EISBN: 978-1-62708-161-0
... for integrated steel mill operations where ore from the ground is converted into steel. The various refining steps that occur in steelmaking are reviewed. The article also describes solid processing of steel, with emphasis on hot and cold rolling, thermomechanical processing, and annealing of flat steel products...
Book Chapter

Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005765
EISBN: 978-1-62708-165-8
..., compounds, furnaces, and containers used in pack carburizing. The successful operation of the pack carburizing process depends on the control of principal variables such as carbon potential, temperature, time, case depth, and steel composition. The three types of furnaces most commonly used for pack...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005583
EISBN: 978-1-62708-174-0
... to 406 mm (16 in.). 1952—Butt, lap, and T-joints Wallace Rudd and Robert Stanton invented a high-frequency contact welding process for welding a large variety of continuous joints. The Rudd and Stanton system operated at 400 kHz and introduced the high-frequency welding current directly...
Book Chapter

By J.F. Libsch
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001387
EISBN: 978-1-62708-173-3
... for refrigeration and air conditioning using a 7.5 kW solid-state unit operating at a frequency of 100 kHz. Fig. 4 Induction brazing installation that uses a 7.5 kW solid-state induction generator operating at 100 kHz to join brass and stainless steel components for heavy-duty vehicle refrigeration and air...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004136
EISBN: 978-1-62708-184-9
... (MCFCs), and solid oxide fuel cells (SOFCs). The article explains the corrosion processes in fuel cells due to solid-gas interactions, solid-liquid interactions, and solid-solid interactions. It discusses the long-term performance stability and long-term degradation processes of PEMFCs, MCFCs, and SOFCs...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005834
EISBN: 978-1-62708-167-2
... of typically 50 to 60% compared to 85 to 95% for solid-state power supplies using transistors. Besides that, the life expectancy of vacuum tubes was only approximately 4000 h, which was its noticeable drawback. The need to operate with a high voltage (over 10,000 V) made the vacuum tube oscillators more...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001368
EISBN: 978-1-62708-173-3
... In this process, a coil of strip material is first formed into a longitudinal hollow on a forming mill. The two edges of the strip are then HF welded and squeezed together to form a continuous welded seam. Materials that can be successfully HF welded into tube and pipe include carbon steels, stainless steels...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004137
EISBN: 978-1-62708-184-9
... of processes, products, and materials. It embraces any metal work that concerns itself with metal removal, forming, joining, and finishing, such as painting. The treatment of bulk solids and the use of dust collectors were previously addressed. Painting operations include spraying, dipping...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001374
EISBN: 978-1-62708-173-3
... Abstract This article describes the high-temperature solid-state welding process used to join members of similar or dissimilar materials by three stages, namely, primary bonding, bond-surface extension, and elimination of the original joining surface. It lists the various advantages...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005633
EISBN: 978-1-62708-174-0
.... The canisters, which are made from 304L stainless steel, are 610 mm (24 in.) in diameter and 3 m (118 in.) in height. The plug configuration is shown in Fig. 12 relative to the hole of the canister being plugged. The considerable upsetting that occurs during the welding process results in a solid-state weld...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004100
EISBN: 978-1-62708-184-9
... performance, corrosion protection, and corrosion control. While these environments may share similarities with others when organized by unit operation or process, they are typically treated on the basis of the industry, specifically its needs and conditions. However, there are environments where the knowledge...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006412
EISBN: 978-1-62708-192-4
... become an increasingly refined engineering specialty. Manufacturing technology has evolved into a remarkably sophisticated complex of metallurgical, chemical, and mechanical processes. The scale of manufacturing operations ranges from the production of small lots by job-shop methods to the extremely high...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001376
EISBN: 978-1-62708-173-3
... Abstract Explosion welding (EXW) is a solid-state metal-joining process that uses explosive force to create an electron-sharing metallurgical bond between two metal components. This article discusses the process attributes of EXW, including metallurgical attributes, metal combinations, size...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001362
EISBN: 978-1-62708-173-3
... welding aluminum alloys, whereas argon-oxygen and argon-carbon dioxide are used when welding steels. Argon-hydrogen is used when welding stainless steels or when surfacing with them. Procedure Process Operating Procedure The plasma arc is ignited using a pilot arc in a fashion similar...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006789
EISBN: 978-1-62708-295-2
... of a fluid is involved in a tribological process, it is usually called erosion. By definition, both involve progressive loss of material or alteration of material from a solid surface, but erosion requires the mechanical action of a fluid, such as a gas or liquid. Sand blown through a steel pipe at high...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006370
EISBN: 978-1-62708-192-4
..., but they may be inadvisable for precision forming where tolerance or surface finish requirements preclude their application. At the other extreme, many hot forming processes are performed without a lubricant, and tolerances and surface roughness will need to be established in secondary operations...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006042
EISBN: 978-1-62708-175-7
... identical capsules for HIP processing. A typical HIP cycle for tool steels is to hold at 1100 °C (2050 °F) for 4 h at 105 MPa (15 ksi), during which time the powder transforms from a nominal 65% of theoretical density into a fully dense pore-free solid. Rapid cooling rates characteristic of gas atomization...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005552
EISBN: 978-1-62708-174-0
... Consumable Electrode Arc Welding Processes A gas-shielded cousin of GTAW is GMAW, in which a continuous solid-wire welding electrode is intended to be consumed to become filler metal for the weld. The process is operated in DCRP to take advantage of the concentration of heat at the tip of the welding...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006403
EISBN: 978-1-62708-192-4
... the components (materials, lubricant, and environment) involved in the friction and wear process and their physical, chemical, and technological properties Operational parameters , such as stress type, load, deformation velocity, temperature, and their functional duration Interaction parameters , which...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005598
EISBN: 978-1-62708-174-0
... and argon-carbon dioxide are used when welding steels. Argon-hydrogen is used when welding stainless steels or when surfacing with them. Procedure Process Operating Procedure The plasma arc is ignited using a pilot arc in a fashion similar to that of a PAW system. The main arc is transferred from...