1-20 of 136

Search Results for thermoplastic polyamide resins

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003447
EISBN: 978-1-62708-195-5
... composites and thermoset-matrix composites. The thermoplastic-matrix composites include thermoplastic polyester resins and fiber resin composites; thermoplastic polyamide resins and fiber-resin composites; and thermoplastic polysulfone resins and fiber-resin composites. polymer-matrix composites...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003032
EISBN: 978-1-62708-200-6
... the mechanical properties, physical properties, and service characteristics of representative composite fiber-resin combinations, including thermoplastic matrix composites such as thermoplastic polyester resins, thermoplastic polyamide resins, and thermoplastic polysulfone resins, and thermoset matrix composites...
Book Chapter

By Daniel A. Scola
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003365
EISBN: 978-1-62708-195-5
... Abstract This article discusses the properties and applications of two types of polyimide resins: condensation polyimides and addition-type polyimides. It describes the chemistry of condensation-type polyimides during synthesis, processing of polyamide acid precursor solution to polyimide...
Image
Published: 01 January 2001
Fig. 6 Mechanical properties of selected matrix resins. Thermoplastics: polyester (unfilled; maximum temperature 140 °C, or 284 °F), polyamide (nylon 6/6, unfilled; maximum temperature 130 °C, or 266 °F), and polysulfane (standard; maximum temperature 160 °C, or 320 °F). Thermosets: epoxy More
Book Chapter

By Kenneth B. Tator
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003692
EISBN: 978-1-62708-182-5
... resins, thermoplastic resins, and cross-linked thermosetting resins. The autooxidative cross-linked resins include alkyd resins and epoxy esters. The article examines the two types of coatings based on thermoplastic resins: those deposited by evaporation of a solvent, commonly called lacquers, and those...
Image
Published: 01 January 1997
Fig. 3 Mechanical properties and service temperatures for selected matrix resins. Thermoplastics: polyester (unfilled; maximum temperature 140 °C, or 248 °F), polyamide (nylon 6/6, unfilled; maximum temperature 130 °C, or 266 °F), and polysulfone (standard; maximum temperature 160 °C, or 320 More
Book Chapter

By Robert Pieper
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006923
EISBN: 978-1-62708-395-9
..., and glass transition temperature. It also provides information on polyimide and bismaleimide resin systems. Representative examples of different types of engineering thermoplastics are discussed primarily in terms of structure and thermal properties. chemical composition elastomeric materials...
Book Chapter

By Peter Martin
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
... crystallinity. Such polymers are termed semicrystalline because the degree of crystallinity never reaches 100%; they include such important thermoplastics as PE and nylons (or polyamides). Most polymers, however, have either very little or no true crystallinity and are generally referred to as noncrystalline...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006922
EISBN: 978-1-62708-395-9
.... This article reviews the numerous considerations that are equally important to help ensure that part failure does not occur. It provides a quick review of thermoplastic and thermoset plastics. The article focuses primarily on thermoset materials that at room temperature are below their glass transition...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003009
EISBN: 978-1-62708-200-6
..., family characteristics, properties and applications of the following advanced thermoplastics: homopolymer and copolymer acetals, fluoropolymers, ionomers, polyamides, polyamide-imides, polyarylates, polyketones, polyaryl sulfones, polybutylene terephthalates, polycarbonates, polyether-imides, polyether...
Book Chapter

By Victoria Burt
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006530
EISBN: 978-1-62708-207-5
... and limitations of adhesive-bonded aluminum joints and the procedures used to produce them. It addresses surface preparation, the addition of interfacial coatings and primers, and the application of thermoplastic and thermosetting resins. The article examines the nature and role of the various layers...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006945
EISBN: 978-1-62708-395-9
... Association NIST National Institute of Standards and Technology NMR nuclear magnetic resonance NR nitrile resins; natural rubber NRM nuclear magnetic resonance PA polyamide PAE polyaryl ether PAEK polyaryl ether ketone (also abbreviated PEK) PAI polyamide-imide PAK polyaromatic ketones PAN polyacrylonitrile...
Book Chapter

By Shari Bugaj
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003441
EISBN: 978-1-62708-195-5
... materials used for thermoset and thermoplastic resin matrices. It reviews the identification of the individual characteristics of thermoset and thermoplastic resin along with the test methods normally used for their determination. The article contains a table that lists properties and tests for uncured...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003031
EISBN: 978-1-62708-200-6
... such resins as polyetheretherketone (PEEK), polyphenylene sulfide (PPS), polyether-imide (PEI) (all of which are intended to maintain thermoplastic character in the final composite) and others, such as polyamide-imide (PAI), which is originally molded as a thermoplastic but is then postcured in the final...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009071
EISBN: 978-1-62708-177-1
...-reinforced polymeric composites are developed from thermoplastic or thermoset resins combined with either discontinuous or continuous unidirectional fibers or woven fabrics ( Fig. 1 ). Typical reinforcements consist of glass, carbon, or aramid fibers, but other materials, such as boron, ceramic...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003023
EISBN: 978-1-62708-200-6
... engineering plastics glass transition temperatures rheological analysis thermal analysis thermal properties thermogravimetric analysis thermomechanical analysis thermoplastic polymers thermosetting polymers thermostat resin systems THERMAL ANALYSIS provides a powerful tool for researchers...
Book Chapter

By Maureen A. Boyle, Cary J. Martin, John D. Neuner
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003362
EISBN: 978-1-62708-195-5
..., no effort has been made to identify where classifications overlap. Room Temperature Curing Agents Room temperature curing agents include aliphatic amines, polyamides, and amidoamines. Aliphatic Amines Aliphatic amines are the curatives most often paired with epoxy resins. When...
Book Chapter

By David K. Leigh, David Bourell
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006543
EISBN: 978-1-62708-290-7
... 585 … … … … PPS Farsoon 8100 PPS … … 47 7 4 295 563 220 428 116 241 PA6 BASF Ultrasint X028 … … 78 11 13 220 428 199 390 100 212 PA, polyamide, TPE, thermoplastic elastomer; TPU, thermoplastic polyurethane; PEKK, polyether ketoneketone; PPS, polyphenylene sulfide...
Book Chapter

By Lee McKague
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003368
EISBN: 978-1-62708-195-5
... Abstract This article provides information on the thermoplastic resins used as matrix materials for continuous fiber reinforced composites. It focuses on the materials that are suitable for fabrication of structural laminates and used for aerospace applications. The article provides...
Book Chapter

By Kenneth B. Tator
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006077
EISBN: 978-1-62708-172-6
... Novolac resin epoxy phosphate ester resin epoxy resins fluorinated epoxy resin ketimines phenolic co-polymers phosphorus-containing epoxy resin polyamides polyoxyalkylene amines waterborne epoxy resin EPOXY COATING SYSTEMS are the workhorses of the corrosion-protection industry...