Skip Nav Destination
Close Modal
By
Charles D. Nelson, Wayne Rasmussen, John Jorstad
By
American Foundry Society Technical Department
By
John Campbell, József Tamás Svidró, Judit Svidró
Search Results for
special patterns
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 1197
Search Results for special patterns
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Published: 31 December 2017
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005308
EISBN: 978-1-62708-187-0
... Abstract This article discusses the types of patterns used for a specific application such as loose patterns, match plate patterns, cope and drag patterns, and special patterns. It describes the principles of the patternmaking techniques used to make expendable molds and for metal casting...
Abstract
This article discusses the types of patterns used for a specific application such as loose patterns, match plate patterns, cope and drag patterns, and special patterns. It describes the principles of the patternmaking techniques used to make expendable molds and for metal casting processes such as die casting and permanent mold casting. The article reviews the pattern features and mold production considerations used in the pattern design, namely, parting line considerations, addition of gates and risers, core prints, and locating points. It examines the pattern allowances for ensuring a dimensionally correct final pattern. A variety of materials and advanced composite materials used in the manufacture of patterns are discussed. The article evaluates the factors influencing the selection of type of patterns for specific castings.
Image
(a) In making the wax pattern for investment molding, special coring proced...
Available to PurchasePublished: 01 December 2008
Fig. 20 (a) In making the wax pattern for investment molding, special coring procedure would be required, to produce radius Y. (b) By permitting the inside corner to be sharp, standard coring will suffice.
More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005255
EISBN: 978-1-62708-187-0
... concludes with information on applications and special versions of the investment casting process. binders casting methods coating inspection investment casting patternmaking plastics pattern tooling pattern and cluster assembly melting equipment Shellvest system ceramic shell molds slurry...
Abstract
This article reviews the pattern materials used in investment casting, which can be loosely grouped into waxes and plastics. The patternmaking process, pattern tooling, and pattern and cluster assembly are described. The article also describes the manufacture of ceramic shell molds and cores, detailing the binders and other materials used, as well as the formulation and control of slurries. Methods for pattern removal, mold firing, melting, casting, postcasting treatment, and inspection are explained. After presenting design recommendations for investment castings, the article concludes with information on applications and special versions of the investment casting process.
Book Chapter
Slurry Molding
Available to PurchaseBook: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005249
EISBN: 978-1-62708-187-0
... sections (≤1.6 mm, or 0.063 in.) can be cast in ceramic molds, using special techniques. Casting surfaces have excellent smoothness—usually 3.2 μm (125 μin.) or better. Dimensional Accuracy Dimensional accuracy depends primarily on the accuracy of the pattern. Metal contraction can normally...
Abstract
This article discusses slurry molding that encompasses two distinct processes: plaster molding and ceramic molding. Plaster mold casting is a specialized casting process used to produce nonferrous castings that have greater dimensional accuracy, smoother surfaces, and more finely reproduced detail. The article describes three generally recognized plaster mold processes, namely, conventional plaster mold casting, the Antioch process, and the foamed plaster process. Ceramic molding techniques are based on processes that employ permanent patterns and fine-grained zircon and calcined, high-alumina mullite slurries for molding. The Shaw process and the proprietary Unicast processes are also discussed.
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003755
EISBN: 978-1-62708-177-1
... system. It discusses the contrasts mechanisms used for imaging and analyzing materials in the SEM. These include the topographic contrast, compositional contrast, and electron channeling pattern and orientation contrast. Special instrumentation and accessory equipment used at elevated pressures...
Abstract
This article outlines the beam/sample interactions and the basic instrumental design of a scanning electron microscopy (SEM), which include the electron gun, probeforming column (consisting of magnetic electron lenses, apertures, and scanning coils), electron detectors, and vacuum system. It discusses the contrasts mechanisms used for imaging and analyzing materials in the SEM. These include the topographic contrast, compositional contrast, and electron channeling pattern and orientation contrast. Special instrumentation and accessory equipment used at elevated pressures and during the X-ray microanalysis are reviewed. The article also provides information on the sample preparation procedure and the materials applications of the SEM.
Image
Tapered hub on this investment cast propeller (a) would require special cor...
Available to PurchasePublished: 01 December 2008
Fig. 22 Tapered hub on this investment cast propeller (a) would require special core pulls to free the wax pattern from undercuts (b). A simplified parting line would be possible if full radii were not required at blade edges (c) and (d).
More
Image
Special coring practice involving additional cost would be required to prod...
Available to PurchasePublished: 01 December 2008
Fig. 27 Special coring practice involving additional cost would be required to produce this investment casting as shown in (a). Normal practice using metal core pins in the pattern die is possible for the casting as shown in (b). Design (b) is less expensive than (a).
More
Image
Special coring practice involving additional cost would be required to prod...
Available to PurchasePublished: 01 December 2008
Fig. 26 Special coring practice involving additional cost would be required to produce this investment casting as shown in (a). Normal practice using metal core pins in the pattern die is possible for the casting as shown in (b). Design (b) is less expensive than (a).
More
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003170
EISBN: 978-1-62708-199-3
... flow diagram of the basic operations for producing a steel casting. Similar diagrams can be applied to other ferrous and nonferrous alloys produced by sand molding The right side of Fig. 1 begins with the task of patternmaking. A pattern is a specially made model of the component...
Abstract
Metal casting is the manufacturing method in which a metal or an alloy is melted, poured into a mold, and allowed to solidify. Typical uses of castings include municipal hardware, water distribution systems (pipes, pumps, and valves), automotive components (engine blocks, brakes, steering and suspension components, etc.), prosthetics, and gas turbine engine hardware. This introduction explains the steps involved in making a casting using a simplified flow diagram, and discusses the ferrous and nonferrous alloys used for metal casting.
Book Chapter
Design for Economical Sand Molding
Available to PurchaseBook: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009018
EISBN: 978-1-62708-187-0
... necessary to produce the outside shape. (See text for discussion.) The pattern for this casting, as originally designed, is shown in Fig. 15(a) . The pattern is made in five sections and requires a special four-part flask. Although the end sections of the flask (for mold sections 1 and 4) may...
Abstract
This article begins with a schematic illustration of basic principles of sand molding. It discusses the general design factors, such as parting lines, location of radii, bosses and undercuts, and rib locations, of sand molding. The article schematically demonstrates alternative design solutions to molding and coring problems and describes the molding sequence. Draft refers to the amount of taper given to the sides of a pattern to enable it to be withdrawn easily from the mold. The article concludes with a simple example demonstrating the influence of a casting requirement on the direction of draft.
Book Chapter
Metalcasting Technology and the Purchasing Process
Available to PurchaseBook: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005188
EISBN: 978-1-62708-187-0
... patterns generally require a greater draft. Under ideal conditions, some patterns as deep as 150 mm (6 in or more may be drawn with almost no draft, using special techniques. Maximum draft should be provided where it does not interfere with desired casting geometry. The metalcasting facility should...
Abstract
This article describes the four basic steps of the purchasing process of cast components. These steps include defining requirements and developing a purchasing plan; requesting and evaluating bids from potential sources; selecting a source and negotiating contract terms; and carrying out the contract and pursuing continuous improvement. It provides guidance on purchasing cast components and explains specific issues and approaches that have proven to be useful in purchasing castings. The article presents a list of the most significant considerations when attempting to determine the overall cost and design requirements of a metal casting.
Book Chapter
Design for Economical Coring
Available to PurchaseBook: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009019
EISBN: 978-1-62708-187-0
...) . Fig. 20 (a) In making the wax pattern for investment molding, special coring procedure would be required, to produce radius Y. (b) By permitting the inside corner to be sharp, standard coring will suffice. Where grooves are required for tool clearance in subsequent machining, the correct...
Abstract
Cores are separate shapes, of sand, metal, or plaster, that are placed in the mold to provide castings with contours, cavities, and passages. Cored holes should be designed simply as the intended function of the casting permits. This article describes the designing of casting for the use of sand cores and to eliminate cores, with illustrations. It provides general rules for designing cored holes in investment castings. The article discusses the general principles of coremaking with illustrations. It concludes with a comparison between coring and drilling.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006519
EISBN: 978-1-62708-207-5
... are details seldom economically justified in aluminum castings, there are instances where special thread forms, serrations or unusual designs are readily obtainable. Usually, investment molds are comprised of dried coats of ceramic slurry and stucco. As an alternative to a wax pattern, a frozen mercury...
Abstract
Investment casting, in which molten metal is poured into hot molds, allows for the production of aluminum parts with extremely thin sections, knife edges and sharp detail. This article describes the various steps in the investment casting process, including patternmaking and dimensioning, the design and manufacture of shell molds, melting and casting methods, and postcasting operations such as knockout, core removal, and cleaning. It also addresses a wide range of design considerations, discusses casting defects, and provides several design examples.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005224
EISBN: 978-1-62708-187-0
... Abstract Semisolid metal (SSM) processing is a special die casting process, where partially solidified metal slurry is injected into a die cavity to form die cast components. This article discusses the flow behavior of an SSM slurry with emphasis on viscosity, rheological behavior, and yield...
Abstract
Semisolid metal (SSM) processing is a special die casting process, where partially solidified metal slurry is injected into a die cavity to form die cast components. This article discusses the flow behavior of an SSM slurry with emphasis on viscosity, rheological behavior, and yield stress. It illustrates the microstructural formation of semisolids under forced convection. The article concludes with an illustration that compares two SSM processes, namely, thixocasting and rheocasting.
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002170
EISBN: 978-1-62708-188-7
... machining, chemical contouring, and chemietching, is a method of processing structural metal parts by controlled chemical etching. The process either thins the parts in specific areas or removes metal from all surfaces. Areas from which metal is not to be removed are protected by special coatings termed...
Abstract
This article discusses the principal process steps, specifications, defects, applications, advantages, and disadvantages of chemical milling (CM) in aerospace industries. The process steps include precleaning, masking, scribing, etching, final cleaning, stripping, and mechanical finishing. The article describes the variables that affect undercut and surface finish obtained by CM. The mechanical properties of chemically milled parts are also discussed.
Book Chapter
Molding and Casting Processes
Available to PurchaseSeries: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006297
EISBN: 978-1-62708-179-5
... Abstract Aggregate molding, or sand casting, is the gravity pouring of liquid metal into a mold that is made of a mixture molded against a permanent pattern. This article summarizes the most important materials in the process of sand casting of cast iron, including different types of molding...
Abstract
Aggregate molding, or sand casting, is the gravity pouring of liquid metal into a mold that is made of a mixture molded against a permanent pattern. This article summarizes the most important materials in the process of sand casting of cast iron, including different types of molding aggregates, clays, water, and additives in green sand, chemically bonded organic resins, and inorganic binders in self-setting, thermosetting, and gas-triggered systems. It discusses three main types of reclamation systems: wet, dry, and thermal. The article concludes with a description of both nonpermanent and permanent mold processes.
Book Chapter
Green Sand Molding
Available to PurchaseBook: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005243
EISBN: 978-1-62708-187-0
... do not have the strength to withstand the pressure exerted during compaction without flexing, the pattern plates are usually mounted against a platen or grid. In most cases, the cope and drag mold halves are filled and compacted with the pattern facing up. Except in the case of special finishing...
Abstract
Green sand molding and chemically bonded sand molding are considered to be the most basic and widely used mold-making processes. This article describes the sand system formulation, preparation, mulling, mold fabrication, and handling of green sand molds. It lists the advantages and disadvantages of green sand molding. The article discusses the primary control parameters for the sand system formulation. It describes two basic types of green sand molds: flask molds and flaskless molds. The article provides a discussion on molding problems, including springback and expansion defects. It considers a variety of sand reclamation systems, including wet washing/scrubbing and thermal-calcining/thermal-dry scrubbing combinations.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001092
EISBN: 978-1-62708-162-7
... (special compositions) A Duplicate patterns for foundry match plates, ceramics, plastics, and pottery C, H, Z Lining and sealing core boxes H Model airplane, railroad, and ship parts G, H, T Spray-metallizing, altering, and repairing patterns and core boxes T, Z Tracer models...
Abstract
This article focuses on the use of indium and bismuth in low-melting-temperature solders and fusible alloys. It describes how the two elements typically occur in nature and how they are recovered and processed for commercial use. It also provides information on designations, classification, composition, properties (including temperatures ranges), and some of the other ways in which indium and bismuth alloys are used.
Book Chapter
Filament Winding
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003039
EISBN: 978-1-62708-200-6
... Abstract Filament winding is a process that allows the precise lay-down of continuous reinforcement in predescribed patterns at a high rate of speed. This article discusses the filament winding process and includes a comparison to other compacting and curing processes. The article describes...
Abstract
Filament winding is a process that allows the precise lay-down of continuous reinforcement in predescribed patterns at a high rate of speed. This article discusses the filament winding process and includes a comparison to other compacting and curing processes. The article describes design factors, and techniques to produce aerodynamic surfaces, improve surface smoothness, and avoid slipping and bridging of filament. The article discusses tooling and the equipment used in the filament winding process, namely, mandrel design, winding machines, tensioners, and ovens.
1