Skip Nav Destination
Close Modal
Search Results for
ternary alloy phase diagram
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 286
Search Results for ternary alloy phase diagram
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006246
EISBN: 978-1-62708-163-4
... Abstract This article presents ternary alloy phase diagrams to be used primarily by engineers to solve industrial problems. The diagrams presented are for stable equilibrium conditions, with the exception of metastable conditions for some diagrams involving carbon and iron. In some ternary...
Abstract
This article presents ternary alloy phase diagrams to be used primarily by engineers to solve industrial problems. The diagrams presented are for stable equilibrium conditions, with the exception of metastable conditions for some diagrams involving carbon and iron. In some ternary diagrams involving carbon and iron, the symbol M is used to represent both iron and the other metallic element when the two metals substitute for each other in a carbide phase.
Book Chapter
Cu (Copper) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006240
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which copper (Cu) is the first-named element in the ternary system. The other elements are Fe, Mn, Ni, Pb, S, Sb, Si, Sn, Ti and Zn. The diagrams are presented with element compositions in weight percent. The article...
Abstract
This article is a compilation of ternary alloy phase diagrams for which copper (Cu) is the first-named element in the ternary system. The other elements are Fe, Mn, Ni, Pb, S, Sb, Si, Sn, Ti and Zn. The diagrams are presented with element compositions in weight percent. The article includes 42 phase diagrams (liquidus projection, solidus projection, isopleths, isothermal section and vertical section).
Book Chapter
Fe (Iron) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006241
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which iron (Fe) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 16 phase diagrams: Fe-Mn-Ni liquidus projection; Fe-Mn-Ni...
Abstract
This article is a compilation of ternary alloy phase diagrams for which iron (Fe) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 16 phase diagrams: Fe-Mn-Ni liquidus projection; Fe-Mn-Ni isothermal section at 750 °C; Fe-Mn-Ni isothermal section at 850 °C; Fe-Mn-Ni isothermal section at 650 °C; Fe-Mn-Ni isothermal section at 550 °C; Fe-Mo-Nb isothermal section at 1050 °C; Fe-Mo-Nb isothermal section at 1150 °C; Fe-Mo-Nb isothermal section at 900 °C; Fe-Mo-Ni liquidus projection; Fe-Mo-Ni isothermal section at 1100 °C; Fe-Mo-Ni isothermal section at 1200 °C; Fe-Ni-W liquidus and solidus projections; Fe-Ni-W isothermal section at 1500 °C; Fe-Ni-W isothermal section at 1455 °C; Fe-Ni-W isothermal section at 1465 °C; and Fe-Ni-W isothermal section at 1400 °C.
Book Chapter
Ge (Germanium) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006242
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which germanium (Ge) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes phase diagram of Ge-Sb-Te liquidus projection...
Abstract
This article is a compilation of ternary alloy phase diagrams for which germanium (Ge) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes phase diagram of Ge-Sb-Te liquidus projection.
Book Chapter
Mo (Molybdenum) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006243
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which molybdenum (Mo) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 8 phase diagrams: Mo-Nb-Ti isothermal section at 600 °C...
Abstract
This article is a compilation of ternary alloy phase diagrams for which molybdenum (Mo) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 8 phase diagrams: Mo-Nb-Ti isothermal section at 600 °C; Mo-Nb-Ti isothermal section at 1100 °C; Mo-Ni-Ti isothermal section at 1200 °C; Mo-Ni-Ti isothermal section at 900 °C; Mo-Ni-W isothermal section at 700 °C; Mo-Ni-W isothermal section at 1000 °C; Mo-Ti-W isothermal section at 2227 °C; and Mo-Ti-W isothermal section at 1000 °C.
Book Chapter
Nb (Niobium) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006244
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which niobium (Nb) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 2 phase diagrams: Nb-Ti-W isothermal section at 600 °C...
Abstract
This article is a compilation of ternary alloy phase diagrams for which niobium (Nb) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 2 phase diagrams: Nb-Ti-W isothermal section at 600 °C; and Nb-Ti-W isothermal section at 1000 °C.
Book Chapter
Ag (Silver) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006232
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which silver (Ag) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 16 phase diagrams: Ag-Au-Cu liquidus projection; Ag-Au-Cu...
Abstract
This article is a compilation of ternary alloy phase diagrams for which silver (Ag) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 16 phase diagrams: Ag-Au-Cu liquidus projection; Ag-Au-Cu isothermal section at 850 °C; Ag-Au-Cu isothermal section at 950 °C; Ag-Au-Cu isothermal section at 775 °C; Ag-Au-Cu isothermal section at 300 °C; Ag-Cd-Cu isothermal section at 600 °C; Ag-Cd-Cu liquidus projection; Ag-Cd-Cu isothermal section at 500 °C; Ag-Cd-Cu isothermal section at 300 °C; Ag-Cd-Zn isothermal section at 600 °C; Ag-Cd-Zn liquidus projection; Ag-Cd-Zn isothermal section at 400 °C; Ag-Cd-Zn isothermal section at 200 °C; Ag-Cu-Zn isothermal section at 600 °C; Ag-Cu-Zn liquidus projection; and Ag-Cu-Zn isothermal section at 350 °C.
Book Chapter
Pb (Lead) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006245
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which lead (Pb) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 7 phase diagrams: Pb-Sb-Sn liquidus projection; Pb-Sb-Sn...
Abstract
This article is a compilation of ternary alloy phase diagrams for which lead (Pb) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 7 phase diagrams: Pb-Sb-Sn liquidus projection; Pb-Sb-Sn isothermal section at 240 °C; Pb-Sb-Sn isothermal section at 189 °C; Pb-Sb-Sn (Pb) liquidus projection; Pb-Sn-Zn liquidus projection; and Pb-Sn-Zn isothermal section at 532 °C.
Book Chapter
Cd (Cadmium) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006237
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which cadmium (Cd) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 4 phase diagrams: Cd-Sb-Sn isothermal section at 212 °C...
Abstract
This article is a compilation of ternary alloy phase diagrams for which cadmium (Cd) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 4 phase diagrams: Cd-Sb-Sn isothermal section at 212 °C; Cd-Sb-Sn liquidus projection; Cd-Sb-Sn isothermal section at 175 °C; and Cd-Sb-Sn isothermal section at 20 °C.
Book Chapter
Co (Cobalt) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006238
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which cobalt (Co) is the first-named element in the ternary system. The other elements are Cr, Cu, Fe, Mo, Ni, Ti, V, and W. The diagrams are presented with element compositions in weight percent. The article includes 36...
Abstract
This article is a compilation of ternary alloy phase diagrams for which cobalt (Co) is the first-named element in the ternary system. The other elements are Cr, Cu, Fe, Mo, Ni, Ti, V, and W. The diagrams are presented with element compositions in weight percent. The article includes 36 phase diagrams (liquidus projection, solidus projection and isothermal section).
Book Chapter
Cr (Chromium) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006239
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which chromium (Cr) is the first-named element in the ternary system. The other elements are Fe, Mn, Mo, N, Nb, Ni, Ti, V and W. The diagrams are presented with element compositions in weight percent. The article...
Abstract
This article is a compilation of ternary alloy phase diagrams for which chromium (Cr) is the first-named element in the ternary system. The other elements are Fe, Mn, Mo, N, Nb, Ni, Ti, V and W. The diagrams are presented with element compositions in weight percent. The article includes 55 phase diagrams (liquidus projection, solidus projection, isothermal section and vertical section).
Book Chapter
Al (Aluminum) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006233
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which aluminum (Al) is the first-named element in the ternary system. The other elements are C, Co, Cr, Cu, Fe, Ga, Li, Mg, Mn, Mo, Nb, Ni, Sb, Si, Ti, U, V and Zn. The diagrams are presented with element compositions...
Abstract
This article is a compilation of ternary alloy phase diagrams for which aluminum (Al) is the first-named element in the ternary system. The other elements are C, Co, Cr, Cu, Fe, Ga, Li, Mg, Mn, Mo, Nb, Ni, Sb, Si, Ti, U, V and Zn. The diagrams are presented with element compositions in weight percent. The article includes 136 phase diagrams (liquidus projection, solidus projection, isothermal section, vertical section, and solvus projection).
Book Chapter
Au (Gold) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006234
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which gold (Au) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes five phase diagrams: Au-Cu-Ni boundaries of solid-state...
Abstract
This article is a compilation of ternary alloy phase diagrams for which gold (Au) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes five phase diagrams: Au-Cu-Ni boundaries of solid-state miscibility gap; Au-Cu-Ni liquidus projection; Au-Cu-Ni miscibility gap at 400 degrees centigrade; Au-Cu-Ni miscibility gap at 700 degrees centigrade; and Au-Sn-Te liquidus projection.
Book Chapter
B (Boron) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006235
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which boron (B) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 2 phase diagrams: B-C-Fe liquidus projection; and B-Fe-Nd...
Abstract
This article is a compilation of ternary alloy phase diagrams for which boron (B) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 2 phase diagrams: B-C-Fe liquidus projection; and B-Fe-Nd liquidus projection.
Book Chapter
C (Carbon) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006236
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which carbon (C) is the first-named element in the ternary system. The other elements are Co, Cr, Cu, Fe, Mn, Mo, N, Ni, S, Si, Ti, V, and W. The diagrams are presented with element compositions in weight percent...
Abstract
This article is a compilation of ternary alloy phase diagrams for which carbon (C) is the first-named element in the ternary system. The other elements are Co, Cr, Cu, Fe, Mn, Mo, N, Ni, S, Si, Ti, V, and W. The diagrams are presented with element compositions in weight percent. The article includes 136 phase diagrams (solidus projection, liquidus projection, isothermal section and vertical section).
Book
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.9781627081634
EISBN: 978-1-62708-163-4
Image
Published: 27 April 2016
Source: V. Raghavan, Phase Diagrams of Ternary Iron Alloys , The Indian Institute of Metals, Calcutta, India, 1987 ( Ref 10 )
More
Image
Published: 27 April 2016
Source: V. Raghavan, Phase Diagrams of Ternary Iron Alloys , The Indian Institute of Metals, Calcutta, India, 1987 ( Ref 10 )
More
Image
Published: 27 April 2016
Source: V. Raghavan, Phase Diagrams of Ternary Iron Alloys , The Indian Institute of Metals, Calcutta, India, 1987 ( Ref 10 )
More
Image
Published: 27 April 2016
Source: V. Raghavan, Phase Diagrams of Ternary Iron Alloys , The Indian Institute of Metals, Calcutta, India, 1987 ( Ref 10 )
More
1