1-6 of 6 Search Results for

semisolid thixomolded AZ91D

Sort by
Image
Published: 01 December 2008
Fig. 1 Microstructures of semisolid Thixomolded AZ91D at solid α prim levels of (a) 4.4%, (b) 28%, and (c) >60%. (d) Distribution of α prim , α pro , α eut , and β eut . (e) Transmission electron micrograph of α eut and β More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005275
EISBN: 978-1-62708-187-0
... is discussed. The article provides information on thixoblending and summarizes results from two independent studies of the mechanical properties of recycled AZ91D. It also describes the factors on which the mechanical properties depend and illustrates microstructures of semisolid thixomolded AZ91D...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003790
EISBN: 978-1-62708-177-1
... the remainder. Source: Ref 7 Magnesium Alloys Although numerous magnesium casting alloys have wide freezing ranges, reported research related to magnesium semisolid metalworking focuses on either AZ91D or AM60B. The chemical compositions of additional magnesium die-casting alloys are presented...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003774
EISBN: 978-1-62708-177-1
...—as fabricated O—annealed H10 and H11—slightly strain hardened H23, H24, and H26—strain hardened and partially annealed T4—solution heat treated T5—artificially aged only T6—solution heat treated and artificially aged T8—solution heat treated, cold worked, and artificially aged For example, AZ91D-F...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005334
EISBN: 978-1-62708-187-0
... AS21A 2.25 0.35 1.0 … … … bal AS21B 2.25 0.10 1.0 … … … bal AS41A 4.25 0.35 1.0 … … … bal AS41B 4.25 0.50 (a) 1.0 … … … bal AZ91A 9.0 0.13 min … … 0.7 … bal AZ91B 9.0 0.13 min … … 0.7 … bal AZ91D 9.0 0.30 (a) … … 0.7 … bal AE44 4.0...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003138
EISBN: 978-1-62708-199-3
... slugs. The “thixomolding” process, which combines the features of die casting and injection molding, is being used to produce alloy AZ91D battery cases for electric vehicles. Sand and Permanent Mold Casting Alloys Several systems of magnesium alloys are available for sand and permanent mold...