1-20 of 1995

Search Results for selective plating

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001261
EISBN: 978-1-62708-170-2
... Abstract Selective plating, also known as brush plating, differs from traditional tank or bath plating in that the workpiece is not immersed in a plating solution (electrolyte). Instead, the electrolyte is brought to the part and applied by a handheld anode or stylus, which incorporates...
Image
Published: 01 January 1994
Fig. 1 Manual operation of selective plating process. Source: Ref 1 More
Image
Published: 01 January 1994
Fig. 3 Turning head. Courtesy of SIFCO Selective Plating More
Image
Published: 01 January 1994
Fig. 4 Rotostylus. Courtesy of SIFCO Selective Plating More
Image
Published: 01 December 1998
Fig. 4 Manual operation of selective plating process More
Book Chapter

By Kenneth R. Newby
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001243
EISBN: 978-1-62708-170-2
... Abstract Hard chromium plating is produced by electrodeposition from a solution containing chromic acid and a catalytic anion in proper proportion. This article presents the major uses of hard chromium plating, and focuses on the selection factors, plating solutions, solution and process...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003215
EISBN: 978-1-62708-199-3
... discusses selective plating, electroforming, and other processes and where they are typically used. copper plating electrodeposition electroforming indium plating lead plating nickel plating plating baths selective plating silver plating zinc plating Copper Plating COPPER can...
Image
Published: 01 November 2010
Fig. 71 Three-dimensional computer model of heating selected areas of a plate by using a hairpin inductor. Courtesy of Infolytica Corp. More
Book Chapter

By Milton F. Stevenson, Sr.
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001247
EISBN: 978-1-62708-170-2
... of cadmium plating with attention to the materials of construction and equipment used. The article provides a description of the selection of plating method with examples, applications, and several postplating processes of cadmium plating. anode system bath temperature brighteners cadmium plating...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005784
EISBN: 978-1-62708-165-8
...: brushing, dipping, dispensing, spraying and stamping. cleaning coating copper plating heat treatment mechanical masking stop-off paints CASE HARDENING may be restricted to selected portions of a surface, so that soft areas remain to allow for secondary operations such as machining, drilling...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003177
EISBN: 978-1-62708-199-3
... Abstract This article describes the presses that are mechanically or hydraulically powered and used for producing sheet, strip, and plate from sheet metal. It also presents the JIC standards for presses, compares the presses based on power source, details the selection criteria and provides...
Book Chapter

Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001309
EISBN: 978-1-62708-170-2
... Abstract The selection of surface treatments for copper and copper alloys is generally based on application requirements for appearance and corrosion resistance. This article describes cleaning, finishing, and coating processes for copper and copper alloys. These processes include pickling...
Book Chapter

By Rebecca Tuszynski, N.V. Mandich
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003022
EISBN: 978-1-62708-200-6
... discusses the selection of plastics for plating. This article also describes metallizing techniques, including plating (electrolytic or electroplating), vacuum metallizing and thermal spraying, and environmental considerations. The article discusses the quality assurance procedures for metallized plastic...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005148
EISBN: 978-1-62708-186-3
..., and the typical materials for punches and blank holders. The article describes the typical causes of wear (galling) of deep-drawing tooling. It analyzes the selection of a harder and more wear-resistant material, the application of a surface coating such as chromium plating to the finished tools, and surface...
Book Chapter

By S.D. Washko, G. Aggen
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
.... The selection of stainless steels may be based on corrosion resistance, fabrication characteristics, availability, mechanical properties in specific temperature ranges and product cost. The fabrication characteristics of stainless steels include formability, forgeability, machinability, and weldability...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005897
EISBN: 978-1-62708-167-2
...: workpiece power estimation; estimation of electrical and thermal efficiency of the coil; and frequency selection for heating solid cylinders, tubes, pipes, slabs, plates, strips, and rectangular workpieces. electrical efficiency frequency induction coils induction hardening pipes plates slabs...
Book Chapter

By Alan Blair
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001252
EISBN: 978-1-62708-170-2
...-speed, selective plating of leadframes or similar electronic components requires the use of extremely high current densities and short plating times. Typical thicknesses range from 1.5 to 5.0 μm deposited in less than 2 s. Under these conditions, solutions containing free cyanide decompose very rapidly...
Book Chapter

By Satyam S. Sahay
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005787
EISBN: 978-1-62708-165-8
... annealing, supercritical or full annealing, and process annealing. Spheroidizing is performed for improving the cold formability of steels. The article provides guidelines for annealing and tabulates the critical temperature values for selected carbon and low-alloy steels and recommended temperatures...
Book Chapter

By Prabir K. Chaudhury, Roger Rees
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003981
EISBN: 978-1-62708-185-6
... Abstract Roll forging is a process for simultaneously reducing the cross-sectional area and changing the shape of heated bars, billets, or plates. This article provides an overview of the process capabilities, production techniques, machines and machine size selection considerations, and types...
Book Chapter

By Pel Lynah
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002154
EISBN: 978-1-62708-188-7
... Abstract Lapping is the lower-pressure, lower-speed, and lower-power application of the use of fixed abrasives. This article begins with a discussion on the process capabilities of lapping and reviews the selection of abrasive and vehicle for lapping. It describes the methods of lapping outer...