failure does not occur. It provides a quick review of thermoplastic and thermoset plastics. The article focuses primarily on thermoset materials that at room temperature are below their glass transition temperature. It describes the motivation for material selection and the goal of the material selection process. The use of material datasheets for material selection as well as the processes involved in plastic material selection and post material selection is also covered.
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006916
EISBN: 978-1-62708-395-9
... and orientation. It also presents examples of failures stemming from material degradation improper use of metal inserts, weak weld lines, insufficient curing of thermosets, and inadequate mixing and impregnation in the case of thermoset composites. injection molding manufacturing-related failures...
Abstract
This article focuses on manufacturing-related failures of injection-molded plastic parts, although the concepts apply to all plastic manufacturing processes It provides detailed examples of failures due to improper material handling, drying, mixing of additives, and molecular packing and orientation. It also presents examples of failures stemming from material degradation improper use of metal inserts, weak weld lines, insufficient curing of thermosets, and inadequate mixing and impregnation in the case of thermoset composites.
Book Chapter
Properties and Performance of Polymer-Matrix Composites
Available to PurchaseBook: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003447
EISBN: 978-1-62708-195-5
... composites and thermoset-matrix composites. The thermoplastic-matrix composites include thermoplastic polyester resins and fiber resin composites; thermoplastic polyamide resins and fiber-resin composites; and thermoplastic polysulfone resins and fiber-resin composites. polymer-matrix composites...
Abstract
This article discusses the materials and properties of polymer-matrix composites to characterize each generic material according to its composition and method of manufacture. It contains a table that lists the key physical, mechanical, thermal, and electrical properties, and in-service conditions of concern for resin-matrix composites. Axes definitions, symbols, and special property calculations for composite material property tests are reviewed. The article provides an overview of the performance capabilities of selected polymer-matrix composite materials such as thermoplastic-matrix composites and thermoset-matrix composites. The thermoplastic-matrix composites include thermoplastic polyester resins and fiber resin composites; thermoplastic polyamide resins and fiber-resin composites; and thermoplastic polysulfone resins and fiber-resin composites.
Image
Light micrographs of specimens of 1215 carbon steel that were salt bath nit...
Available to PurchasePublished: 15 January 2021
Fig. 3 Light micrographs of specimens of 1215 carbon steel that were salt bath nitrided and mounted in different resins. (a) Thermosetting epoxy resin. (b) Phenolic thermosetting resin. (c) Methyl methacrylate thermoplastic resin. (d) Electroless nickel plated and mounted in thermosetting
More
Image
Fusion-bonded epoxy coatings are a one part, heat-cured, thermosetting epox...
Available to PurchasePublished: 30 September 2015
Fig. 2 Fusion-bonded epoxy coatings are a one part, heat-cured, thermosetting epoxy coating designed for corrosion protection of metal and electrical insulation. They depend on the chemistry of the materials used. The chemistry in turn relies on the formulation components—epoxy resin ( Ref 5
More
Image
Proper encapsulation of thermal spray coatings. (a) Thermosetting encapsula...
Available to PurchasePublished: 01 December 2004
Fig. 8 Proper encapsulation of thermal spray coatings. (a) Thermosetting encapsulation for dense, nonfriable coatings. Temperature: 140 °C (285 °F). Heat time: 4 to 6 min. Cool time: 2 min. (b) Room-temperature epoxy encapsulation with vacuum impregnation (25 in. mercury) for porous, friable
More
1