1-20 of 99

Search Results for thermoset polyimide resins

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 January 2001
Fig. 98 Dielectric strength versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 January 2001
Fig. 101 Ultimate tensile strength versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 January 2001
Fig. 102 Ultimate shear strength versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 January 2001
Fig. 103 Dissipation factor versus temperature for thermoset polyimide resin and resin-matrix composites. MC, molding compound More
Image
Published: 01 January 2001
Fig. 104 Dielectric constant versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 November 1995
Fig. 98 Dielectric strength versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 November 1995
Fig. 101 Ultimate tensile strength versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 November 1995
Fig. 102 Ultimate shear strength versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 November 1995
Fig. 103 Dissipation factor versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 November 1995
Fig. 104 Dielectric constant versus temperature for thermoset polyimide resin and resin-matrix composites More
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003032
EISBN: 978-1-62708-200-6
... such as thermoset polyester resins, thermoset phenolic resins, thermoset epoxy resins, thermoset polyimide resins, and thermoset bismaleimide resins. fiber-resin mechanical properties physical properties thermoplastic matrix composite thermoset matrix composites THE DESIGN AND ANALYSIS of aerospace...
Image
Published: 01 January 2001
Fig. 99 Ultimate compressive strength versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 November 1995
Fig. 99 Ultimate compressive strength versus temperature for thermoset polyimide resin and resin-matrix composites More
Image
Published: 01 January 2001
Fig. 100 Coefficient of thermal expansion versus temperature for thermoset polyimide resin and resin-matrix composites. 10 –6 /K × 5 9 =μin./in. ×°F More
Image
Published: 01 November 1995
Fig. 100 Coefficient of thermal expansion versus temperature for thermoset polyimide resin and resin-matrix composites. 10 −6 /K × 5 9 = μin./in. × °F More
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003447
EISBN: 978-1-62708-195-5
... thermoset epoxy resins thermoset polyimide resins thermoset bismaleimide resins THE DESIGN AND ANALYSIS of composite components and assemblies require a detailed knowledge of materials properties, which, in turn, depend on the manufacturing, machining, and assembly methods used. This article selects...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003010
EISBN: 978-1-62708-200-6
... the general and family characteristics of thermosetting resin families, including allyls, aminos (urea formaldehyde and melamine formaldehyde), cyanates, epoxies, polybenzimidazoles, unsaturated polyesters, thermoset polyimides, phenolics, and vinyl esters. It also explains processing methods, including...
Book Chapter

By Susan Robitaille
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003367
EISBN: 978-1-62708-195-5
... Abstract Cyanate ester resins are a family of high-temperature thermosetting resins that bridge the gap in thermal performance between engineering epoxy and high-temperature polyimides. This article discusses the chemistry, properties and characteristics of the cyanate ester resins...
Book Chapter

By Robert Pieper
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006923
EISBN: 978-1-62708-395-9
... (a) (a) Polyether-imide 215 420 (a) (a) Polysulfone 193 380 (a) (a) Polyimide (thermoplastic) 280–330 535–625 (a) (a) Thermoset resins Amino (melamine-formaldehyde) None (b) None (b) … … Bismaleimide 230–345 (c) 450–650 (c) … … Epoxy 60–175 140–350...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003034
EISBN: 978-1-62708-200-6
... reinforcement and polyester, melamine, and epoxy resin systems extended the range of thermoset material capabilities. More recent developments of carbon and aramid fibers and of polyimide and silicone matrices offer further enhancements of the engineering properties that are available in thermoset molding...