1-20 of 91 Search Results for

thermoplastic resin matrices

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003441
EISBN: 978-1-62708-195-5
... materials used for thermoset and thermoplastic resin matrices. It reviews the identification of the individual characteristics of thermoset and thermoplastic resin along with the test methods normally used for their determination. The article contains a table that lists properties and tests for uncured...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003031
EISBN: 978-1-62708-200-6
... properties and impact resistance of composite matrices have led to the development and limited use of new high-temperature thermoplastic resin matrices. These materials are very different from the commodity thermoplastics (such as polyethylene, polyvinyl chloride, and polystyrene) that are commonly used...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003466
EISBN: 978-1-62708-195-5
... from epoxy matrix materials. Minimal fractographic data from other brittle thermoset resin systems are also presented. The article discusses the interlaminar fracture of composites with ductile thermoplastic matrices. It also provides information on the translaminar fracture features of the composite...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009071
EISBN: 978-1-62708-177-1
... Polymer matrices used for composite materials can be generally described as either thermoplastics or thermosets. Thermosets are polymer resins that crosslink and form a three-dimensional structure when cured. Once cured, the network structure is irreversible and cannot be reshaped or made to flow below...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003351
EISBN: 978-1-62708-195-5
.... Although polyimides may be thermosetting or thermoplastic, most composite applications use the thermosetting types, which are fully covered in this Section. The addition-type bismaleimide (BMI) resins are also covered in this Section. The use of high-performance thermoplastics as matrices in continuous...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009082
EISBN: 978-1-62708-177-1
... durability. The microstructure of the matrix is dictated by the matrix component(s) and, in many cases, is influenced by the cure cycle. It is commonly thought that the microstructure of thermoplastic matrices is affected more by the cure cycle than the microstructure of thermosetting matrices. This is due...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009080
EISBN: 978-1-62708-177-1
... Abstract This article describes the dispersed-phase toughening of thermoset matrices by the development of multiphase-structure thermosetting matrices using rubber and/or thermoplastic materials. It discusses two main methods for manufacturing prepregs, namely, single-pass impregnation...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003350
EISBN: 978-1-62708-195-5
... and fishing rods), piping for chemical processing plants, and printed circuit boards. Organic Matrices for Aerospace Organic matrices for aerospace applications include epoxy, bismaleimide, and polyimide resins. Various other thermoset and thermoplastic resins are in development or use for specific...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009075
EISBN: 978-1-62708-177-1
... to be fully visible. The features of a multiphase polymer matrix, such as a thermoset containing a second-phase thermoplastic or elastomer, are usually not resolved using bright-field illumination. Although some phases may be observable with dark-field techniques, most multiphase polymer matrices require...
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003370
EISBN: 978-1-62708-195-5
... proportions for specific resin paste formulations. Some ingredients, such as release agents and thermoplastic syrups, can be added by the resin supplier. As described below, each additive provides important properties to the SMC, either during the processing and molding steps or in the finished parts...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003401
EISBN: 978-1-62708-195-5
... of producing a part with the required geometry, but it is also important to note that the technique selected influences surface finish, allowable reinforcement configurations, available resins and their properties as matrices, as well as a host of other properties, including cost. Table 1 illustrates some...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009079
EISBN: 978-1-62708-177-1
... or mechanical loading of the composite material. Even small microcracks can propagate in tough materials in the right environment, creating paths for water, solvents, and cryogenic liquids, which can cause further damage. The composite constituents (such as resin matrix and fibers) and the ratio...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003381
EISBN: 978-1-62708-195-5
... Abstract Hygrothermal behavior of cured composite materials relates to the combined and commonly synergistic effects of moisture absorption and temperature on various physical, chemical and mechanical properties. This article focuses on the influence of resins or matrices, reinforcements...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003368
EISBN: 978-1-62708-195-5
... Abstract This article provides information on the thermoplastic resins used as matrix materials for continuous fiber reinforced composites. It focuses on the materials that are suitable for fabrication of structural laminates and used for aerospace applications. The article provides...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003419
EISBN: 978-1-62708-195-5
... on the matrix being a thermoset polymer. The main reason for the lack of widespread acceptance of thermoplastic matrices is that they tend to be more difficult to process into a composite than thermosets. However, this fact does not mean that there are no techniques to manufacture composites with thermoplastic...
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003412
EISBN: 978-1-62708-195-5
... Abstract Curing is the irreversible change in the physical properties of a thermosetting resin brought about by a chemical reaction, condensation, ring closure, or addition. This article discusses the material types and functions of various components considered in the preparation for curing...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003373
EISBN: 978-1-62708-195-5
... matrices graphite diamond fullerenes nanotubes thermoplastic precursor thermosetting precursor evaporative precursor chemical vapor infiltration APPLICATIONS involving very high temperature or highly corrosive environments often have requirements that exceed the capabilities of plastic...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
.... For example, cross linking can be used to produce high-performance composite matrices that can be molded as thermoplastics and subsequently cross linked to produce varying degrees of thermosetting properties. Similarly, elastomers or rubbers can use different degrees of cross linking to vary the properties...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003006
EISBN: 978-1-62708-200-6
... epoxy (EP), phenolic, and unsaturated polyester (UP) resins. Epoxies are used as both commodity and engineering adhesives and as matrices for high-performance composites. Phenolic resins are used in commodity applications such as ashtrays and cutlery handles, as well as for brake pistons and electrical...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003465
EISBN: 978-1-62708-195-5
... T g can lead to microcracking. In addition, for a multiphase resin (for example, elastomeric or thermoplastic modified), thermal analysis can determine the T g of the modifying second phase. If such a fingerprint differs to a significant degree from a control sample, there may be a problem...