Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005252
EISBN: 978-1-62708-187-0
... molding and green sand molding. casting dimensional accuracy green sand molding shell molding tensile strength mold cracking soft molds peelback mold shift shell coremaking sand reclamation resin-sand properties mold defects mold patterns THE SHELL PROCESS was first developed...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005242
EISBN: 978-1-62708-187-0
..., namely, ceramic shells and rammed graphite, for casting reactive metals such as titanium or zirconium. ceramic shells coremaking green sand operations titanium zirconium clay resin-bonded sand systems no-bake binder systems heat-cured binder systems cold box binder systems rammed graphite...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005244
EISBN: 978-1-62708-187-0
... the shell process). The shell (Croning) process—which is one of the more prevalent binder methods—is detailed in the next article, “Shell Molding and Shell Coremaking,” in this Volume. Core Baking (Oil Sand) Oil-sand mixtures are used for cores in sand molds, and by varying their composition...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005354
EISBN: 978-1-62708-187-0
... Abstract No-bake sand molds are based on the curing of inorganic or organic binders with either gaseous catalysts or liquid catalysts. This article reviews the major aspects of no-bake sand bonding in terms of coremaking, molding methods, and sand processing. It discusses the points to be noted...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005308
EISBN: 978-1-62708-187-0
... of coremaking process used and the number of cores required. Sand cores that develop strength during the high-temperature curing of thermal-setting binders (shell hot box and warm box cores) require heat-conducting metal core boxes. (Core sand binder systems and coremaking machines are discussed in the article...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003172
EISBN: 978-1-62708-199-3
... Chromite sand Zircon sand Heat-cured resin binder processes Shell process (Croning process) Furan hot box Phenolic hot box Warm box (furfuryl/catalyst) Oven bake (core oil) Cold box resin binder processes Phenolic urethane Furan/SO 2 Free radical cure (acrylic/epoxy...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005186
EISBN: 978-1-62708-187-0
... on a part are also possible, ranging from a rougher as-cast surface of sand-molded casting to the smoother surfaces obtained through shell molding, investment casting, or other casting methods. In general, casting can provide various functional advantages for component design that include: Design both...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006297
EISBN: 978-1-62708-179-5
..., such as causticized lignite and graphitic materials ( Ref 18 , 19 ). Water-absorbent materials, such as wood flour, oat hulls, peanut shells, and so on, are examples of cellulose-based additives. They are added to green sand to capture free moisture. Sand mixtures containing cellulose exhibit better static flow...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009019
EISBN: 978-1-62708-187-0
... for the use of sand cores and to eliminate cores, with illustrations. It provides general rules for designing cored holes in investment castings. The article discusses the general principles of coremaking with illustrations. It concludes with a comparison between coring and drilling. castings drilling...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005334
EISBN: 978-1-62708-187-0
... pouring magnesium molding sands machining characteristics high-temperature alloys MAGNESIUM ALLOY CASTINGS can be produced by nearly all of the conventional casting methods, namely, sand, permanent, and semipermanent mold and shell, investment, and die casting. The choice of a casting method...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009020
EISBN: 978-1-62708-187-0
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005299
EISBN: 978-1-62708-187-0
... (principally shell molding and no-bake), approximately 30% of cast steel tonnage Permanent molding (32%), typically to produce carbon steel railroad wheels in graphite molds Small amounts of cast steel are also produced by investment casting (3%), centrifugal casting (3%), and lost foam (0.4...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005326
EISBN: 978-1-62708-187-0
... -bonded sand, or resin-bonded sand (shell molds) on equipment ranging from highly mechanized or automated machines to that required for floor or hand molding methods, depending on the size and number of castings to be produced. Cores are generally produced in cold-box-type bonded sand on highly automated...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006333
EISBN: 978-1-62708-179-5
... is done in the primary melting furnace. Molds are produced in green sand, silicate CO 2 -bonded sand, or resin-bonded sand (shell molds) on equipment ranging from highly mechanized or automated machines to that required for floor or hand molding methods, depending on the size and number of castings...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005243
EISBN: 978-1-62708-187-0
... are shell molding and no-bake molding. The shell and no-bake methods are discussed in subsequent articles in this Volume. The base aggregates and types of binders are discussed in the article “Aggregates and Binders for Expendable Molds” in this Volume. Some advantages of green sand molding include...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
.... In shell-mold castings of gray iron, the high thermal conductivity of the mold produces an initial chill of the iron surface. Subsequent annealing of the surface by the heat of the casting results in a skin that is almost 100% ferrite; such a skin has poor wear properties and should be removed by machining...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.9781627081993
EISBN: 978-1-62708-199-3