1-20 of 1112

Search Results for special-purpose tool steel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 October 2014
Fig. 9 Hardness of low-alloy special-purpose tool steels after tempering for 2 h More
Image
Published: 01 October 2014
Fig. 10 Tempering characteristics of carbon-tungsten special-purpose tool steels tempered 2 h after being brine quenched More
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005972
EISBN: 978-1-62708-168-9
... discussed include water-hardening tool steels, shock-resisting tool steels, oil hardening cold-work tool steels, low-alloy special-purpose tool steels, and carbon-tungsten special-purpose tool steels. carbon-tungsten special-purpose tool steel cold work tool steel heat treatment oil hardening cold...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003202
EISBN: 978-1-62708-199-3
... steels, high-speed tool steels, low-alloy special-purpose tool steels, and mold steels. The article presents tables that list the temperature ranges, holding time, and hardness values for all of these heat treating processes. heat treating high-carbon high-chromium cold work tool steels high...
Book Chapter

Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002181
EISBN: 978-1-62708-188-7
..., milling, and sawing. The article explains the machining of the following tool steels: water hardening; types A, D and O cold-work; hot work; high speed, low-alloy special-purpose; and low-carbon mold. It details the machining of tool steel gears. The article also discusses the grinding of tool steels...
Book Chapter

By Alan M. Bayer, Lee R. Walton
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001041
EISBN: 978-1-62708-161-0
... steels, including high-speed steels, hot and cold-work steels, shock-resisting steels, and special-purpose steels. Hot-work steels are designed to withstand excessive amounts of heat, pressure, and abrasion, suiting them for punching, shearing, and high-temperature forming applications. Cold-work tool...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003114
EISBN: 978-1-62708-199-3
... Abstract This article discusses the characteristics, composition limits, and classification of wrought tool steels, namely high-speed steels, hot-work steels, cold-work steels, shock-resisting steels, low-alloy special-purpose steels, mold steels, water-hardening steels, powder metallurgy tool...
Book Chapter

Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003979
EISBN: 978-1-62708-185-6
... 2000–2200 980 1800 Low-alloy special-purpose tool steels L1, L2, L6 815 1500 1040–1150 1900–2100 845 1550 L3 815 1500 980–1095 1800–2000 845 1550 Carbon-tungsten special-purpose tool steels F2, F3 815 1500 980–1095 1800–2000 900 1650 Low-carbon mold steels...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003148
EISBN: 978-1-62708-199-3
..., cemented carbides, magnetic materials, low-expansion alloys, and high-speed tool steels. cobalt cobalt alloys corrosion-resistant alloys high-temperature alloys mechanical properties mining special-purpose alloys superalloys uses of cobalt wear-resistant alloys COBALT is a tough silvery...
Book Chapter

By D.A. Stephenson
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002487
EISBN: 978-1-62708-194-8
... in mass and batch production environments. It discusses the factors affecting the total cost of a machining operation, including raw material costs, labor costs, and equipment costs. The article describes three types of machining systems, namely, general-purpose machine tools, production machining systems...
Book Chapter

Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002135
EISBN: 978-1-62708-188-7
... board, tube sheet, and other special-purpose drilling machines. Programmable controllers are also used on some drilling machines and drill heads. Tape-controlled radial, turret, or horizontal drilling machines simplify tooling because a means of holding and positioning the work is the only...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003186
EISBN: 978-1-62708-199-3
..., and outlines the type of costs incurred by the process. It describes the types of machining equipment, including general-purpose machine tools, production machining systems, and computer numerically controlled machining systems. The article lists the common classes of metallic work materials, in order...
Book Chapter

By J.R. Davis
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001306
EISBN: 978-1-62708-170-2
... … S7 … T41907 0.45–0.55 0.20–0.80 0.20–1.00 3.00–3.50 … 1.30–1.80 … 0.20–0.30 (d) … Low-alloy special-purpose tools steels L2 … T61202 0.45–1.00 (b) 0.10–0.90 0.50 max 0.70–1.20 … 0.25 max … 0.10–0.30 … L6 L6 T61206 0.65–0.75 0.25–0.80 0.50 max 0.60–1.20 1.25...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003096
EISBN: 978-1-62708-199-3
..., specially heat treated for high-temperature service A 523 Resistance-welded or seamless steel pipe (plain end) for high-pressure electric cable conduit A 524 (a) Seamless carbon steel pipe for atmospheric service and lower temperatures A 587 (a) Resistance-welded low-carbon steel pipe...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005117
EISBN: 978-1-62708-186-3
... and is encased in tool steel for strength. Hard stock may also be pierced with this type of punch. A large number of special punches are used to create special types and shapes of holes. A blade-type punch is used for piercing long, narrow slots. It consists of a steel blade mounted in a special retainer...
Book Chapter

Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002136
EISBN: 978-1-62708-188-7
... hardness (65 HRC or higher) to obtain optimum surface finish and tool life. Many standard and special reamers are made of solid carbide or contain carbide inserts. Although more expensive than high-speed steel, carbide will often outlast it ten times or more when reaming steel at near-optimum hardness...
Book Chapter

By Gary Adams
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002187
EISBN: 978-1-62708-188-7
... of tool-workpiece welding. Cutting fluids help both by lubricating the tool surfaces and by cooling the tool and workpiece. Cutting Tools In general, high-speed steel tools are suitable. Carbide tools are preferred by some for high-volume, heavy machining at high speeds if the higher tooling costs...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003152
EISBN: 978-1-62708-199-3
... steel-bonded TiCs used for forming tools and other wear components have achieved commercial success for nonmachining applications. Manufacture of Cemented Carbides All cemented carbide components are manufactured by powder metallurgy (P/M) processing. As described below, the important steps...
Book Chapter

By Alan M. Bayer, Bruce A. Becherer
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002121
EISBN: 978-1-62708-188-7
... additions, has relatively little effect on the toughness. For this reason, vanadium-bearing grades are a very good choice when very fast cutting operations are demanded, as in finishing cuts, or when the surface of the material is hard and scaly. The special characteristics of the high-speed tool steels...
Book Chapter

Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002144
EISBN: 978-1-62708-188-7
... as peripheral mills, face mills, end mills, and special mills. Cutters can be of the solid, tipped, or inserted tooth types and have the same materials as single-point tools. Large cutters commonly have teeth of expensive material that are inserted and locked in place in a soft steel or cast iron body...