Skip Nav Destination
Close Modal
Search Results for
sulfur binary system
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 237 Search Results for
sulfur binary system
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006201
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data sulfur binary system THIS ARTICLE includes systems where sulfur is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which sulfur (S) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006211
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data tellurium binary system THIS ARTICLE includes systems where tellurium is the first...
Abstract
This article is a compilation of binary alloy phase diagrams for which tellurium (Te) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006204
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data selenium binary system THIS ARTICLE includes systems where selenium is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which selenium (Se) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006213
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data titanium binary system THIS ARTICLE includes systems where titanium is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which titanium (Ti) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006207
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data tin binary system THIS ARTICLE includes systems where tin is the first-named element...
Abstract
This article is a compilation of binary alloy phase diagrams for which tin (Sn) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006170
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data potassium binary system THIS ARTICLE includes systems where potassium is the first...
Abstract
This article is a compilation of binary alloy phase diagrams for which potassium (K) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006186
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data sodium binary system THIS ARTICLE includes systems where sodium is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which sodium (Na) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006295
EISBN: 978-1-62708-179-5
... then is discussed in terms of their influence on the activity of carbon, which provides information on the stability of the main carbon-rich phases of iron-carbon alloys, that is, graphite and cementite. Thermodynamics of Binary Fe-<italic>X</italic> Systems The Fe-C, Fe-Si, and Fe-S systems...
Abstract
The control of the solidification process of cast iron requires understanding and control of the thermodynamics of the liquid and solid phases and of the kinetics of their solidification, including nucleation and growth. This article addresses issues that allow for the determination of probability of formation and relative stability of various phases. These include the influence of temperature and composition on solubility of various elements in iron-base alloys; calculation of solubility lines, relevant to the construction of phase diagrams; and calculation of activity of various components. It discusses the role of alloying elements in terms of their influence on the activity of carbon, which provides information on the stability of the main carbon-rich phases of iron-carbon alloys, that is, graphite and cementite. The article reviews the carbon solubility in multicomponent systems, along with saturation degree and carbon equivalent.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006174
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data lithium binary system phase data THIS ARTICLE includes systems where lithium is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which lithium (Li) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006173
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data lanthanum binary system phase data THIS ARTICLE includes systems where lanthanum is the first...
Abstract
This article is a compilation of binary alloy phase diagrams for which lanthanum (La) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006158
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams cesium binary system crystallographic data phase data THIS ARTICLE includes systems where cesium is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which cesium (Cs) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006168
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data mercury binary system phase data THIS ARTICLE includes systems where mercury is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which mercury (Hg) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006160
EISBN: 978-1-62708-163-4
.... For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data dysprosium binary system phase data THIS ARTICLE includes systems where dysprosium...
Abstract
This article is a compilation of binary alloy phase diagrams for which dysprosium (Dy) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006154
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams cerium binary system crystallographic data phase data THIS ARTICLE includes systems where cerium is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which cerium (Ce) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006192
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data lead binary system phase data THIS ARTICLE includes systems where lead is the first-named element...
Abstract
This article is a compilation of binary alloy phase diagrams for which lead (Pb) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006178
EISBN: 978-1-62708-163-4
.... For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data molybdenum binary system phase data THIS ARTICLE includes systems where molybdenum...
Abstract
This article is a compilation of binary alloy phase diagrams for which molybdenum (Mo) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006145
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. arsenic binary system binary phase diagrams crystallographic data phase data THIS ARTICLE includes systems where arsenic is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which arsenic (As) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006193
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data palladium binary system phase data THIS ARTICLE includes systems where palladium is the first...
Abstract
This article is a compilation of binary alloy phase diagrams for which palladium (Pd) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006189
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data nickel binary system phase data THIS ARTICLE includes systems where nickel is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which nickel (Ni) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Book Chapter
Book: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006150
EISBN: 978-1-62708-163-4
... binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams bismuth binary system crystallographic data phase data THIS ARTICLE includes systems where bismuth is the first-named...
Abstract
This article is a compilation of binary alloy phase diagrams for which bismuth (Bi) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.