Published: 30 September 2015
Fig. 30 The conceptual outline of supersolidus liquid-phase sintering densification for three particles: (a) initial particle packing, (b) formation of initial liquid with insufficient wetting of grain boundaries for densification, (c) viscous flow densification of semisolid particles, and (d More
Image
Published: 15 June 2020
including fracture surface micrographs, and two examples showing partial denture framework and small-scale knee (f) before and (g) after sintering. SLPS, supersolidus liquid phase sintering. Source: Ref 48 More
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006117
EISBN: 978-1-62708-175-7
... densification grain boundaries grain growth hot isostatic pressing liquid-phase sintering microstructure phase diagram pressure-assisted sintering sinter forging sintering solid-state sintering spark plasma sintering supersolidus liquid-phase sintering transient liquid-phase sintering uniaxial hot...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006573
EISBN: 978-1-62708-290-7
... carbon at ~1 wt.% facilitated sintering because it led to supersolidus liquid phase sintering (SLPS), thus enhancing densification to a relative bulk density of 99.8%. Optical micrographs from sintered parts at low temperatures (1300 and 1285 °C, or 2372 and 2345 °F) indicated that a porous structure...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006569
EISBN: 978-1-62708-290-7
.... , and Elliott A. , “ Supersolidus Liquid Phase Sintering of H13 Tool Steel Fabricated via Binder Jet Additive Manufacturing ,” in TMS Annual Meeting & Exhibition , 2018 . 59. Liu Y. , Tandon R. , and German R. M. , “ Modeling of supersolidus liquid phase sintering: II...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006582
EISBN: 978-1-62708-290-7
...-base superalloys Inconel 625 and Inconel 718 ( Ref 10 , 33 , 34 ). Sintering studies have considered the influence of powder size distribution on supersolidus liquid-phase sintering ( > 1290 °C, or 2355 °F) as a means for sintering to full density. However, powder size has been found to influence...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003789
EISBN: 978-1-62708-177-1
... equipment and techniques and provides data on etchants and etching procedures. specimen grinding liquid-phase sintering macroexamination metallographic examination microstructure particle size analysis powder metallurgy alloys particle shape analysis specimen polishing specimen preparation...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006364
EISBN: 978-1-62708-192-4
...) ( Ref 64 ). Cemented carbides are generally processed by liquid phase sintering. For wear-protection applications, studs or wear plates made from coarse-grained cemented carbides can be applied on substrate materials by brazing or adhesive bonding. Another method is the deposition of thin coatings...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004002
EISBN: 978-1-62708-185-6
... Duralcan Cast+extruded 2618 Al 2 O 3 20 Ref 9 Chesapeake Composite Corp Liquid-metal infiltration DSC-A1 Al 2 O 3 34, 37 Ref 10 Alcan Cast A359 SiC 20 Ref 11 Treibacher Schleifmittel, Germany Gas pressure infiltration A1 Al 2 O 3 40–55 Ref 12 Not reported Cast...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005808
EISBN: 978-1-62708-165-8
..., and thermokinetic phase transformations. It also describes the influence of cooling rate on laser heat treatment and the effect of processing parameters on temperature, microstructure, and case depth hardness. chemical vapor deposition electroless plating electroplating glazing hardening hardness heat...