1-20 of 113 Search Results for

semi-continuous furnaces

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001386
EISBN: 978-1-62708-173-3
... brazing and reviews three types of furnaces: continuous, semi-continuous, and batch. It presents three examples of the industrial applications of the furnace brazing: vacuum devices, jet engines, and automotive industries. The health and safety guidelines to be followed during the furnace brazing are also...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005274
EISBN: 978-1-62708-187-0
...-Solid Processing of Alloys and Composites , ( Limassol, Cyprus ), 2004 6. Pan Q.Y. , Findon M. , and Apelian D. , “The Continuous Rheoconversion Process (CRP): A Novel SSM Approach,” Eighth International Conference on Semi-Solid Processing of Alloys and Composites , ( Limassol...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003808
EISBN: 978-1-62708-183-2
... based on 5 year exposure data Test site Ten year corrosion loss Hot-dip galvanized Type I aluminized Type II aluminized g/m 2 mils μm g/m 2 mils μm g/m 2 mils μm Porter County, IN (semi-industrial) 121.6 0.68 17.2 14.7 0.19 4.9 8.5 0.10 2.6 East Chicago...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006518
EISBN: 978-1-62708-207-5
... extrusion profile Full utilization of this capability of the extrusion process depends on the ingenuity of designers in creating new and useful configurations. Profiles are classified with respect to producibility into solid, hollow, and semi-hollow types, and further classified by rules based...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005784
EISBN: 978-1-62708-165-8
... manually by simply painting with a flat, soft brush. At the same time, stop-off paints can be tailored to the customer's needs, which allows a variety of modern semi- or fully automatic application technologies. Prior to application of any of these technologies, proper mixing of the paint is of utmost...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006136
EISBN: 978-1-62708-175-7
... V.S. , and Duz V.A. , “Semi-Continuous Magnesium-Hydrogen Reduction Process for Manufacturing of Hydrogenated,” Purified Titanium Powder , U.S. Patent No. 8,007,562 , filed 12/29/2008, issued 08/30/2011 11. Klevtsov A.G. , Nikishin A.M. , Shuvalov J.V. , Moxson V.S...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006498
EISBN: 978-1-62708-207-5
..., and Properties Commercial Castings References References 1. Flemings M.C. , Behavior of Metal Alloys in the Semi-Solid State , Met. Trans. A , Vol 22A ( No. 5 ), 1991 , p 957 – 981 10.1007/BF02661090 2. Kirkwood D.H. , Semisolid Metal Processing , Inter. Mater. Rev...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004022
EISBN: 978-1-62708-185-6
...Tabulation of optimal die semi-angle versus ram velocity Table 1 Tabulation of optimal die semi-angle versus ram velocity Ram velocity, mm/s Optimal die semi-angle, (θ) Objective function, J ( t ) Center burst, F 30 68 29 −0.19 40 62 29 −0.10 50 56 29 −0.03 60...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005902
EISBN: 978-1-62708-167-2
... refractory: Ramming with a semi-elastic mass (usually phosphate-bonded ramming masses on corundum bases with additives to improve the resistance to slag) Bricking with cinder blocks on corundum bases Casting masses (low or ultralow cement types, with low water contents) Apart from the dry...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006118
EISBN: 978-1-62708-175-7
... of the ceramic tiles, as well as excessive distortion of sintered parts. Excessive grain growth is also an undesirable outcome of very high sintering temperatures. Vacuum furnaces can be batch or semi-continuous. Reduction of interstitials (C, O, N) is highly effective in vacuum sintering, and the quality...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006529
EISBN: 978-1-62708-207-5
...Abstract Abstract Brazing technology is continually advancing for a variety of metals including aluminum and its alloys and nonmetals. This article discusses the key physical phenomena in aluminum brazing and the materials for aluminum brazing, including base metals, filler metals, brazing...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006280
EISBN: 978-1-62708-169-6
... Mn; 0.10–0.65 S; 0.10 B; 0.10 Zr; 0.10 C; 0.10 Ti C84030 82.0–89.0 2.0–4.0 0.09 5.0–14.0 0.40 1.0–1.5 0.50–2.0 … … 0.05 P; 0.20 Mn; 0.10–0.65 S; 0.10 B; 0.10 Zr; 0.10 C; 0.10 Ti Semi-red and leaded semi-red cast brasses C84200 78.0–82.0 4.0–6.0 2.0–3.0 10.0–16.0 0.4 0.25...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006276
EISBN: 978-1-62708-169-6
...–C82800 >94% Cu Red and leaded red brasses C83300–C83810 Cu-Sn-Zn-Pb (82–94% Cu) Semi-red and leaded semi-red brasses C84200–C84800 Cu-Sn-Zn-Pb (75–82% Cu) Yellow and leaded yellow brasses C85200–C85800 Cu-Zn-Pb Manganese bronzes and leaded manganese bronzes (e) C86100–C86800 Cu...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005643
EISBN: 978-1-62708-174-0
... of engineering Gas metal arc welding (flux cored wire) Arc Direct current; electrode positive Flux is enclosed in tubular electrode of small diameter; automatic or semi-automatic; wire fed continuously through a gun with or without a gas shield Slag and gas, either self-generated or from external source...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005898
EISBN: 978-1-62708-167-2
... of Classical Problems Using the Heat Diffusion Equation Cases for Semi-Infinite Solid (x≥ 0) with Initial Temperature <italic>T</italic>(<italic>x</italic>, 0) = <italic>T</italic><sub><italic>i</italic></sub> For constant surface temperature T (0, t ) = T s : (Eq 47) T ( x , t...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005975
EISBN: 978-1-62708-168-9
.... However, except for thin tools, which are air-quenched between plates to keep them straight, it is customary to quench in oil from muffle or semi-muffle furnaces in molten salt from a high-temperature salt bath or with pressurized nitrogen in vacuum furnaces. After its temperature has been equalized...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005961
EISBN: 978-1-62708-168-9
... ) that are widely used in specific applications. Three basic classes of PH stainless steels are: Austenitic PH stainless steels (e.g., A-286) Semi-austenitic PH stainless steels (e.g., 17-7 PH) Martensitic PH stainless steels (e.g., 17-4 PH) Composition of selected AISI standard precipitation...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003420
EISBN: 978-1-62708-195-5
.... This combined with the fact that semi-solid materials are more viscous than their aluminum-matrix alloy means that they enter the die cavity with much less turbulence and less entrapped air. To best use the thixotropic behavior of aluminum MMCs, a minimum gate velocity of 30 m/s (100 ft/s) is recommended...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006374
EISBN: 978-1-62708-192-4
... Porous iron powder 15 60 Total 100 100 Metallic content &gt;75% &gt;75% Examples of organic resin-bonded brake formulations Table 2 Examples of organic resin-bonded brake formulations Component Formulation, wt% NAO Low-met Semi-metallic Binders 10 10 8...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005895
EISBN: 978-1-62708-167-2
... in the solid state and efficiently isolates the melt from the contamination. With typical operating frequency of approximately 10 kHz, most of the molten mass is pushed from the walls by the electromagnetic field (semi-levitated), therefore preventing excessive heat losses and providing high overheating...