1-20 of 243

Search Results for sputtering deposition

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By S.L. Rohde
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001288
EISBN: 978-1-62708-170-2
... surface. This article provides an overview of the advantages and limitations of sputter deposition. It focuses on the most common sputtering techniques, namely, diode sputtering, radio-frequency sputtering, triode sputtering, magnetron sputtering, and unbalanced magnetron sputtering. The article discusses...
Image
Published: 01 January 1994
Fig. 4 Structure-zone model for sputter-deposited films ( Ref 33 ) More
Image
Published: 01 January 1994
Fig. 5 Columnar morphologies of (a) sputter-deposited stainless steel and (b) vacuum-deposited aluminum films More
Image
Published: 01 January 1994
Fig. 6 Picture of a “nodule” in a thick sputter-deposited chromium film More
Image
Published: 01 January 2005
Fig. 6 Sputter-deposited chromium-niobium and chromium-tantalum alloys. (a) Corrosion rates of alloys compared to pure chromium, niobium, and tantalum. (b) Polarization curves of sputter-deposited chromium-niobium alloys and pure chromium and niobium. The number corresponds to the atomic More
Image
Published: 01 November 1995
Fig. 26 Physical vapor deposition process used to apply coating by sputtering More
Image
Published: 01 January 1994
Fig. 4 Relative effect of deposition temperature and bias on reactively sputter-deposited titanium nitride. A lower resistivity rating indicates that the titanium film is more dense (that is, hard) and stoichiometric. Source: Ref 46 More
Book Chapter

By Alain Dollet
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005434
EISBN: 978-1-62708-196-2
... phenomena in continuous media and transition regime flows of VPP. It explains the methods used for molecular modeling in computational materials science. The article also presents examples that illustrate multiscale simulations of CVD or PVD processes and examples that focus on sputtering deposition...
Book Chapter

By Donald M. Mattox
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001289
EISBN: 978-1-62708-170-2
... particles leaving a source ( Ref 5 , 6 ). This differentiation is important when using sputtering as a source for deposition because reflected high-energy neutrals from the target can have an important effect on the growing film. Figure 1 shows the distance traveled by particles of differing masses (12...
Image
Published: 01 January 1994
Fig. 7 Deposit of sputtered atoms on 4140 sample plasma nitrided at 540 °C (1000 °F) with a load of mechanical components in industrial equipment. Pressure applied during the nitriding cycle was 5 mbar. Etched with 3% nital More
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001352
EISBN: 978-1-62708-173-3
... (PM) sputtering ( Ref 30 , 31 , 32 , 33 ). Prior to deposition, the surface oxide layer may require removal from the base metal in order to achieve adequate adhesion of the silver. The surface oxide layer is usually removed by chemical- or sputter-etching methods. One advantage of vacuum...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005556
EISBN: 978-1-62708-174-0
...) evaporation ( Ref 15 , 19 , 20 , 21 , 22 , 23 , 24 , 25 , 26 ), ion plating using sputtering ( Ref 27 , Ref 28 , 29 ), and planar-magnetron (PM) sputtering ( Ref 30 , Ref 31 , Ref 32 , 33 ). Prior to deposition, the surface oxide layer may require removal from the base metal in order...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001286
EISBN: 978-1-62708-170-2
... deposition (PVD) film can be understood by understanding the film formation process. The formation of a useful and commercially attractive engineered surface using any PVD process (vacuum deposition, sputter deposition, or ion plating) involves several stages: Choice of the substrate (“real surface...
Image
Published: 01 January 1993
Fig. 9 Comparison between the rupture time versus effective (von Mises) stress behavior in shear, at torsional stresses less than the maximum of HHC-deposited silver interlayers, compared with that of tension, calculated using FEM analyses of PM sputter-deposited silver interlayers More
Image
Published: 31 October 2011
sputter-deposited silver interlayers More
Image
Published: 01 January 1994
Fig. 7 Film stress as a function of gas pressure in postcathode magnetron sputter-deposited molybdenum films ( Ref 39 ) More
Image
Published: 01 January 1993
Fig. 2 Effect of interlayer thickness tensile strength of solid-state-welded silver interlayers fabricated using PM sputter deposition and electrodeposition, compared with Ag-4Pd brazed interlayers More
Image
Published: 31 October 2011
Fig. 2 Effect of interlayer thickness on ultimate tensile strength of solid-state-welded silver interlayers fabricated using planar-magnetron sputter deposition and electrodeposition, compared with Ag-4Pd brazed interlayers More
Image
Published: 01 January 1993
Fig. 8 Effective (von Mises) stress-strain behavior for a 150 μm (6 mil) thick silver interlayer ( t / d = 0.024), fabricated using PM sputter deposition, tested in torsion, along with results reported for bulk polycrystalline (annealed) silver More
Image
Published: 31 October 2011
Fig. 8 Effective (von Mises) stress-strain behavior for a 150 μm (6 mils) thick silver interlayer ( t / d = 0.024), cated using planar-magnetron (PM) sputter deposition, tested in torsion, along with results reported for bulk polycrystalline (annealed) silver More