1-18 of 18 Search Results for

sonic thermography

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 January 2003
Fig. 3 Sonic thermography arrangement. (a) Ultrasonic (UT) gun energizes sample. Cork insulators mechanically isolate samples from the backing plate. Infrared (IR) camera captures images. (b) Thermograph from IR camera detects a crack at the root of the slot. More
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006444
EISBN: 978-1-62708-190-0
... Abstract Vibrothermography, also known as sonic thermography, sonic infrared (IR), thermosonics, and vibroacoustic thermography, is a nondestructive evaluation (NDE) technique for finding cracks and delaminations through vibration-induced heating. This article describes the four parts...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003657
EISBN: 978-1-62708-182-5
... active thermography. The components include an excitation source, a thermographic camera, and a computer with software that controls the instrumentation, acquires data, and displays the results. The article discusses the process and experimental setup of sonic thermography used for crack detection...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006453
EISBN: 978-1-62708-190-0
... and selective excitation configuration of the signal-generation mechanisms in thermal nondestructive evaluation methods. The three widely used approaches to TNDE are surface-excited thermography, vibrothermography, and thermoelastic stress analysis. The article provides information on the common features...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006438
EISBN: 978-1-62708-190-0
..., heat input, and high-resolution instrument. IR systems sensitive to surface emissivity Rapid examination of large areas. Can be adapted to production inspections Circuit board solder joints, solar cells, heat transfer equipment, metals, composites, concrete Sonic IR/vibro-thermography, inductive...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.9781627081900
EISBN: 978-1-62708-190-0
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003653
EISBN: 978-1-62708-182-5
... or infrared light, and some unique methods utilizing reflected and amplified light to look at surface topography, triboluminescent sensing, thermography, and the superconducting quantum interference device (SQUID). Reports describing these methods are included in NACE Symposia on corrosion monitoring...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006478
EISBN: 978-1-62708-190-0
... acoustic transducer, radiography, thermography, and low-frequency vibration methods. The article also provides information on NDE methods commonly used for metal-matrix composites. acoustic emission computed tomography digital radiography eddy-current electromagnetic acoustic transducer fiber...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006557
EISBN: 978-1-62708-290-7
... for growth continue to be sought. Thermal Process-Monitoring Methods Thermal techniques collect temperature profiles from irradiated surfaces to help predict areas with less fusion, where defects are likely to be present. Thermal NDE techniques, including infrared thermography and pyrometry, have...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003457
EISBN: 978-1-62708-195-5
..., laminates during repair or high heat exposure Erosion Radome, engine inlet cowl, leading-edge fairing Overstress Overactuation due to system failure Actuated components such as flaps, powered doors Buffeting, sonic fatigue, vibration High sonic areas such as near engines, i.e., flap track...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006936
EISBN: 978-1-62708-395-9
... materials ( Ref 1 – 7 ). The techniques can be used to characterize material discontinuities such as delaminations, cracks, voids, and matrix-rich pockets. It is also possible to visualize fiber orientation, measure changes in material thickness, and determine elastic and sonic properties. Ultrasonic...
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.9781627084390
EISBN: 978-1-62708-439-0
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
... input, and high-resolution instrument. IR systems are sensitive to surface emissivity. Rapid examination of large areas. Can be adapted to production inspections Circuit board solder joints, solar cells, heat-transfer equipment, metals, composites, concrete Sonic IR/vibro-thermography, inductive IR...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006564
EISBN: 978-1-62708-290-7
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.9781627082907
EISBN: 978-1-62708-290-7
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003057
EISBN: 978-1-62708-200-6
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.9781627082006
EISBN: 978-1-62708-200-6
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003068
EISBN: 978-1-62708-200-6