1-20 of 324 Search Results for

strips

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003179
EISBN: 978-1-62708-199-3
... Abstract This article discusses the operating principles, types, and applications of shearing and slitting of different forms of steel, including plates, flat sheets, bars, coiled sheet and strips. In addition, it provides a detailed account of the cutting methods such as oxyfuel gas cutting...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003094
EISBN: 978-1-62708-199-3
... Abstract Low-carbon steel sheet and strip are used primarily in consumer goods. This article discusses quality descriptors and mechanical properties of low-carbon steel sheet and strip and carbon and low-alloy steel plate. Alloy steel sheet and strip are used primarily for those special...
Book Chapter

By Ted Kostilnik
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001235
EISBN: 978-1-62708-170-2
... shot peening of production parts. It concludes with information on the SAE standard J442 that describes the test strips, strip holder, and gage used in measuring shot peening intensity. cold working compressive stress gage peening intensity shot peening shot propelling equipment shot...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001271
EISBN: 978-1-62708-170-2
... and process classification. continuous electrodeposited coatings continuous electroplated steel continuous plating equipment electrodeposition steel strip CONTINUOUS ELECTRODEPOSITION involves electroplating a pure metal or alloy coating onto an endless steel strip. In practice, this is...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003177
EISBN: 978-1-62708-199-3
... Abstract This article describes the presses that are mechanically or hydraulically powered and used for producing sheet, strip, and plate from sheet metal. It also presents the JIC standards for presses, compares the presses based on power source, details the selection criteria and provides...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005295
EISBN: 978-1-62708-187-0
... Abstract This article discusses the methods, equipment, and theory for pouring, solidifying, and stripping steel ingots. It describes the two basic types of pouring methods: top pouring and bottom pouring. The equipment includes hot tops, ingot molds, and stools. The design of the ingot is...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005286
EISBN: 978-1-62708-187-0
... continuous processes, namely, twin-roll strip casting, slab casting, and wheel-belt processes. It concludes with information on postsolidification processes, including stress relief and scalping. direct chill process solidification twin-roll strip casting wheel-belt process ingot molten-metal...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005288
EISBN: 978-1-62708-187-0
... Abstract This article reviews the history and methods of copper alloy continuous casting. The methods include vertical continuous casting and horizontal continuous casting. The article discusses the upcasting methods used in vertical continuous casting and strip casting used in horizontal...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006024
EISBN: 978-1-62708-172-6
... surface preparation methods that range from simple solvent cleaning to hand and power tool cleaning, dry and wet abrasive blast cleaning, centrifugal wheel blast cleaning, chemical stripping, and waterjetting for the application of the coating system. In addition, the article provides a description of the...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0001832
EISBN: 978-1-62708-181-8
... stripping, organic-solvent cleaning, water-base detergent cleaning, cathodic cleaning, and chemical-etch cleaning. cleaning cracks fractography nondestructive inspection specimen preparation specimen preservation specimen sectioning steel fracture FRACTURE SURFACES are fragile and subject...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003100
EISBN: 978-1-62708-199-3
... Abstract This article describes the types of steels, including high-strength structural carbon steels and high-strength low-alloy steels (HSLA), available in all standard wrought forms such as sheet, strip, plate, structural shapes, bars, bar-size shapes. It discusses the special sections that...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001225
EISBN: 978-1-62708-170-2
... Abstract Molten salt baths are anhydrous, fused chemical baths used at elevated temperatures for a variety of industrial cleaning applications. This article discusses their applications in paint stripping, polymer removal, casting cleaning, glass removal, and plasma/flame spray removal. It...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001249
EISBN: 978-1-62708-170-2
... Abstract This article focuses on the electrodeposition of indium and its alloys, such as indium-antimony, indium-gallium, and indium-bismuth, in nonaqueous indium plating baths. It also provides information on the stripping of indium plate from plated components and presents an overview of the...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003804
EISBN: 978-1-62708-183-2
... agriculture. These products include bars, rods, wires, hot and cold rolled sheets, strip plates, tin mill products, steel tubes, castings, and forgings. The article also provides information on the methods used to prevent or control the rusting of ferrous materials, namely, alloying, coating, and covering...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003159
EISBN: 978-1-62708-199-3
...-expansion alloys are used in various applications such as rods and tapes for geodetic surveying, moving parts that require control of expansion (such as pistons for some internal-combustion engines), bimetal strip, components for electronic devices etc. This article discusses the properties, composition...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003141
EISBN: 978-1-62708-199-3
..., including all operations that convert ingot into general mill products, such as billet, bar, plate, sheet, strip, tube, and wire. The section on secondary fabrication describes processes such as die forging, extrusion, hot and cold forming, machining, chemical milling, and joining. The article presents a...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003217
EISBN: 978-1-62708-199-3
... continuous electrodeposition for steel strip and babbitting and discusses phosphate and chromate conversion coatings as well. It also addresses painting, discussing types and selection, surface preparation, and application methods. In addition, the article describes rust-preventive compounds and their...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001269
EISBN: 978-1-62708-170-2
... applied to the steel strip during the cold-reduction process to facilitate rolling. Normal, unavoidable surface oxidation is the other type. The surface of every processed steel strip has one or both of these contaminants, which must be removed before dip, barrier, or conversion coatings can be applied...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005408
EISBN: 978-1-62708-196-2
... is the occurrence of earing in the production of beverage cans of Al-Mn-Mg alloys ( Ref 1 , Ref 2 , Ref 3 ). It is generally known that the formation of a suitable texture with minimum earing at final gage is critically dependent on the texture in the hot strip and the amount of subsequent cold...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001229
EISBN: 978-1-62708-170-2
... + Fe). In cases of rapid cooling, which can occur with rod and bar, substantial amounts of wustite are retained in the cooled product. When cooling after hot rolling is relatively slow, as it is with coiled strip, magnetite is the main oxide constituent of the scale in the cooled product. Pickling is...