1-20 of 312 Search Results for

single edge notch bending testing

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003256
EISBN: 978-1-62708-176-4
... of plastics include the short-term tensile test, the compressive strength test, the flexural strength test, and the heat deflection temperature test. The most commonly used tests for impact performance of plastics are the Izod notched-beam test, the Charpy notched-beam test, and the dart penetration...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002400
EISBN: 978-1-62708-193-1
...-point bend ( Ref 24 ), notched four-point bend ( Ref 25 , 26 ), and cantilever beam ( Ref 27 , 28 , 29 ) specimens have all been used, and they have in common a maximum applied surface tensile stress and decreasing tensile stress with increasing distance into the specimen. Axial fatigue testing of...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003308
EISBN: 978-1-62708-176-4
... previously noted, the specimen in the Charpy test is supported on both ends and is broken by a single blow from a pendulum that strikes the middle of the specimen on the unnotched side. The specimen breaks at the notch, the two halves fly away, and the pendulum passes between the two parts of the anvil. The...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003257
EISBN: 978-1-62708-176-4
..., tensile, compressive, hardness, torsion and bend, shear load, shock, and fatigue and creep testings. It describes the design criteria for combined properties derived from each of the mechanical testing. The article concludes with a discussion on the effect of environment on the mechanical properties...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005149
EISBN: 978-1-62708-186-3
... Abstract Sheet metal forming operations are so diverse in type, extent, and rate that no single test provides an accurate indication of the formability of a material in all situations. This article presents an overview of types of forming, formability problems, and principal methods of...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003311
EISBN: 978-1-62708-176-4
... on ceramics and CMCs: single edge notch bending, compact tension, double cantilever beam testing, chevron notch methods, and double torsion. It presents descriptions organized by their specimen types, and includes the advantages and disadvantages, as well as the experimental control schemes employed...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003269
EISBN: 978-1-62708-176-4
..., or rotation of the test section, the specimen is mounted in a jig ( Fig. 8 ). A novel alternative is shown in Fig. 9 in which the test specimen is subjected to normal and bending forces that minimize shear stress concentrations at the notches and provide a uniform shear stress between the notches...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003391
EISBN: 978-1-62708-195-5
... shown significant benefit. These include notched (open and/or filled hole) tension and compression, inter/intralaminar shear and tension, and pin bearing. structural sizing test-analysis correlation notched compression intralaminar shear intralaminar tension notched tension pin bearing...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003310
EISBN: 978-1-62708-176-4
... and B and b are the dimensions of the specimen in the plane of the crack. Testing is most commonly performed on single-edge notched bend or on compact tension specimens containing machined notches (see Fig. 2 in the article “Fracture Toughness Testing” in this Volume). ASTM E 1737 specifies that...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002360
EISBN: 978-1-62708-193-1
... middle-tension M(T) geometries. Single-edge bend SE(B), arc-shaped A(T), and disk-shaped compact DC(T) specimen geometries and their K -calibrations are discussed in ASTM E 399. Comparable tolerances should be specified for “nonstandard” specimens. The selection of an appropriate geometry requires...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003325
EISBN: 978-1-62708-176-4
... Abstract This article discusses the standard test methods that can be applied to many types of welds: tension, bending, impact, and toughness testing. It provides information on four qualification stages, namely, the weld material qualification, base material qualification, the weld procedure...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006761
EISBN: 978-1-62708-295-2
... techniques and discusses the advantages and limitations of each technique when used in failure analysis. The focus is on various types of static load testing, hardness testing, and impact testing. The testing types covered include uniaxial tension testing, uniaxial compression testing, bend testing, hardness...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003314
EISBN: 978-1-62708-176-4
... fatigue testing machines and bending fatigue machines. Load cells, grips and alignment devices, extensometry and strain measuring devices, environmental chambers, graphic recorders, furnaces, and heating systems of ancillary equipment are discussed. The article presents technologies available to...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009007
EISBN: 978-1-62708-185-6
..., compression test, and bend test. It examines specialized tests including plane-strain compression test, partial-width indentation test, secondary-tension test, and ring compression test. The article explains that workability is determined by two main factors: the ability to deform without fracture and the...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003436
EISBN: 978-1-62708-195-5
... Abstract This article introduces the principal methodologies and some technologies that are being applied for nondestructive evaluation of composite materials. These include ultrasonic testing (UT), air-coupled UT, laser UT, ultrasonic spectroscopy, leaky lamb wave method, acousto...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001034
EISBN: 978-1-62708-161-0
... welds. The major tests that are discussed in this article are weld tension test, bend test, the drop-weight test, the Charpy V-notch test, the crack tip opening displacement test, and stress-corrosion cracking test. arc welding cold cracking fabrication hot cracking low-alloy steels...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003312
EISBN: 978-1-62708-176-4
... test methods described in ASTM C 1421. Each bar represents the mean plus or minus one standard deviation. SEPB, single-edge precracked beam; SCF, surface crack in flexure; CNB, chevron notched beam. Adapted from Ref 18 Fig. 16 Comparison of fracture-toughness test results from multiple...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002380
EISBN: 978-1-62708-193-1
... model for the other discussions. The details of this test can be found in Ref 6 . The first element of the test is the selection of a test specimen. Five different specimen geometries are allowed. These are the single edge-notched bend specimen, SE(B), compact specimen, C(T), arc-shape tension...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.9781627081764
EISBN: 978-1-62708-176-4
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003306
EISBN: 978-1-62708-176-4
... and unloading of the specimen, that is, fatigue loading. Refer to ASTM E 399 ( Ref 6 ) for details on precracking. Fig. 2 Specimen types used in the K Ic test (ASTM E 399). (a) Single edge-notched bend, SE(B). (b) Compact specimen, C(T). (c) Arc-shaped tension specimen, A(T). (d) Disk-shaped...