1-20 of 483 Search Results for

solid metal induced embrittlement

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003554
EISBN: 978-1-62708-180-1
... Abstract Metal-induced embrittlement is a phenomenon in which the ductility or fracture stress of a solid metal is reduced by surface contact with another metal in either liquid or solid form. This article summarizes the characteristics of solid metal induced embrittlement (SMIE) and liquid...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006786
EISBN: 978-1-62708-295-2
... Abstract Metal-induced embrittlement is a phenomenon in which the ductility or the fracture stress of a solid metal is reduced by surface contact with another metal in either the liquid or solid form. This article summarizes some of the characteristics of liquid-metal- and solid-metal-induced...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003636
EISBN: 978-1-62708-182-5
... Abstract Embrittlement that occurs below the melting point of the embrittling species is known as solid metal induced embrittlement (SMIE) of metals. This article provides a discussion on the characteristics and investigations of SMIE, liquid metal induced embrittlement, and delayed failure...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003632
EISBN: 978-1-62708-182-5
... to as hydrogen embrittlement), liquid-metal embrittlement, and solid metal induced embrittlement. In general, these different phenomena show many similarities, and it would at first seem appropriate to propose an all-encompassing mechanism to account for these behaviors. For example, all of these phenomena...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003603
EISBN: 978-1-62708-182-5
... is often externally applied. For hydrogen damage, liquid metal induced embrittlement, and solid metal induced embrittlement, the stress is induced by reactions with the environment. Microbiologically Influenced Corrosion The final article “Microbiologically Influenced Corrosion,” discusses...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003635
EISBN: 978-1-62708-182-5
... Abstract Liquid metal induced embrittlement (LMIE) is the reduction of the fracture resistance of a solid material during exposure to a liquid metal. This article discusses the mechanisms and occurrence condition of LMIE and describes the effects of metallurgical factors, such as grain size...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.9781627081832
EISBN: 978-1-62708-183-2
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006540
EISBN: 978-1-62708-183-2
... Institute of Standards and SLPR self-linear polarization resistance SMIE solid metal induced embrittlement resistance Technology SRB sulfate-reducing bacteria; solid rocket IUPAC International Union of Pure and nm nanometer No. number booster (space shuttle) Applied Chemistry NSF National Sanitation...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006828
EISBN: 978-1-62708-329-4
...; it does not have to be a result of retained flux residue. Liquid Metal Induced Embrittlement and Solid Metal Induced Embrittlement Liquid metal induced embrittlement (LMIE) and solid metal induced embrittlement (SMIE) should always be considered in a failure involving a braze joint. (Articles about...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003719
EISBN: 978-1-62708-182-5
... hydrogen electrode ep plastic strain range mm millimeter SLPR self-linear polarization resistance et total strain range mol mole SMIE solid metal induced embrittlement g overpotential MPa megapascal SRB sulfate-reducing bacteria; solid rocket lm micron (micrometer) mpy mils per year m kinematic viscosity...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0005547
EISBN: 978-1-62708-161-0
... quenched SMill solid-metal-induced embrittlement WRC Welding Research Council B, p beta SNECMA Societe Nationale d'Etude et yr year o angular measure; degree r, 'Y gamma de Construction de Moteurs 'C degree Celsius (centigrade) SPC statistical process control °F degree Fahrenheit 4, o delta SQ structural...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006777
EISBN: 978-1-62708-295-2
... Hydrogen embrittlement by grain-boundary absorption of hydrogen Stress-corrosion cracking, can be intergranular or transgranular Liquid metal induced embrittlement, for example, mercury in brass, lithium in 304 stainless steel Solid metal induced embrittlement Low-melting-temperature elements...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003225
EISBN: 978-1-62708-199-3
... are shown for each temperature. Brittle fractures can occur by either transgranular or intergranular cracking. Intergranular fractures are specific to certain conditions that induce the embrittlement, such as temper embrittlement, hydrogen embrittlement, stress-corrosion cracking, and liquid-metal...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001039
EISBN: 978-1-62708-161-0
... form of embrittlement and influences the behavior and properties of nearly all ferrous alloys and many metals. The article explains why hydrogen embrittlement is so widespread and reviews the many types of damage it can cause. It also explores other forms of embrittlement, including metal-induced...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.9781627081825
EISBN: 978-1-62708-182-5
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.9781627081801
EISBN: 978-1-62708-180-1
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003540
EISBN: 978-1-62708-180-1
... absorption of hydrogen Stress-corrosion cracking (sometimes) Liquid metal induced embrittlement (LMIE), for example, mercury in brass, lithium in 304 stainless steel Solid metal induced embrittlement (SMIE) The following sections describe more detail of some typical embrittlement mechanisms...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003543
EISBN: 978-1-62708-180-1
... of an overload failure. It also presents examples of thermally and environmentally induced embrittlement effects that can alter the overload fracture behavior of metals. atomic structure brittle cracking crack propagation crystalline structure ductile cracking ductility environmentally induced...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0006548
EISBN: 978-1-62708-180-1
... SIMS secondary ion mass spectroscopy SLC sustained load cracking SMAW shielded metal arc welding SMIE solid metal induced embrittlement S-N stress-number of cycles SRB sulfate-reducing bacteria SSC sulfide-stress cracking tc critical thickness T thickness T throat T temperature Tc recrystallization...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2
... the likelihood of overload fractures are included. The article focuses primarily on the contribution of embrittlement to overload failure. The embrittling phenomena are described and differentiated by their causes, effects, and remedial methods, so that failure characteristics can be directly compared during...