1-20 of 217 Search Results for

supplemental corrosion protection

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004122
EISBN: 978-1-62708-184-9
... help to meet the army's needs. It includes information on supplemental corrosion protection, which improves the corrosion resistance of a material. References References 1. Holley A.E. , “Aging Systems 'Classic to Geriatric to Jurassic' When Will It Stop?” DoD Maintenance Symposium...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004126
EISBN: 978-1-62708-184-9
.... , Electroplating , McGraw-Hill , 1978 • Winston Revie R. , Ed., Uhlig's Corrosion Handbook , 2nd ed. , John Wiley & Sons , 2000 Level of Required Protection Electroplating Conversion Coating Supplemental Oils Paint Coatings Other Finishes Accelerated Corrosion Tests...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004100
EISBN: 978-1-62708-184-9
... is usually achieved through the use of protective coatings and supplemented by using cathodic protection. Sacrificial anodes are often chosen for offshore platforms because they are simple, rugged, and become effective immediately on platform launch. The primary corrosion protection for ship hulls...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004169
EISBN: 978-1-62708-184-9
... adhesion caused by silicone contamination Fig. 15 Aluminum floor structure corrosion in a 767 at forward entry door Fig. 16 Typical floor structure design for corrosion protection Fig. 17 Protecting aluminum against galvanic corrosion from contact with carbon fiber reinforced...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004164
EISBN: 978-1-62708-184-9
... lightweight metals (aluminum alloys and magnesium) as compared with diesel engines, which use cast iron and steel. Aluminum and cast iron require different inhibitor packages for protection against corrosion. In addition to differences in design and cooling system conditions, use of heavy-duty coolant...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004109
EISBN: 978-1-62708-184-9
... sacrificial anodes impractical. Corrosion control of marine pipelines is usually achieved through the use of protective coatings and supplemental CP. A variety of organic protective coatings can be used. They are usually applied in a factory so that the only field-applied coatings are at joints...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005714
EISBN: 978-1-62708-171-9
... materials Material Resistivity, μΩ • cm Bulk copper 1.68 Hard-drawn copper 1.77 Cold-spray (Acupowder 500) copper 2.39 Twin-wire arc copper 3.05–6.0 Plasma-arc copper 5.45 Source: Ref 19 Corrosion protection for automotive body and chassis structures relies primarily...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002392
EISBN: 978-1-62708-193-1
... 29. U.S. Air Force Personnel, private discussion 30. CFR Title 14, Part 25.609, Protection of Structure 31. “Corrosion Control for Aircraft, Federal Aviation Administration Advisory Circular AC 43-4A, July 1991 32. Bauccia M.L. , “Corrosion Control in the Aircraft Industry...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001461
EISBN: 978-1-62708-173-3
... spray aluminum and zinc coatings has seen a significant increase in the United States during recent years. The corrosion protection provided by these coatings can be as much as an order of magnitude greater than that obtained with traditional coating approaches. In addition, thermal spray coatings can...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004113
EISBN: 978-1-62708-184-9
... Mildly corrosive >10,000 Negligible (very low levels of corrosion) Source: Ref 6 Cathodic protection system characteristics Table 3 Cathodic protection system characteristics   Galvanic (sacrificial) Impressed current External power required None Required Driving...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003698
EISBN: 978-1-62708-182-5
...-diethylaniline 23 N,N-dimethyl-meta-toluidine 52 N,N-dimethyl-para-toluidine 80 N,N-diethyl-ortho-toluidine 15 N,N-diethyl-meta-toluidine 12 N,N-diethyl-para-toluidine 44 Source: Ref 19 Volatile corrosion inhibitors for protection of ferrous metals Table 2 Volatile corrosion...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005851
EISBN: 978-1-62708-167-2
... (uninhibited, nonconductive, i.e., nonautomotive type) mixed with water serves as a buffer and has a filming agent that keeps the water from becoming too aggressive to prevent corrosion. Also, this protects from freeze damage if heat is lost in the plant for an extended period of time. Water that has...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005668
EISBN: 978-1-62708-198-6
... into this category. These metals are thermodynamically unstable in the presence of oxygen or water, and they derive their corrosion resistance from the presence at the surface of a thin oxide film, called the passive film, which acts as a protective barrier between the metal and its environment ( Ref 6 ). Passive...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003614
EISBN: 978-1-62708-182-5
... A. and Praschak E. , “Supplemental Investigation of Protection Afforded by Selected Coating Systems Against Filiform Corrosion,” Research Institute for Pigments and Paints, Stuttgart, Germany, 1996 7. Funke W. , Prog. Org. Coatings , Vol 9 , 1981 , p 29 10.1016/0033-0655(81)80014-3 8...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006413
EISBN: 978-1-62708-192-4
... Sequence IIIF Sequence IIIF Sequence IIIF … (a) Within CI-4, the Mack T-11 is only a requirement for engine oils pursuing the API CI-4 Plus Category Supplement Fig. 4 Pressure traces for normal combustion and preignition from LSPI (low-speed preignition) engine test. Source: Ref 25...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004108
EISBN: 978-1-62708-184-9
... References 1. “Preservation Instructions for MSC Ships,” COMSC 4750.2c, Department of Navy ( www.msc.navy.mil/instructions/doc/47502c.doc , accessed Dec 2005 ) 2. Preiser H.S. , Jacketing and Coating , in Handbook of Corrosion Protection for Steel Structures in Marine Environments...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004134
EISBN: 978-1-62708-184-9
... Protection of Production Platforms in Cold Seawaters,” NACE International , 1981 9. Hughes J. , King G. , and Ganther W. , “The Application of Corrosion Information for the Conservation of Historic Buildings and Artefacts (sic) in Antarctica,” paper presented at the Northern Area...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006405
EISBN: 978-1-62708-192-4
... supplemental inhibitors to protect lubricants under increasingly hostile conditions. Most lubrication applications expose lubricants to oxygen in some manner. The attack of oxygen on the weaker sites in the lubricant, predominantly allylic, benzylic, and tertiary hydrogens, produces peroxy or other...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001462
EISBN: 978-1-62708-173-3
... Aluminum and zinc TSCs have a long history of corrosion protection in structural steel work: Buildings Bridges Towers Radio and TV antenna masts Steel gantry structures High-power search radar aerials Overhead walkways Railroad overhead line support columns Electrification...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006580
EISBN: 978-1-62708-210-5
... very good resistance to corrosion in sand and permanent mold castings and good resistance in die castings. Chemical conversion coating protection is good in die castings and very good in sand and permanent mold castings. The alloys are suitable for marine applications and other uses requiring corrosion...