1-20 of 827

Search Results for secondary fabrication

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001081
EISBN: 978-1-62708-162-7
... are converted into general mill products and secondary fabrication (forging, extrusion, forming, machining, chemical milling and joining) of finished shapes from mill products and the heat treatment of titanium alloys. fabrication forgings heat treatment mechanical properties microstructure mill...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003141
EISBN: 978-1-62708-199-3
..., including all operations that convert ingot into general mill products, such as billet, bar, plate, sheet, strip, tube, and wire. The section on secondary fabrication describes processes such as die forging, extrusion, hot and cold forming, machining, chemical milling, and joining. The article presents...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006058
EISBN: 978-1-62708-175-7
... Abstract This article briefly describes the production of beryllium powder and beryllium/beryllium oxide metal-matrix powder. It discusses fully dense consolidation methods: vacuum hot pressing, hot isostatic pressing, and cold isostatic pressing. Secondary fabrication operations of beryllium...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001084
EISBN: 978-1-62708-162-7
..., refining, and melting. It also discusses the primary and secondary fabrication of zirconium and hafnium and its alloys. The article talks about the metallurgy of zirconium and its alloys with emphasis on allotropic transformation, cold work and recrystallization, anisotropy and preferred orientation...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003149
EISBN: 978-1-62708-199-3
... Abstract This article discusses the general characteristics, primary and secondary fabrication methods, product forms, and corrosion resistance of zirconium and hafnium. It describes the physical metallurgy of zirconium and its alloys, providing details on allotropic transformation...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001057
EISBN: 978-1-62708-162-7
... Abstract Aluminum, the second most plentiful metallic element, is an economic competitor in various applications owing to its appearance, light weight, fabricability, physical properties, mechanical properties, and corrosion resistance. This article discusses the primary and secondary...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006133
EISBN: 978-1-62708-175-7
... Abstract Refractory metals are typically processed from powders into ingots that are subsequently swaged into round bars or rolled into plates. Secondary operations are required to fabricate more complex refractory metal components. This article discusses two such secondary operations, namely...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003013
EISBN: 978-1-62708-200-6
... of these resins. Classification Plastics recycling is classified into four categories: primary, secondary, tertiary, and quaternary. Primary Recycling Primary recycling is the reprocessing of scrap plastics that are generated in-house during normal production or during fabrication of finished...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001091
EISBN: 978-1-62708-162-7
... recovery from bauxite, zinc ore and secondary recovery process and purification. The article briefly describes the fabrication process of gallium arsenide crystals. Furthermore, the article gives a short note on world supply and demand of gallium and concludes with research and development on gallium...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003121
EISBN: 978-1-62708-199-3
... Abstract Aluminum and its alloys are used in a broad range of applications. This article discusses the primary and secondary production of aluminum and the classification system for cast and wrought products. It describes some of the more common manufactured forms, including commercial wrought...
Image
Published: 15 June 2020
Fig. 13 Shows the effect of energy density on (a) secondary arm spacing, and (b) hardness of H13 and D2 steels fabricated using DMT. Source: Ref 22 More
Image
Published: 01 June 2024
Fig. 30 Secondary electron SEM fractographs of fatigue crack initiation at a nonmetallic inclusion in an airplane wing spar fabricated from aluminum alloy 6061-T651 More
Image
Published: 01 June 2024
Fig. 10 Secondary electron SEM fractograph of microvoid coalescence fracture features in a helicopter rotor control system drive pin fabricated from AerMet100 alloy quenched and aged to 53 HRC More
Image
Published: 01 June 2024
Fig. 39 Secondary electron SEM fractograph of a low-cycle fatigue fracture surface on a fractured aircraft turbine engine fan blade fabricated from wrought alloy Ti-8Al-1Mo-1V More
Image
Published: 01 June 2024
Fig. 54 Secondary electron SEM fractograph of a fractured connecting rod from an aircraft reciprocating engine. The rod is fabricated from quenched-and-tempered alloy steel, and the fracture surface exhibits mechanical damage due to smearing. More
Image
Published: 01 June 2024
Fig. 40 Secondary electron SEM fractograph showing the transition from stage 2 fatigue fracture to stage 3 monotonic fracture (overstress) in a turbine engine diffuser case wall (fabricated from a nickel-base high-temperature superalloy). Original magnification: 200× More
Image
Published: 01 June 2024
Fig. 58 Secondary electron SEM fractograph of a fractured turbine engine shaft. The shaft is fabricated from GE1014 ultrahigh-strength steel. The fracture exhibits cleavagelike transgranular features. Original magnification: 3.46 k×. (See Fig. 59 for reference fracture created under More
Image
Published: 01 June 2024
Fig. 49 Secondary electron SEM fractograph of a fractured commercial airplane landing gear. The gear is fabricated from quenched-and-tempered type 300M steel. The fractograph shows the transition from stress-corrosion cracking (SCC) to fatigue to final overstress fracture once a critical crack More
Image
Published: 01 June 2024
Fig. 59 Secondary electron SEM fractographs of a notched specimen used to create a reference fracture under controlled hydrogen-charging parameters. The sample is fabricated from GE1014 ultrahigh-strength steel. (a) Overall fracture. Original magnification: 37×. (b) Environmentally assisted More
Image
Published: 01 January 1987
Fig. 1060 Surface of a fracture in an aircraft lower-bulkhead cap fabricated from an extrusion of aluminum alloy 7075-T6. The cap was cut open to expose the fracture for inspection, and evidence of corrosion was found along the edge at which fracture was initiated (bottom edge in this view More