Published: 01 December 2008
Fig. 3 Schematic of Massachusetts Institute of Technology's Semisolid Rheocasting (SSR) process. Source: Ref 2 More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005274
EISBN: 978-1-62708-187-0
... Abstract This article illustrates various rheocasting processes. These include new rheocasting, semisolid rheocasting, subliquidus casting, rheo-diecasting, swirled enthalpy equilibration device process, slurry-on-demand process, and continuous rheoconversion processes. rheocasting...
Image
Published: 01 December 2008
Fig. 5 Schematic of the rheocasting semisolid metal (SSM) route compared to thixocasting. MHD, magnetohydrodynamic; GR, grain refining More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005272
EISBN: 978-1-62708-187-0
...: thixocasting, rheocasting, and thixomolding. rheocasting semisolid metal casting thixocasting thixomolding SEMISOLID METAL (SSM) PROCESSING, also known as semisolid metal casting, semisolid forming, or semisolid metal forging, is a special die casting process wherein a partially solidified metal...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006498
EISBN: 978-1-62708-207-5
... claimed for semisolid casting. It describes the four notable processes used to produce semisolid castings: thixocasting, rheocasting, thixomolding, and wrought processes. Most commercial aluminum semisolid casters use either thixocasting or rheocasting. The article discusses the die design, process...
Image
Published: 01 January 1990
Fig. 9 Semisolid-metal processing with a rheocaster. Commercial semisolid-metal processing is based on thixocasting. More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005224
EISBN: 978-1-62708-187-0
... stress. It illustrates the microstructural formation of semisolids under forced convection. The article concludes with an illustration that compares two SSM processes, namely, thixocasting and rheocasting. microstructual formation rheocasting semisolid metal processing thixocasting viscosity...
Image
Published: 01 December 2008
Fig. 7 Schematic of semisolid metal (SSM) processing routes: thixocasting versus rheocasting. MHD, magnetohydrodynamic; GR, grain refinement More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005187
EISBN: 978-1-62708-187-0
..., such as die casting, squeeze casting, and semisolid processing. The article contains tables that compare some of the typical capabilities of shape casting processes. casting ceramics die casting sand squeeze casting plaster graphite molding SHAPE CASTING, as a metal-forming process, both...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003790
EISBN: 978-1-62708-177-1
..., followed by flash and overflow removal in a trim press. Fig. 2 Typical indirect semisolid metalworking manufacturing cell Direct Processes Direct processes, usually termed rheocasting, avoid the production and reheating of billet stock material. The semisolid metal mixture is produced...
Book Chapter

By Justin Heimsch
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005273
EISBN: 978-1-62708-187-0
... to describe processes that require specially processed billet material that is reheated to the semimolten state just before injection ( Ref 2 ). Alternatively, processes that create semisolid structures directly from the liquid state are referred to as rheocasting ( Ref 2 ). The goal of this article...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006574
EISBN: 978-1-62708-210-5
... die casting and its derivatives processes, such as semisolid metalcasting (thixocasting), slurry-on-demand (rheocasting), and squeeze casting. Fluidity in die casting is somewhat lower than Silafont-36 (alloy 365.0), due to its lower silicon content. However, the tendency for shrinkage formation...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005266
EISBN: 978-1-62708-187-0
... castings are shown in Fig. 2 . There are three different types of high-integrity die casting processes: squeeze casting, semisolid casting, and high-vacuum die casting. Fig. 2 Typical semisolid high-integrity die casting products. Courtesy of NADCA ( Ref 1 ) Squeeze Casting Squeeze...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001061
EISBN: 978-1-62708-162-7
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005287
EISBN: 978-1-62708-187-0
..., and semisolid forming based on rheocasting/thixocasting principles. Of these casting methods, high-pressure die casting of aluminum is the dominant nonferrous casting process ( Fig. 1 ). Fig. 1 Nonferrous casting processes by tons poured. Source: From data of AFS 2002 survey. This article provides...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006488
EISBN: 978-1-62708-207-5
... in a mold by various casting methods. Virtually every casting method that can be used with unreinforced aluminum has been used with DRA composites. These include the sand, gravity die (permanent mold), investment, squeeze, and lost foam casting processes as well as high-pressure die casting. A semisolid...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003420
EISBN: 978-1-62708-195-5
... materials can also be run with or without vacuum. Flow Characteristics Aluminum MMCs may be up to 50 times more viscous than their matrix alloy due to the fact that they are semisolid materials (molten metal/solid particle mixtures). The thixotropic behavior of these aluminum semisolid composites can...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003172
EISBN: 978-1-62708-199-3
... Horizontal centrifugal casting Hybrid processes Squeeze casting Semisolid metal casting (rheocasting) (a) When sand or plaster complex cores are used instead of metal cores, the term semipermanent mold casting should be used. Of the expendable mold/permanent pattern processes...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5
... include molding and pattern distinctions such as lost foam (evaporative pattern), shell and V-mold, and process derivatives such as squeeze casting, low-pressure permanent mold, vacuum riserless casting, and semisolid forming based on rheocasting/thixocasting principles. Of these casting methods, high...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005331
EISBN: 978-1-62708-187-0
... of the solidification time. Nondendritic Microstructures Emerging casting processes include thixocasting and rheocasting. Both are variants of semisolid metal casting and have evolved from work at the Massachusetts Institute of Technology in the 1970s. Both variants are capable of creating a nondendritic...