1-20 of 2309

Search Results for surface treatments

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002466
EISBN: 978-1-62708-194-8
... Abstract Surface treatments are used in a variety of ways to improve the material properties of a component. This article provides information on surface treatments that improve service performance so that the design engineer may consider surface-engineered components as an alternative to more...
Image
Published: 01 January 2006
Fig. 11 Effect of punch surface treatments on wear measured in a simulation test More
Image
Published: 01 January 2005
Fig. 26 Thickness of various coatings and surface treatments. PVD, physical vapor deposition; CVD, chemical vapor deposition. Source: Ref 49 More
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006522
EISBN: 978-1-62708-207-5
... corrosion resistance and surface treatment. It describes the thermodynamics of equilibrium oxidation processes and non-equilibrium corrosion processes. The article provides a discussion on aluminum oxidation under atmospheric and dynamic conditions. It presents the potential/pH (Pourbaix) diagram...
Image
Published: 01 January 1994
Fig. 2 Typical plasma surface treatment system More
Image
Published: 01 January 1993
Fig. 14 Effect of surface treatment on the lap shear strength of AS4-APC-2 laminate. Source: Ref 15 More
Image
Published: 01 January 2006
Fig. 10 Comparison of surface treatment techniques. (a) Process temperature of techniques. (b) Surface finish and dimensional tolerance. (c) Abrasive wear resistance. CVD, chemical vapor deposition; PVD, physical vapor deposition. Source: Ref 2 More
Image
Published: 01 August 2013
Fig. 2 Comparison of surface hardness results of various heat treatments and coatings. PVD, physical vapor deposition More
Image
Published: 12 September 2022
Fig. 7 Influence of heat and chemical treatments on surface roughness parameter ( R a ), water and formamide contact angle, and surface energy. SLM, selective laser melting; HF, hydrofluoric acid; HNO 3 , nitric acid. Adapted from Ref 129 More
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003220
EISBN: 978-1-62708-199-3
... Abstract Although stainless steel is naturally passivated by exposure to air and other oxidizers, additional surface treatments are needed to prevent corrosion. Passivation, pickling, electropolishing, and mechanical cleaning are important surface treatments for the successful performance...
Book Chapter

By James E. Hillis
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001310
EISBN: 978-1-62708-170-2
... Abstract Surface treatments are applied to magnesium parts primarily to improve their appearance and corrosion resistance. Mechanical and chemical cleaning methods are used singly or in combination, depending on the specific application and product involved to ensure repetitive reliability...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001312
EISBN: 978-1-62708-170-2
... Abstract Zirconium and hafnium surfaces require cleaning and finishing for reasons such as preparation for joining, heat treatment, plating, forming, and producing final surface finishes. This article provides information on various surface treatment processes, surface soil removal, blast...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003212
EISBN: 978-1-62708-199-3
... Abstract This article is a general introduction to surface engineering of engineering components, providing an overview of the applications of surface treatments and the environmental protection regulations directly or indirectly related to surface engineering processes. engineering...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003114
EISBN: 978-1-62708-199-3
... steels, and precision-cast tool steels. It describes the effects of surface treatments on the basic properties of tool steels, including hardness, resistance to wear, deformation, and toughness. The article provides information on fabrication characteristics of tool steels, including machinability...
Book Chapter

By Om S. Kolluri
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001319
EISBN: 978-1-62708-170-2
... Abstract This article provides an overview of plasma surface treatments for plastics. It covers the equipment and methods used in plasma processing, providing detailed explanations of the plasma discharge reactions and how they affect surface state and topography. It also provides information...
Book Chapter

By Jim Knapp, Don Lemen
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005716
EISBN: 978-1-62708-171-9
... under two basic categories: surface treatments, such as dimensional, non-dimensional, and geometric finishing; and internal treatments, such as sealing, heat treating, and peening. It also describes various inspection and testing methods, including destructive and non-destructive inspections, often...
Book Chapter

By Rajiv Shivpuri, Sailesh Babu, S.L. Semiatin
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003976
EISBN: 978-1-62708-185-6
.... Recommendations on the selection of the materials for hot forging, hot extrusion, cold heading, and cold extrusion are presented. The article discusses the methods of characterizing abrasive wear and factors affecting abrasive wear. It discusses various die coatings and surface treatments used to extend the lives...
Book Chapter

By Jack Snodgrass, Jim Moran
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003674
EISBN: 978-1-62708-182-5
... Abstract This article addresses the general effects of the composition, mechanical treatment, surface treatment, and processing on the corrosion resistance of aluminum and aluminum alloys. There are five major alloying elements: copper, manganese, silicon, magnesium, and zinc, which...
Book Chapter

By Dana Elza, Gene White
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002168
EISBN: 978-1-62708-188-7
... lasers. It discusses the operating parameters of concern in percussion drilling and trepanning. The process variables in surface treatment and laser cutting, as well as the operating parameters of concern in laser welding are reviewed. The article also explains the various categories of surface treatment...
Book Chapter

Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006436
EISBN: 978-1-62708-192-4
... Abstract This article describes the surface modification treatments used to modify the tribological properties of titanium alloys. These include physical vapor deposition and thermochemical conversion treatments. The physical vapor deposition includes ion implantation, sputtering, evaporation...